BR112023000877A2 - Liga de chumbo, eletrodo positivo para bateria de armazenamento de chumbo, bateria de armazenamento de chumbo e sistema de armazenamento de energia - Google Patents
Liga de chumbo, eletrodo positivo para bateria de armazenamento de chumbo, bateria de armazenamento de chumbo e sistema de armazenamento de energiaInfo
- Publication number
- BR112023000877A2 BR112023000877A2 BR112023000877A BR112023000877A BR112023000877A2 BR 112023000877 A2 BR112023000877 A2 BR 112023000877A2 BR 112023000877 A BR112023000877 A BR 112023000877A BR 112023000877 A BR112023000877 A BR 112023000877A BR 112023000877 A2 BR112023000877 A2 BR 112023000877A2
- Authority
- BR
- Brazil
- Prior art keywords
- lead
- storage battery
- positive electrode
- less
- mass
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C11/00—Alloys based on lead
- C22C11/06—Alloys based on lead with tin as the next major constituent
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/14—Electrodes for lead-acid accumulators
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/12—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of lead or alloys based thereon
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/06—Lead-acid accumulators
- H01M10/12—Construction or manufacture
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/06—Lead-acid accumulators
- H01M10/18—Lead-acid accumulators with bipolar electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M2004/026—Electrodes composed of, or comprising, active material characterised by the polarity
- H01M2004/028—Positive electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Cell Electrode Carriers And Collectors (AREA)
- Battery Electrode And Active Subsutance (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2020133406 | 2020-08-05 | ||
| PCT/JP2021/028490 WO2022030416A1 (ja) | 2020-08-05 | 2021-07-30 | 鉛合金、鉛蓄電池用正極、鉛蓄電池、及び蓄電システム |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| BR112023000877A2 true BR112023000877A2 (pt) | 2023-02-14 |
Family
ID=80118071
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| BR112023000877A BR112023000877A2 (pt) | 2020-08-05 | 2021-07-30 | Liga de chumbo, eletrodo positivo para bateria de armazenamento de chumbo, bateria de armazenamento de chumbo e sistema de armazenamento de energia |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US20230170464A1 (https=) |
| EP (1) | EP4194574A4 (https=) |
| JP (2) | JP7575462B2 (https=) |
| CN (1) | CN116034175B (https=) |
| AU (1) | AU2021321667A1 (https=) |
| BR (1) | BR112023000877A2 (https=) |
| WO (1) | WO2022030416A1 (https=) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPWO2022224622A1 (https=) * | 2021-04-20 | 2022-10-27 | ||
| WO2024225273A1 (ja) * | 2023-04-28 | 2024-10-31 | 古河電気工業株式会社 | 圧延鉛合金箔、鉛蓄電池用電極、及び鉛蓄電池 |
Family Cites Families (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4148175B2 (ja) * | 2004-03-31 | 2008-09-10 | 新神戸電機株式会社 | 鉛合金及びそれを用いた鉛蓄電池 |
| JP5087950B2 (ja) * | 2007-02-27 | 2012-12-05 | 新神戸電機株式会社 | 鉛蓄電池 |
| US8828582B2 (en) * | 2011-05-11 | 2014-09-09 | Gridtential Energy, Inc. | Battery and assembly method |
| WO2014149254A2 (en) * | 2013-03-15 | 2014-09-25 | Dhar Subhash K | Metallic allyos having amorphous, nano-crystallline, or microcrystalline structure |
| JP6049528B2 (ja) * | 2013-04-11 | 2016-12-21 | 古河電池株式会社 | 正極格子基板の製造方法 |
| JP6504055B2 (ja) * | 2013-10-15 | 2019-04-24 | 株式会社Gsユアサ | 制御弁式鉛蓄電池 |
| EP3125341B1 (en) * | 2014-03-28 | 2018-11-14 | Hitachi Chemical Company, Ltd. | Lead storage cell and electrode collector for lead storage cell |
| US10276895B2 (en) * | 2015-01-08 | 2019-04-30 | Gs Yuasa International Ltd. | Positive electrode grid for lead acid batteries and method for producing the same, and lead acid battery |
| JP2019067522A (ja) * | 2017-09-28 | 2019-04-25 | 古河電池株式会社 | 鉛蓄電池用正極格子体の製造方法、蓄電池用正極格子体、及び鉛蓄電池 |
-
2021
- 2021-07-30 WO PCT/JP2021/028490 patent/WO2022030416A1/ja not_active Ceased
- 2021-07-30 AU AU2021321667A patent/AU2021321667A1/en not_active Abandoned
- 2021-07-30 BR BR112023000877A patent/BR112023000877A2/pt not_active IP Right Cessation
- 2021-07-30 JP JP2022541516A patent/JP7575462B2/ja active Active
- 2021-07-30 CN CN202180056879.XA patent/CN116034175B/zh active Active
- 2021-07-30 EP EP21854057.3A patent/EP4194574A4/en not_active Withdrawn
-
2023
- 2023-01-31 US US18/162,408 patent/US20230170464A1/en active Pending
- 2023-08-22 JP JP2023134641A patent/JP2023162291A/ja not_active Withdrawn
Also Published As
| Publication number | Publication date |
|---|---|
| EP4194574A4 (en) | 2024-09-25 |
| WO2022030416A1 (ja) | 2022-02-10 |
| AU2021321667A1 (en) | 2023-03-16 |
| JP7575462B2 (ja) | 2024-10-29 |
| CN116034175A (zh) | 2023-04-28 |
| US20230170464A1 (en) | 2023-06-01 |
| EP4194574A1 (en) | 2023-06-14 |
| JP2023162291A (ja) | 2023-11-08 |
| CN116034175B (zh) | 2024-04-12 |
| JPWO2022030416A1 (https=) | 2022-02-10 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| BR112023000877A2 (pt) | Liga de chumbo, eletrodo positivo para bateria de armazenamento de chumbo, bateria de armazenamento de chumbo e sistema de armazenamento de energia | |
| Zhang et al. | Long-term atmospheric corrosion of aluminum alloy 2024-T4 in coastal environment: Surface and sectional corrosion behavior | |
| Song et al. | Corrosion behaviour of extruded AM30 magnesium alloy under salt-spray and immersion environments | |
| Somlyo et al. | Elemental distribution in Rana pipiens retinal rods: quantitative electron probe analysis. | |
| CN101477010B (zh) | 一种腐蚀产物膜磨损性能及腐蚀电化学测试装置 | |
| Kaewmaneekul et al. | Effect of aluminium on the passivation of zinc–aluminium alloys in artificial seawater at 80 C | |
| Shahabi-Navid et al. | NaCl-induced atmospheric corrosion of the MgAl alloy AM50-the influence of CO2 | |
| CN105466843A (zh) | 一种沿海地区输电线路杆塔腐蚀剩余寿命预测方法 | |
| Klemper | An adenosine triphosphate-dependent calcium uptake pump in human neutrophil lysosomes. | |
| Mei et al. | Effects of dry/wet ratio and pre-immersion on stress corrosion cracking of 7050-T7451 aluminum alloy under wet-dry cyclic conditions | |
| Ge et al. | Stress corrosion cracking behavior of 2024 and 7075 high-strength aluminum alloys in a simulated marine atmosphere contaminated with SO2 | |
| Streicher | The dissolution of aluminum in sodium hydroxide solutions | |
| Shi et al. | Comments on the paper entitled “Observations of the galvanostatic dissolution of pure magnesium” by NT Kirkland, G. Williams and N. Birbilis | |
| Yin et al. | Enthalpies of dilution of aqueous Li2B4O7 solutions at 298.15 K and application of ion-interaction model | |
| Gelbach | The Activity Coefficients and Transference Numbers of Potassium Iodide1 | |
| FR3087944B1 (fr) | Generateur electrochimique au lithium et au fluorure de carbone comprenant un materiau d'electrode negative specifique | |
| Arkhipov et al. | Electrode potentials of bismuth in a mixture of potassium and lead chlorides | |
| Zhang et al. | Atmospheric corrosion of 7B04 aluminum alloy in marine environments | |
| Haynie et al. | Stress-corrosion cracking of aluminum alloys | |
| Weech et al. | STUDIES ON PERMEABILITY OF MEMBRANES: VIII. The Behavior of the Dried Collodion Membrane toward Bivalent Cations. | |
| Bakar et al. | Corrosion Protection Coatings from Size-Specified Graphene Oxide | |
| Marić et al. | Structural and climate performance indicators in service life prediction of concrete bridges in multi-hazard environment | |
| Bryan et al. | Composition and Evolution of Sea-Salt Deliquescent Brines on SNF Storage Canister Surfaces. | |
| Bao et al. | Effect of the addition of ZrO 2 on the liquidus temperature of nNaF· AlF 3-Al 2 O 3 molten salt system | |
| Horváth | Laboratory and Plant Measurements on Anode Process in Aluminum Electrolysis |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| B08F | Application dismissed because of non-payment of annual fees [chapter 8.6 patent gazette] |
Free format text: REFERENTE A 4A ANUIDADE. |
|
| B08K | Patent lapsed as no evidence of payment of the annual fee has been furnished to inpi [chapter 8.11 patent gazette] |
Free format text: EM VIRTUDE DO ARQUIVAMENTO PUBLICADO NA RPI 2841 DE 17-06-2025 E CONSIDERANDO AUSENCIA DE MANIFESTACAO DENTRO DOS PRAZOS LEGAIS, INFORMO QUE CABE SER MANTIDO O ARQUIVAMENTO DO PEDIDO DE PATENTE, CONFORME O DISPOSTO NO ARTIGO 12, DA RESOLUCAO 113/2013. |