CN100335839C - 钢套钢耐高温直埋防腐保温系统 - Google Patents
钢套钢耐高温直埋防腐保温系统 Download PDFInfo
- Publication number
- CN100335839C CN100335839C CNB2005100546276A CN200510054627A CN100335839C CN 100335839 C CN100335839 C CN 100335839C CN B2005100546276 A CNB2005100546276 A CN B2005100546276A CN 200510054627 A CN200510054627 A CN 200510054627A CN 100335839 C CN100335839 C CN 100335839C
- Authority
- CN
- China
- Prior art keywords
- steel
- high temperature
- enclosing
- pipe
- temperature resistant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种由保温管道、三通、弯头、固定支座环板、补偿器、疏水管和排潮管组成的钢套钢耐高温直埋防腐保温系统,其特点是钢套钢耐高温直埋防腐保温管道、三通和补偿器,从里到外依次由内钢管、高温黏合剂层、硅酸盐高温纤维毡减阻层、硅酸盐保温瓦层、有机耐高温硬质聚氨酯泡沫塑料保温层、螺旋焊缝保护钢管、6-8微米的环氧粉末涂层、170-250微米的胶粘剂层和3-5毫米的高密度聚乙烯保护层组成,并在硅酸盐保温瓦层的保温瓦缝之间填有憎水泡沫石棉。这种钢套钢蒸汽直埋防腐保温系统具有能承重、不变形、保温效果好、热量损失少、防腐效果好和寿命长等优点,特别适用于温度高于300℃的过热蒸汽地下输送。
Description
技术领域
本实用新型涉及直埋保温系统,特别涉及一种用于地下输送高温过热蒸汽的钢套钢耐高温直埋防腐保温系统。
背景技术
目前城市供热管道多采用直埋铺设方式,即供热管道直接埋在地下,现有供热管道的结构一般为:最内层为金属管道,金属管道外设有保温层,保温层多为两层:内保温层为保温瓦块扣合而成,外保温层为聚氨酯硬质泡沫塑料,最外层是PVC材料的塑料管保护层。具有如下缺点,由于保温瓦块之间有诸多接缝,当过热蒸汽通过钢管时,由保温瓦块材料的特性所决定的,保温瓦块会发生微量收缩现象,造成逐个接缝宽度加大,钢管内的热量通过各接缝处散发,不仅造成热量损失,同时还会造成外保护层受热软化膨胀,加速其老化,最后开裂渗水。即浪费能源又缩短了保温系统的使用寿命。虽然有诸多专利和文献报道了各种保温管道的制作方法,但它们大部分仅用于输送300℃以下的过热蒸汽,不能用于输送300℃以上的热电厂产生的高达350℃以上的高温过热蒸汽。即使有一些特殊的保温管道用于350℃以上的高温过热蒸汽输送,但由于其在三通、弯头、固定支座环板、补偿器、疏水管和排潮管等环节保温处理不完善,同样造成能源的浪费,并且这种特殊的保温管道造价较高。
发明内容
本发明的目的在于通过提供一种具有独特结构的钢套钢耐高温直埋防腐保温系统,用于输送高温过热蒸汽,以达到减少热量损失、延长保温管道寿命和降低造价的目的。
本发明解决其技术问题所采用的技术方案是:提供一种钢套钢耐高温直埋防腐保温系统,由保温管道、三通、弯头、固定支座环板、补偿器、疏水管和排潮管组成,其特点是:
a、保温管道、三通和补偿器为钢套钢耐高温直埋防腐保温管道、钢套钢耐高温直埋防腐保温三通和钢套钢耐高温直埋防腐保温补偿器,从里到外依次由内钢管、高温黏合剂层、硅酸盐高温纤维毡减阻层、硅酸盐保温瓦层、有机耐高温硬质聚氨酯泡沫塑料保温层、螺旋焊缝保护钢管、6-8微米的环氧粉末涂层、170-250微米的胶粘剂层和3-5毫米的高密度聚乙烯保护层组成,并在硅酸盐保温瓦层的保温瓦缝之间填有憎水泡沫石棉;
b、弯头、疏水管和排潮管为钢套钢耐高温直埋防腐保温弯头、钢套钢耐高温直埋防腐保温疏水管和钢套钢耐高温直埋防腐保温排潮管,从里到外依次由内钢管(1)、岩棉管(18)、保护钢管(5)、6-8微米的环氧粉末涂层(6)、170-250微米的胶粘剂层(7)和3-5毫米的高密度聚乙烯保护层(8)组成;
c、固定支座环板分别焊接在保温管的保护钢管和内钢管上,并通过固定支座加强筋加以固定支撑。
本发明所述的高温黏合剂层的黏合剂由以下重量比的组分组成:
有机硅树脂 20
氧化铝粉溶剂 7
混合溶剂 10
云母粉 6
其中混合溶剂为甲苯和丙酮的体积比为2∶1,这种黏合剂能够承受很高的温度,在400℃下,不流动,不变质;所述的硅酸盐高温纤维毡减阻层为硅酸铝高温纤维毡;所述的硅酸盐保温瓦层为轻质微孔硅酸钙制成的保温瓦;所述的胶粘剂层为ABS胶粘剂,其组成成分具有如下重量比:甲乙酮∶ABS∶甲苯=6∶4∶5。
这种钢套钢耐高温直埋防腐保温系统中的保温管道、三通和补偿器的制作方法是:a、取焊缝高度为2-4毫米的PN1.6螺旋钢管、或者无缝钢管做内钢管,表面除锈处理后喷涂耐高温无机黏合剂(在焊缝两侧留出2-3毫米距离),再粘上高温纤维毡做减阻层,当钢管受热伸缩时,起到减阻和保护其外层保温层的作用。b、在减阻层外侧扣合两层保温瓦块,以轻质微孔硅酸钙制成的保温瓦为最佳,扣合时各相邻接缝互相错位,并在环缝和纵缝等各接缝处嵌入憎水泡沫石棉做涨缩层,当保温瓦块受热发生微量收缩使相邻瓦块接缝加宽时,憎水泡沫石棉涨缩层随之膨胀,以防止热量由此散发,达到良好的保温效果。c、在保温瓦块外侧,采用定心法套上螺旋焊缝保护钢管,使保护钢管与蒸汽钢管同轴。d、向保护钢管与保温瓦块之间注入硬质聚氨酯泡沫塑料的发泡料,发泡后3分钟即可固化形成硬质聚氨酯泡沫塑料保温层。e、在保护钢管外壁抛光,达到近白级,再进行中频加热后,喷涂6-8微米的环氧粉末涂层、170-250微米的胶粘剂层和3-5毫米的高密度聚乙烯保护层,制成钢套钢耐高温直埋防腐保温系统中的保温管道、三通、补偿器和弯头。制作钢套钢耐高温直埋防腐保温弯头、疏水管和排潮管的方法差别只是在于内钢管和保护钢管之间采用岩棉管进行保温。
本发明所提供的钢套钢耐高温直埋防腐保温系统,与现有保温系统相比,增加了保温系统的承重能力,不易变形,保温效果均匀;具有耐高温、保温效果好、热量损失少、防腐效果好和寿命长等优点,特别适用于温度高于300℃的过热蒸汽的输送,具有良好的市场前景。
下面结合实施例和附图对本发明作进一步说明。
附图说明
图1钢套钢蒸汽直埋防腐保温系统中保温管道、三通和弯头的管口截面图。
图2钢套钢耐高温直埋防腐保温系统各组元的组合剖面全图。
图3带排潮管、疏水管的钢套钢耐高温直埋防腐保温系统的固定支座剖面图。
图4钢套钢耐高温直埋防腐保温系统的三通剖面图。
图5钢套钢耐高温直埋防腐保温系统的弯头剖面图。
图6钢套钢耐高温直埋防腐保温系统的保温补偿器剖面图。
图中,1.内钢管,2.硅酸盐高温纤维毡减阻层,3.硅酸盐保温瓦层,4.聚氨酯泡沫塑料保温层,5.保护钢管,6.环氧粉末涂层,7.胶粘剂层,8.聚乙烯保护层,9.憎水泡沫石棉,10.黏合剂层,11.支座加强筋,12.保温管道,13.三通,14.疏水管,15.排潮管,16.补偿器,17.弯头,18.支座环板,19.岩棉管。
具体实施方式
实施例1.a、取焊缝高度为2-4毫米的PN1.6螺旋钢管、或者无缝钢管做内钢管(1),表面除锈处理后喷涂耐高温无机黏合剂(10)(在焊缝两侧留出2-3毫米距离),再粘上高温纤维毡(2)做减阻层,当钢管受热伸缩时,起到减阻和保护其外层保温层的作用。b、在减阻层外侧扣合两层保温瓦块(3),以轻质微孔硅酸钙制成的保温瓦为最佳,扣合时各相邻接缝互相错位,并在环缝和纵缝等各接缝处嵌入憎水泡沫石棉(9)做涨缩层,当保温瓦块受热发生微量收缩使相邻瓦块接缝加宽时,憎水泡沫石棉涨缩层随之膨胀,以防止热量由此散发,达到良好的保温效果。c、在保温瓦块外侧,采用定心法套上螺旋焊缝保护钢管(5),使保护钢管与蒸汽钢管同轴。d、向保护钢管与保温瓦块之间注入硬质聚氨酯泡沫塑料的发泡料,发泡后3分钟即可固化形成硬质聚氨酯泡沫塑料保温层(4)。e、在保护钢管外壁抛光,达到近白级,再进行中频加热后,喷涂6-8微米的环氧粉末涂层(6)、170-250微米的胶粘剂层(7)和3-5毫米的高密度聚乙烯保护层(8),制成钢套钢耐高温直埋防腐保温系统中的保温管道(12)、钢套钢耐高温直埋防腐保温三通(13)和补偿器(16)。制作钢套钢耐高温直埋防腐保温弯头(17)、疏水管(14)和排潮管(15)的方法差别只是在于内钢管和保护钢管之间采用岩棉管(19)进行保温。固定支座环板(18)分别焊接在保温管的保护钢管(5)和内钢管(1)上,并通过固定支座加强筋(11)加以固定支撑。
由钢套钢耐高温直埋防腐保温保温管道(12)、三通(13)、补偿器(16)、弯头(17)、疏水管(14)、排潮管(15)和固定支座环板(18)组成钢套钢耐高温直埋防腐保温系统。
Claims (5)
1.一种钢套钢耐高温直埋防腐保温系统,由保温管道、三通、弯头、固定支座环板、补偿器、疏水管和排潮管组成,其特征在于:
a、保温管道、三通和补偿器为钢套钢耐高温直埋防腐保温管道(12)、钢套钢耐高温直埋防腐保温三通(13)和钢套钢耐高温直埋防腐保温补偿器(16),从里到外依次由内钢管(1)、高温黏合剂层(10)、硅酸盐高温纤维毡减阻层(2)、硅酸盐保温瓦层(3)、有机耐高温硬质聚氨酯泡沫塑料保温层(4)、螺旋焊缝保护钢管(5)、6-8微米的环氧粉末涂层(6)、170-250微米的胶粘剂层(7)和3-5毫米的高密度聚乙烯保护层(8)组成,并在硅酸盐保温瓦层(3)的保温瓦缝之间填有憎水泡沫石棉(9);
b、弯头、疏水管和排潮管为钢套钢耐高温直埋防腐保温弯头(17)、钢套钢耐高温直埋防腐保温疏水管(14)和钢套钢耐高温直埋防腐保温排潮管(15),从里到外依次由内钢管(1)、岩棉管(19)、保护钢管(5)、6-8微米的环氧粉末涂层(6)、170-250微米的胶粘剂层(7)和3-5毫米的高密度聚乙烯保护层(8)组成;
c、固定支座环板(18)分别焊接在保温管的保护钢管(5)和内钢管(1)上,并通过固定支座加强筋(11)加以固定支撑。
2.根据权利要求1所述的钢套钢耐高温直埋防腐保温系统,其特征在于所述的高温黏合剂层(10)的黏合剂由以下重量比的组分组成:
有机硅树脂 20
氧化铝粉溶剂 7
混合溶剂 10
云母粉 6
其中混合溶剂为体积比为2∶1的甲苯和内酮。
3.根据权利要求1所述的钢套钢耐高温直埋防腐保温系统,其特征在于所述的硅酸盐高温纤维毡减阻层(2)为硅酸铝高温纤维毡。
4.根据权利要求1所述的钢套钢耐高温直埋防腐保温系统,其特征在于所述的硅酸盐保温瓦层(3)为轻质微孔硅酸钙制成的保温瓦。
5.根据权利要求1所述的钢套钢耐高温直埋防腐保温系统,其特征在于所述的胶粘剂层为ABS胶粘剂,其组成成分具有如下重量比:甲乙酮∶ABS∶甲苯=6∶4∶5。