WO2014061591A1 - Feuille électroconductrice et écran tactile - Google Patents

Feuille électroconductrice et écran tactile Download PDF

Info

Publication number
WO2014061591A1
WO2014061591A1 PCT/JP2013/077772 JP2013077772W WO2014061591A1 WO 2014061591 A1 WO2014061591 A1 WO 2014061591A1 JP 2013077772 W JP2013077772 W JP 2013077772W WO 2014061591 A1 WO2014061591 A1 WO 2014061591A1
Authority
WO
WIPO (PCT)
Prior art keywords
electrode
conductive sheet
layer
lattices
lattice
Prior art date
Application number
PCT/JP2013/077772
Other languages
English (en)
Japanese (ja)
Inventor
博重 中村
Original Assignee
富士フイルム株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 富士フイルム株式会社 filed Critical 富士フイルム株式会社
Publication of WO2014061591A1 publication Critical patent/WO2014061591A1/fr

Abstract

L'invention se rapporte à une feuille électroconductrice apportant une meilleure visibilité, ainsi qu'à un écran tactile. Dans une feuille électroconductrice (1), une couche de premières électrodes (10) comportant une pluralité de colonnes de premières électrodes (12), une couche d'isolation transparente (30) et une couche de secondes électrodes (40) comportant une pluralité de colonnes de secondes électrodes (42) sont empilées dans cet ordre. Les premières électrodes (12) comprennent une pluralité de premiers treillis (26) qui incluent M × N groupes de treillis. Les secondes électrodes (42) comprennent une pluralité de seconds treillis (56) qui incluent M × N groupes de treillis. La couche de premières électrodes (10) et la couche de secondes électrodes (40) sont disposées de manière à ce que la pluralité de premiers treillis (26) et la pluralité de seconds treillis (56) ne se chevauchent pas, et de manière à ce que, lorsqu'on les observe du dessus, la pluralité de premiers treillis (26) et la pluralité de seconds treillis (56) soient ininterrompues sur l'intégralité d'une surface. M et N sont des nombres entiers, et M + N ≤ 9.
PCT/JP2013/077772 2012-10-16 2013-10-11 Feuille électroconductrice et écran tactile WO2014061591A1 (fr)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2012228753A JP2014081766A (ja) 2012-10-16 2012-10-16 導電シート及びタッチパネル
JP2012-228753 2012-10-16

Publications (1)

Publication Number Publication Date
WO2014061591A1 true WO2014061591A1 (fr) 2014-04-24

Family

ID=50488157

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2013/077772 WO2014061591A1 (fr) 2012-10-16 2013-10-11 Feuille électroconductrice et écran tactile

Country Status (3)

Country Link
JP (1) JP2014081766A (fr)
TW (1) TW201428574A (fr)
WO (1) WO2014061591A1 (fr)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
GB2559646A (en) * 2017-02-09 2018-08-15 Solomon Systech Ltd Touch Sensor
CN108984053A (zh) * 2017-06-01 2018-12-11 乐金显示有限公司 触摸显示装置和触摸面板

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2016039127A1 (fr) 2014-09-12 2016-03-17 ポリマテック・ジャパン株式会社 Feuille de capteur et panneau de capteur
CN106155450B (zh) * 2016-07-29 2022-10-21 厦门天马微电子有限公司 集成触控显示面板和显示装置

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US20040239650A1 (en) * 2003-06-02 2004-12-02 Mackey Bob Lee Sensor patterns for a capacitive sensing apparatus
US20120062250A1 (en) * 2010-09-15 2012-03-15 Au Optronics Corp. Capacitive touch sensor and capacitive touch apparatus
JP2012146277A (ja) * 2010-05-27 2012-08-02 Fujifilm Corp 導電シート及び静電容量方式タッチパネル

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US20040239650A1 (en) * 2003-06-02 2004-12-02 Mackey Bob Lee Sensor patterns for a capacitive sensing apparatus
JP2012146277A (ja) * 2010-05-27 2012-08-02 Fujifilm Corp 導電シート及び静電容量方式タッチパネル
US20120062250A1 (en) * 2010-09-15 2012-03-15 Au Optronics Corp. Capacitive touch sensor and capacitive touch apparatus

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
GB2559646A (en) * 2017-02-09 2018-08-15 Solomon Systech Ltd Touch Sensor
CN108984053A (zh) * 2017-06-01 2018-12-11 乐金显示有限公司 触摸显示装置和触摸面板
CN108984053B (zh) * 2017-06-01 2021-09-10 乐金显示有限公司 触摸显示装置和触摸面板

Also Published As

Publication number Publication date
JP2014081766A (ja) 2014-05-08
TW201428574A (zh) 2014-07-16

Similar Documents

Publication Publication Date Title
JP5318998B2 (ja) 導電シート及びタッチパネル
JP5875484B2 (ja) 導電シート及びタッチパネル
US9055680B2 (en) Electroconductive sheet and touch panel
JP5638027B2 (ja) 導電シート及び静電容量方式タッチパネル
JP6728084B2 (ja) タッチパネル用導電性フィルム、表示装置、導電性フィルム、タッチパネル及びセンサ本体
JP5345980B2 (ja) 透明導電性基板、タッチパネル用導電シート及びタッチパネル
KR101641760B1 (ko) 도전 시트 및 터치 패널
WO2012157555A1 (fr) Feuille conductrice et panneau tactile
WO2011065383A1 (fr) Feuille conductrice, procédé d'utilisation de la feuille conductrice et écran tactile de type capacitif
WO2012157557A1 (fr) Feuille conductrice et panneau tactile
JP5507343B2 (ja) タッチパネル及び導電シート
JP5638459B2 (ja) タッチパネル及び導電シート
JP5748647B2 (ja) 導電シート及びタッチパネル
JP5509186B2 (ja) タッチパネル及びタッチパネル用導電シート
JP5850967B2 (ja) タッチパネル用導電シート及びタッチパネル
WO2014061591A1 (fr) Feuille électroconductrice et écran tactile
JP5777251B2 (ja) タッチパネル用導電シート及びタッチパネル

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 13847092

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 13847092

Country of ref document: EP

Kind code of ref document: A1