WO2009069782A1 - 連続鋳造中の溶融金属の成分調製方法及びその装置 - Google Patents
連続鋳造中の溶融金属の成分調製方法及びその装置 Download PDFInfo
- Publication number
- WO2009069782A1 WO2009069782A1 PCT/JP2008/071726 JP2008071726W WO2009069782A1 WO 2009069782 A1 WO2009069782 A1 WO 2009069782A1 JP 2008071726 W JP2008071726 W JP 2008071726W WO 2009069782 A1 WO2009069782 A1 WO 2009069782A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- molten metal
- composition
- continuous casting
- during continuous
- apparatus therefor
- Prior art date
Abstract
Priority Applications (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2008801180362A CN101878079B (zh) | 2007-11-30 | 2008-11-28 | 连续铸造中熔融金属的成分调节方法及其装置 |
US12/745,518 US8201614B2 (en) | 2007-11-30 | 2008-11-28 | Method and an apparatus of controlling chemical composition of a molten metal during continuous casting |
EP08854593.4A EP2226138A4 (en) | 2007-11-30 | 2008-11-28 | METHOD FOR REGULATING THE COMPOSITION OF A MOLTEN METAL IN A CONTINUOUS CASTING AND APPARATUS THEREOF |
Applications Claiming Priority (4)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2007311616 | 2007-11-30 | ||
JP2007-311616 | 2007-11-30 | ||
JP2008-302813 | 2008-11-27 | ||
JP2008302813A JP5224363B2 (ja) | 2007-11-30 | 2008-11-27 | 連続鋳造中の溶融金属の成分調製方法及びその装置 |
Publications (1)
Publication Number | Publication Date |
---|---|
WO2009069782A1 true WO2009069782A1 (ja) | 2009-06-04 |
Family
ID=40678671
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
PCT/JP2008/071726 WO2009069782A1 (ja) | 2007-11-30 | 2008-11-28 | 連続鋳造中の溶融金属の成分調製方法及びその装置 |
Country Status (7)
Country | Link |
---|---|
US (1) | US8201614B2 (ja) |
EP (1) | EP2226138A4 (ja) |
JP (1) | JP5224363B2 (ja) |
KR (1) | KR20100097681A (ja) |
CN (1) | CN101878079B (ja) |
TW (1) | TWI391192B (ja) |
WO (1) | WO2009069782A1 (ja) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
RU191826U1 (ru) * | 2018-11-22 | 2019-08-23 | Федеральное государственное автономное образовательное учреждение высшего образования "Уральский федеральный университет имени первого Президента России Б.Н. Ельцина" | Устройство фиксации нагревателя в электропечи |
Families Citing this family (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US8509942B2 (en) * | 2011-03-31 | 2013-08-13 | Furukawa Electronic Co., Ltd. | Method for producing metal ingot, method for controlling liquid surface, and ultrafine copper alloy wire |
JP5764431B2 (ja) * | 2011-08-23 | 2015-08-19 | 古河電気工業株式会社 | 金属鋳塊製造方法、金属鋳塊製造装置 |
CN105536082B (zh) * | 2016-01-27 | 2017-12-26 | 苏州元禾医疗器械有限公司 | 一种液量控制方法、装置、系统及负压创面治疗设备 |
CN112880401A (zh) * | 2019-11-29 | 2021-06-01 | 科德尔科股份公司 | 用于测量熔炼炉中白金属中铜的百分比的系统 |
JP7394017B2 (ja) * | 2020-05-14 | 2023-12-07 | Jx金属株式会社 | 金属合金の製造方法 |
JP7158434B2 (ja) * | 2020-05-14 | 2022-10-21 | Jx金属株式会社 | 銅合金インゴット、銅合金箔、および銅合金インゴットの製造方法 |
CN113145811B (zh) * | 2021-04-16 | 2022-10-18 | 鞍钢股份有限公司 | 一种高铝钢调铝装置及使用方法 |
Citations (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5865554A (ja) | 1981-10-14 | 1983-04-19 | Sumitomo Electric Ind Ltd | 導電用合金の連続鋳造圧延方法 |
JPS59169654A (ja) | 1983-03-15 | 1984-09-25 | Kawasaki Steel Corp | 溶融金属の化学成分調整方法 |
JPS59171834A (ja) | 1983-03-03 | 1984-09-28 | リムカ・リサ−チ・インコ−ポレ−テツド | 溶融金属内の粒子の検出測定方法並びに装置 |
JPH05277641A (ja) | 1992-04-03 | 1993-10-26 | Nippon Steel Corp | 複層金属材の連続鋳造方法 |
JPH0663710A (ja) | 1992-08-12 | 1994-03-08 | Hitachi Cable Ltd | 連続鋳造装置 |
JPH08300119A (ja) | 1995-05-08 | 1996-11-19 | Nikko Kinzoku Kk | 高導電性銅合金の製造方法 |
JPH10193059A (ja) | 1997-01-16 | 1998-07-28 | Furukawa Electric Co Ltd:The | 連続鋳造装置および前記装置を用いた合金の連続鋳造方法 |
JP2002003964A (ja) * | 2000-06-27 | 2002-01-09 | Chiba Inst Of Technology | 高い曲げ疲労特性を有する銅合金線、棒、帯等の長尺体及びその製造方法 |
JP2002086251A (ja) | 2000-09-13 | 2002-03-26 | Hitachi Cable Ltd | 合金の連続鋳造方法 |
JP2006341268A (ja) | 2005-06-08 | 2006-12-21 | Mitsubishi Materials Corp | 銅合金の連続製造装置及び銅合金の連続製造方法 |
JP2007146226A (ja) | 2005-11-28 | 2007-06-14 | Jfe Steel Kk | 拡管性に優れた油井管用ステンレス鋼管 |
JP2007311616A (ja) | 2006-05-19 | 2007-11-29 | Seiko Epson Corp | 面発光レーザおよびその製造方法 |
JP2008302813A (ja) | 2007-06-07 | 2008-12-18 | Honda Motor Co Ltd | ストラット式サスペンション装置 |
Family Cites Families (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3752753A (en) * | 1971-04-30 | 1973-08-14 | G Fitterer | Method of fabricating a sensor for the determination of the oxygen content of liquid metals |
JPS55128353A (en) | 1979-03-28 | 1980-10-04 | Hitachi Seisen Kk | Manufacture of copper alloy wire |
JPH0723092Y2 (ja) * | 1989-06-01 | 1995-05-31 | 三菱マテリアル株式会社 | 連続鋳造装置 |
JPH0462461A (ja) * | 1990-06-29 | 1992-02-27 | Mitsubishi Materials Corp | 銅融体中のりんの定量方法 |
EP0470608B1 (en) * | 1990-08-09 | 1999-11-24 | Nippon Steel Corporation | Method and apparatus for continuous casting |
TW297788B (ja) * | 1994-12-15 | 1997-02-11 | Sumitomo Metal Ind | |
US6022421A (en) * | 1998-03-03 | 2000-02-08 | Sonsub International, Inc, | Method for remotely launching subsea pigs in response to wellhead pressure change |
US6769152B1 (en) * | 2002-06-19 | 2004-08-03 | Parnell Consultants, Inc. | Launcher for passing a pig into a pipeline |
US7481239B2 (en) * | 2004-11-02 | 2009-01-27 | Stinger Wellhead Protection, Inc. | Gate valve with replaceable inserts |
DE112006003294B4 (de) * | 2005-12-05 | 2019-02-21 | Ulvac, Inc. | Dampfabscheidungsvorrichtung |
CN1987441A (zh) * | 2006-12-13 | 2007-06-27 | 陈欢 | 一种检测再生铜线材材质的方法 |
-
2008
- 2008-11-27 JP JP2008302813A patent/JP5224363B2/ja active Active
- 2008-11-28 WO PCT/JP2008/071726 patent/WO2009069782A1/ja active Application Filing
- 2008-11-28 CN CN2008801180362A patent/CN101878079B/zh not_active Expired - Fee Related
- 2008-11-28 US US12/745,518 patent/US8201614B2/en not_active Expired - Fee Related
- 2008-11-28 EP EP08854593.4A patent/EP2226138A4/en not_active Withdrawn
- 2008-11-28 TW TW097146150A patent/TWI391192B/zh not_active IP Right Cessation
- 2008-11-28 KR KR1020107012570A patent/KR20100097681A/ko not_active Application Discontinuation
Patent Citations (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5865554A (ja) | 1981-10-14 | 1983-04-19 | Sumitomo Electric Ind Ltd | 導電用合金の連続鋳造圧延方法 |
JPS59171834A (ja) | 1983-03-03 | 1984-09-28 | リムカ・リサ−チ・インコ−ポレ−テツド | 溶融金属内の粒子の検出測定方法並びに装置 |
JPS59169654A (ja) | 1983-03-15 | 1984-09-25 | Kawasaki Steel Corp | 溶融金属の化学成分調整方法 |
JPH05277641A (ja) | 1992-04-03 | 1993-10-26 | Nippon Steel Corp | 複層金属材の連続鋳造方法 |
JPH0663710A (ja) | 1992-08-12 | 1994-03-08 | Hitachi Cable Ltd | 連続鋳造装置 |
JPH08300119A (ja) | 1995-05-08 | 1996-11-19 | Nikko Kinzoku Kk | 高導電性銅合金の製造方法 |
JPH10193059A (ja) | 1997-01-16 | 1998-07-28 | Furukawa Electric Co Ltd:The | 連続鋳造装置および前記装置を用いた合金の連続鋳造方法 |
JP2002003964A (ja) * | 2000-06-27 | 2002-01-09 | Chiba Inst Of Technology | 高い曲げ疲労特性を有する銅合金線、棒、帯等の長尺体及びその製造方法 |
JP2002086251A (ja) | 2000-09-13 | 2002-03-26 | Hitachi Cable Ltd | 合金の連続鋳造方法 |
JP2006341268A (ja) | 2005-06-08 | 2006-12-21 | Mitsubishi Materials Corp | 銅合金の連続製造装置及び銅合金の連続製造方法 |
JP2007146226A (ja) | 2005-11-28 | 2007-06-14 | Jfe Steel Kk | 拡管性に優れた油井管用ステンレス鋼管 |
JP2007311616A (ja) | 2006-05-19 | 2007-11-29 | Seiko Epson Corp | 面発光レーザおよびその製造方法 |
JP2008302813A (ja) | 2007-06-07 | 2008-12-18 | Honda Motor Co Ltd | ストラット式サスペンション装置 |
Non-Patent Citations (3)
Title |
---|
KITA; MORITA; MATSUMOTO: "Specific resistance measurement of molten Cu-In-Sn alloy", THE SUMMARY OF THE SPEECH IN THE JAPANESE INSTITUTE OF METALS, vol. 86, 1980, pages 166 |
MORI, SANO, JOURNAL OF TETSU-TO-HAGANE, vol. 67, 1981, pages 672 - 695 |
See also references of EP2226138A4 |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
RU191826U1 (ru) * | 2018-11-22 | 2019-08-23 | Федеральное государственное автономное образовательное учреждение высшего образования "Уральский федеральный университет имени первого Президента России Б.Н. Ельцина" | Устройство фиксации нагревателя в электропечи |
Also Published As
Publication number | Publication date |
---|---|
KR20100097681A (ko) | 2010-09-03 |
CN101878079B (zh) | 2012-12-19 |
TW200932400A (en) | 2009-08-01 |
CN101878079A (zh) | 2010-11-03 |
TWI391192B (zh) | 2013-04-01 |
EP2226138A1 (en) | 2010-09-08 |
US20100307711A1 (en) | 2010-12-09 |
JP5224363B2 (ja) | 2013-07-03 |
US8201614B2 (en) | 2012-06-19 |
JP2009148824A (ja) | 2009-07-09 |
EP2226138A4 (en) | 2014-11-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
WO2009069782A1 (ja) | 連続鋳造中の溶融金属の成分調製方法及びその装置 | |
TW200611761A (en) | Process and apparatus for the continuous production of a thin metal strip | |
PL1824617T3 (pl) | Sposób odlewania z walcowaniem, o podwyższonej szybkości odlewania i następującym po nim walcowaniem na gorąco stosunkowo cienkich pasm metalu, zwłaszcza materiału stalowego, oraz zespół odlewniczo-walcowniczy | |
WO2007048240A3 (en) | In-line salt refining of molten aluminium alloys | |
WO2009149013A3 (en) | Compositions comprising nanomaterials and method for using such compositions for histochemical processes | |
EP2032727A4 (en) | METHOD, APPARATUS AND MEANS FOR PRODUCING METALS IN A MELTING LIQUID SALT AS ELECTROLYTES | |
UA95129C2 (ru) | Способ для поддержания, по крайней мере, частично ручного управления прокатным станом металлообработки | |
WO2006032347A3 (de) | Verfahren und einrichtung zum herstellen von flüssigem stahl | |
WO2007015131A3 (en) | An electrode and a method for forming an electrode | |
WO2014127921A3 (en) | Submerged entry nozzle | |
WO2005123304A3 (de) | Giessverfahren und giessanlage für aluminium bzw. aluminiumlegierungen | |
Tao et al. | Prediction of molten steel end point temperature in LF based on modified artificial neural network. | |
Hu et al. | Progress on single crystals of refractory metals of their alloys. | |
ZA201002933B (en) | Method and device for equalizing the solidification process of a fusible metal,particularly produced by means of strand or strip casting | |
Shang et al. | Sources and control of inclusions in billets. | |
Tan et al. | Intelligent temperature prediction model for plate rolling. | |
Pascual | Emerging melt quality control solution technologies for aluminium melt | |
Chang et al. | Method of controlling solidification quality in electroslag remelting process | |
He et al. | Improvement of central segregation in SWRH 82 B continuous casting bloom. | |
WO2013102922A3 (en) | An apparatus and a method of controlling glass sheet thickness | |
Yao et al. | Heat flux in mold for continuous casting round billet. | |
WO2009107119A3 (en) | System and method for reduction of heat treatment in metal casts | |
Kruse | Heating up for Strength | |
TH100390A (th) | วิธีการและเครื่องสำหรับการควบคุมสารผสมเคมีของโลหะหลอมเหลวในระหว่างการเทหล่อต่อเนื่อง | |
Singh et al. | CHARACTERIZATION OF MOLD FLUXES FOR CONTINUOUS CASTING OF STEELS |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
WWE | Wipo information: entry into national phase |
Ref document number: 200880118036.2 Country of ref document: CN |
|
121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 08854593 Country of ref document: EP Kind code of ref document: A1 |
|
WWE | Wipo information: entry into national phase |
Ref document number: 12745518 Country of ref document: US |
|
NENP | Non-entry into the national phase |
Ref country code: DE |
|
WWE | Wipo information: entry into national phase |
Ref document number: 2008854593 Country of ref document: EP |
|
ENP | Entry into the national phase |
Ref document number: 20107012570 Country of ref document: KR Kind code of ref document: A |
|
WWE | Wipo information: entry into national phase |
Ref document number: 3601/CHENP/2010 Country of ref document: IN |
|
WWE | Wipo information: entry into national phase |
Ref document number: PI 2010002488 Country of ref document: MY |