CN100488400C - 一种币章的制作方法 - Google Patents

一种币章的制作方法 Download PDF

Info

Publication number
CN100488400C
CN100488400C CNB2005100276440A CN200510027644A CN100488400C CN 100488400 C CN100488400 C CN 100488400C CN B2005100276440 A CNB2005100276440 A CN B2005100276440A CN 200510027644 A CN200510027644 A CN 200510027644A CN 100488400 C CN100488400 C CN 100488400C
Authority
CN
China
Prior art keywords
coin
oval
cushion block
blank cake
cake
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CNB2005100276440A
Other languages
English (en)
Other versions
CN1891098A (zh
Inventor
章军
刘耀光
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China Banknote Printing and Minting Group Co Ltd
Original Assignee
China Banknote Printing and Minting Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China Banknote Printing and Minting Corp filed Critical China Banknote Printing and Minting Corp
Priority to CNB2005100276440A priority Critical patent/CN100488400C/zh
Publication of CN1891098A publication Critical patent/CN1891098A/zh
Application granted granted Critical
Publication of CN100488400C publication Critical patent/CN100488400C/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种币章的制作方法,其特征为:所述币章的制作方法包括以下步骤,a、先冲制成币章坯饼;b、将币章坯饼冲去椭圆形内孔;c、在币章坯饼的椭圆形内孔中卡放一椭圆形垫块;d、在开有椭圆形孔的模具上进行压印;e、压印成型后取出椭圆形垫块;f、最后在椭圆形内孔镶嵌一镀金物件。本发明由于增加了在币章坯饼的椭圆形内孔中卡放一椭圆形垫块、在模具相对应位置设置相应的椭圆形孔,在开有椭圆形孔的模具上进行压印,然后压印成型后取出椭圆形垫块的步骤,解决了压印过程中椭圆形内孔变形,同时消除了内孔壁有冲痕的问题。

Description

一种币章的制作方法
技术领域:
本发明属于币章的技术领域,具体地说是涉及一种改进的币章制作工艺。
背景技术:
目前的镂空纪念章从外形来分有相当一部分为外圆内方、外圆内圆等,这种镂空纪念章一般均为同心圆,也就是内孔与外圈的圆的圆心一致,在内孔镶嵌有物件,制作工艺采用先压印再冲空,然后在内孔进行镶嵌,内孔不仅容易受损甚至整体变形,且内孔壁有冲痕影响外观。
发明内容:
本发明的目的是提供一种币章的制作方法,它可解决内孔变形,和内孔壁有冲痕的问题。
为了实现上述目的,本发明的技术方案是:一种币章的制作方法,其特征在于:所述币章的制作方法包括以下步骤,a、先冲制成币章坯饼;b、将币章坯饼冲去椭圆形内孔;c、在币章坯饼的椭圆形内孔中卡放一椭圆形垫块;d、在开有椭圆形孔的模具上进行压印;e、压印成型后取出椭圆形垫块;f、最后在椭圆形内孔镶嵌一镀金物件;其中垫块的尺寸比椭圆形内孔的尺寸大0.1-3毫米,垫块的厚度比币章坯饼的厚度大0.2-5毫米,在模具中开有的椭圆形孔的尺寸比币章坯饼椭圆形内孔的尺寸大0.2-4毫米。
本发明由于增加了在币章坯饼的椭圆形内孔中卡放一椭圆形垫块、在模具相对应位置设置相应的椭圆形孔,在开有椭圆形的模具上进行压印,然后压印成型后取出椭圆形垫块的步骤,解决了压印过程中椭圆形内孔变形,同时消除了内孔壁有冲痕的问题。
附图说明:
图1为本发明中的冲孔步骤示意图
图2为本发明中的压印步骤示意图
具体实施方式:
下面结合附图和实施例对本发明进一步的描述。
本发明为一种币章的制作方法,其特征在于:所述币章的制作方法包括以下步骤,a、先冲制成币章坯饼1;b、将币章坯饼进行冲空形成椭圆形内孔;c、在币章坯饼的椭圆形内孔中卡放一椭圆形垫块2;d、在模具相对应位置设置相应的椭圆形孔,在开有椭圆形孔的模具3上进行压印;e、压印成型后取出椭圆形垫块;f、最后在椭圆形内孔镶嵌一镀金物件。实施中币章坯饼为圆形或椭圆形,同时为冲制成的币章坯饼进行光边。垫块为钢性垫块,垫块的周边为倾斜状,倾斜的角度为5-30度;垫块的尺寸比椭圆形内孔的尺寸大0.1-3毫米,垫块的厚度比币章坯饼的厚度大0.2-5毫米;在模具中开有的椭圆形孔的尺寸比币章坯饼椭圆形内孔的尺寸大0.2-4毫米,在压印过程中,由于强压力的作用,会产生金属的流动,椭圆形内孔必然会产生变形,而增设的椭圆形垫块和在开有椭圆形孔的模具上进行压印可保证压印时模具的上模不触及到垫块,这样椭圆形内孔就不会产生变形,且垫块的周边有一定的倾斜度,因此很容易从椭圆形内孔中取出,且由于压印的吨位可达350吨,在压印时币章坯饼的椭圆形内孔的孔壁与椭圆形垫块的周边进行充分的挤压,而椭圆形垫块的硬度大于币章坯饼的硬度,可消除椭圆形内孔孔壁的冲痕,因此,最终完成的币章椭圆形的内孔尺寸为椭圆形垫块的尺寸,实施中币章坯饼为圆形,币章坯饼内的椭圆形内孔与币章圆形坯饼的外圆为非同心圆;在椭圆形内孔镶嵌一圆雕形可左右晃动的十二生肖动物的镀金物件,本制作方法中的冲制成币章坯饼、将币章坯饼冲、模具的制作、在模具上进行压印和在椭圆形内孔镶嵌一镀金物件均为现有技术,在此不做具体描述。
实施例1
首先冲制成厚度为3.5毫米,直径为59.55毫米的圆形银章坯饼;然后将圆形银章坯饼冲去椭圆形内孔,该椭圆形内孔与银章坯饼的外圆不是同心圆;在币章坯饼的椭圆形内孔中卡放一有斜度的椭圆形钢性垫块,此钢性垫块的材质采用轴承钢,硬度HRC60,钢性垫块的厚度为8毫米;在开有椭圆形孔的模具上进行压印,压印的吨位为350吨,使椭圆形内孔的孔壁与钢性垫块进行挤压,消除了椭圆形内孔孔壁的冲痕;压印成型后取出椭圆形垫块;最后在椭圆形内孔镶嵌一镀金鸡。
实施例2
首先冲制成厚度为2.5毫米,直径为39.8毫米的圆形金币坯饼;然后将圆形金币坯饼冲去椭圆形内孔,该椭圆形内孔与金币坯饼的外圆不是同心圆;在金币坯饼的椭圆形内孔中卡放一有斜度的椭圆形钢性垫块,此钢性垫块的材质采用轴承钢,硬度HRC60,钢性垫块的厚度为5毫米;在开有椭圆形孔的模具上进行压印,压印的吨位为330吨,使椭圆形内孔的孔壁与钢性垫块进行挤压,消除了椭圆形内孔孔壁的冲痕;压印成型后取出椭圆形垫块;最后在椭圆形内孔镶嵌一金狗。

Claims (5)

1、一种币章的制作方法,其特征在于:所述币章的制作方法包括以下步骤,a、先冲制成币章坯饼;b、将币章坯饼冲去椭圆形内孔;c、在币章坯饼的椭圆形内孔中卡放一椭圆形垫块,椭圆形垫块的硬度大于币章坯饼的硬度;d、在开有椭圆形孔的模具上进行压印;e、压印成型后取出椭圆形垫块;f、最后在椭圆形内孔镶嵌一镀金物件;其中垫块的横截面大小尺寸比椭圆形内孔的尺寸大0.1-3毫米,垫块的厚度比币章坯饼的厚度大0.2-5毫米,在模具中开有的椭圆形孔的尺寸比币章坯饼椭圆形内孔的尺寸大0.2-4毫米。
2、如权利要求1所述的一种币章的制作方法,其特征在于:币章坯饼为圆形或椭圆形。
3、如权利要求1或2所述的一种币章的制作方法,其特征在于:冲制成币章坯饼后进行光边。
4、如权利要求1或2所述的一种币章的制作方法,其特征在于:垫块为钢性垫块,垫块的周边为倾斜状,倾斜的角度为5-30度。
5、如权利要求1或2所述的一种币章的制作方法,其特征在于:币章坯饼为圆形,币章坯饼内的椭圆形内孔与币章圆形坯饼的外圆为非同心圆;在椭圆形内孔镶嵌一圆雕形可左右晃动的十二生肖动物的镀金物件。
CNB2005100276440A 2005-07-08 2005-07-08 一种币章的制作方法 Active CN100488400C (zh)