CN100401561C - 无汞扣式电池负极锌膏 - Google Patents
无汞扣式电池负极锌膏 Download PDFInfo
- Publication number
- CN100401561C CN100401561C CNB2006100371789A CN200610037178A CN100401561C CN 100401561 C CN100401561 C CN 100401561C CN B2006100371789 A CNB2006100371789 A CN B2006100371789A CN 200610037178 A CN200610037178 A CN 200610037178A CN 100401561 C CN100401561 C CN 100401561C
- Authority
- CN
- China
- Prior art keywords
- zinc
- mercury
- cream
- button cell
- indium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (5)