WO2000034760A1 - Electrochemical noise technique for corrosion - Google Patents
Electrochemical noise technique for corrosion Download PDFInfo
- Publication number
- WO2000034760A1 WO2000034760A1 PCT/US1999/029203 US9929203W WO0034760A1 WO 2000034760 A1 WO2000034760 A1 WO 2000034760A1 US 9929203 W US9929203 W US 9929203W WO 0034760 A1 WO0034760 A1 WO 0034760A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- electrode
- potential
- current
- working electrode
- working
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Links
Classifications
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N17/00—Investigating resistance of materials to the weather, to corrosion, or to light
- G01N17/02—Electrochemical measuring systems for weathering, corrosion or corrosion-protection measurement
Definitions
- the present invention relates to an electrochemical noise technique for determining corrosion rate.
- Electrochemical noise may be defined as the spontaneous fluctuations of current and potential generated by corrosion reactions.
- Various methods have been used to detect corrosion reactions, including a linear polarization resistance method in which a direct current (DC) signal is applied to a corroding cell consisting of two or three electrodes and the resulting DC polarization is monitored. Provided that the applied current is small so that the potential shift is less than 20 millivolts (mV), the response is linear in most cases and the measured resistance, commonly known as the polarization resistance, may be related inversely to the rate of the uniform corrosion attack.
- DC direct current
- mV millivolts
- U.S. Patent No. 5,139,627 to Eden et al. discloses a system which employs two working electrodes fabricated with the same material and exposed to the same corrosion conditions as the metallic surface to be tested. This system further employs means for measuring the coupling current between the working electrodes, means for measuring electrochemical potential noise originating from the electrodes, and means for comparing the coupling current with the electrochemical current noise to provide an output indicative of the degree to which corrosion is localized.
- Eden et al. utilize open circuit potential conditions, employing two working electrodes in an electrolyte environment wherein both electrodes are short circuited with a low resistance amp meter. The current between these two working electrodes is the result of corrosion occurring on them, with the measurement of the net current relating to the corrosion on both of them.
- the present invention relates to an electrochemical noise method for determining the corrosion rate of a conductive article, comprising: placing a working electrode, reference electrode, and counter electrode in a corrosive environment of interest, wherein said working electrode has substantially the same composition as the article; measuring potential at open circuit between the working electrode and the reference electrode over a first period of time; placing the working electrode under a potentiostatic control; and measuring current between the working electrode and the counter electrode for second period of time.
- the present invention further relates to a working electrode which is composed of the material of interest; a counter electrode which is inert in an environment of interest; a reference electrode which is inert in the environment of interest; and a measurement system connected to said working electrode, counter electrode, and said reference electrode, wherein said measurement system is capable of monitoring potential between said working electrode and said reference electrode and monitoring current between said counting electrode and said working electrode.
- Figure 1 is a schematic of one embodiment of the electrochemical noise system of the present invention.
- Figure 2 is a schematic of another embodiment of the electrochemical noise system of the present invention.
- Figure 3 is a graphical representation of potential/current versus time raw data plot for potentiostatic ECN in brine/air.
- Figure 4 is a graphical representation of potential/current noise data versus time raw data plot for potentiostatic ECN in brine/air.
- Figure 5 is a graphical representation comparing potentiostatic ECN and zero resistant ammeter mode in brine/air solution for voltage versus time.
- Figure 6 is a graphical representation comparing potentiostatic ECN and zero resistant ammeter mode in brine/air solution for current versus time.
- Figure 7 is a graphical representation of potential versus time showing the effect of flow on current/potential noise in brine/carbon dioxide solution.
- Figure 8 is a graphical representation of current versus time showing the effect of flow on current/potential noise in brine/carbon dioxide solution.
- Figure 9 is a graphical representation of potential versus time showing the effect of quaternary amine inhibitor on current/potential noise in brine/carbon dioxide solution.
- Figure 10 is a graphical representation of current versus time showing the effect of quaternary amine inhibitor on current/potential noise in brine/carbon dioxide solution.
- the present invention relates to determining corrosion rate on a metallic surface using a unique electrochemical noise technique.
- the working electrode is fabricated from the same material as the item of concern (i.e. the component, article).
- the material is a metal or metal alloy.
- the counter electrode can be formed of any material, including the same material as the working electrode, the counter electrode preferably comprises material which is inert in the particular environment of interest.
- the counter electrode may be platinum, nickel- based (e.g., Hastalloy C276), iron based (e.g., stainless steel) or a chromium-based alloy, or mixtures and alloys thereof, or any other electrically conductive, non- corrosive material.
- the reference electrode can comprise any material, but preferably comprises an inert, electrically conductive material which may be the same or a different material as employed by the counter electrode.
- the working, counter, and reference electrodes are disposed in the same environment as the component of interest, in a spaced relation to one another.
- a potential between the working and reference electrodes is measured first at open circuit potential for a certain period of time.
- the period of time which can be any length of time, is typically less than 1 minute, and preferably less than about 10 seconds (sec), with less than about 1 sec. especially preferred for convenience and reduced testing time.
- a potential equivalent to the measured potential at that time is then applied to the working electrode by switching from open circuit to potentiostatic control.
- the current between the working electrode and the counter electrode can be measured for a second period (although this second period of time can be any period, the same amount of time is preferred). A new cycle can then be performed after the potentiostatic current measurement.
- the measured potential and current noise can then be utilized to determine the general and localized corrosion rate using conventional calculation techniques which typically use the average current (root mean square (RMS;) and average potential (RMSv) and standard deviation of current ( ⁇ i).
- RMS root mean square
- RMSv average potential
- ⁇ i standard deviation of current
- general corrosion (I corr ) is known to be related to resistance noise (R N ) as follows:
- a working electrode 3 is disposed between and in spaced relation to both reference electrode 1 and counter electrode 5.
- the counter electrode 5 and working electrode 3 are connected to a potentiostat 7 which feeds into comparator 17 (R N ) and a localized corrosion measurement device 15 capable of measuring localized corrosion as a function of time.
- reference electrode 1 and working electrode 3 are connected to electrochemical potential noise monitoring apparatus 9 (i.e., voltmeter) which feeds into comparator 17 and power density analyzer 11. From that input, in combination with input from the electrochemical current noise measuring apparatus 7, localized corrosion rate can be determined.
- Electrochemical potential noise monitoring apparatus 9 additionally feeds input to comparator 17 to determine general corrosion rate as a function of time.
- EXAMPLE 1 The following example is the measurement of corrosion rate for a mild steel (e.g., ASTM steel C1018) in a mixture of brine, hydrocarbon, and carbon dioxide environment using the embodiment shown in Figure 1.
- the counter and reference electrodes are Hastalloy C276 (commercially available from Metal Samples, Inc., GA), while the working electrode is mild steel C1018.
- EXAMPLE 2 The current and potential noise data were sampled between a 1 and 60 second period with current being measured when potential was held and the potential measured with the current open-circuit.
- the standard mode of operation used the system illustrated in Figure 2, and consisted of the following sequence:
- Figure 3 shows the potential/current versus time curves in a brine/air solution obtained with the potentiostatic EC ⁇ (P-EC ⁇ ) technique.
- the time periods chosen for this test were A equals 40 seconds, B equals 40 seconds, and C equals 0.
- A the potential was measured and the current was zero.
- B the potential was constant (potential noise value) and the current was measured.
- the initial increase in current was due to the double layer capacitive current followed by a continuous increase/decrease in anodic/cathodic current.
- the first value after the initial current increase was recorded (current noise) and plotted together with the potential noise as shown in Figure 4.
- the potentiostatic EC ⁇ technique was further evaluated for the effect of stirring and the addition of a corrosion inhibitor on current and potential noise in a carbon dioxide (CO )-containing brine solution.
- the parameters used in this study were, A equals 1 second, B equals 10 seconds, C equals 0 seconds.
- Figures 7 and 8 show the current and potential noise in the brine/CO 2 solution with and without stirring obtained using the potentiostatic ECN technique. It can be seen that stirring (at about 100 revolutions per minute (rpm) or less) has a significant effect on current and potential noise resulting in ten-fold reduction in fluctuations (i.e. standard deviations). The rms of current noise was also decreased by a similar amount. Thus, the changes in current and potential fluctuations with time were related to changes in flow rate/flow regime in this particular system. The effect of an inhibitor (e.g. quaternary amine) on the current and potential noise in stirred brine/CO 2 solution was shown in Figures 9 and 10.
- an inhibitor e.g. quaternary amine
- the system of the present invention can be further simplified by automating the system using an appropriate computer system and software.
- the software should be able to control all necessary switching and measurements as described herein. By automating the current system, error introduced due to human interaction and delay can be eliminated.
- the present invention is a simplified corrosion measurement system and method. Unlike the prior art which requires the use of two identical working electrodes formed of the same material as the article, the present invention utilizes one working electrode (different counter and reference electrodes), thereby eliminating error created by differences between the electrodes since all the measured data are from the same electrode. Additional advantages include that there is an improved correlation between the current and potential noise (i.e. same source); corrosion rate is measured at open circuit potential (OCP) without disturbing the system; and there is little or no loss of long-term current/potential drift signal (DC components).
- OCP open circuit potential
- the present invention can be utilized to determine corrosion rate in applications where the use of the two working electrode system is, if not impossible, at least impractical, such as rotating disc and rotating cylinder electrode systems, or any other high shear environment. Additionally, in the two working electrode system, it was unknown which electrode was corroding and thereby providing the data. In the present system, it is clearly established where the data originates, allowing good correlation between current and potential noise to be established. Finally, unlike the prior art, the size and geometry of the working electrode of the present invention is not limited.
Landscapes
- Life Sciences & Earth Sciences (AREA)
- General Health & Medical Sciences (AREA)
- General Physics & Mathematics (AREA)
- Environmental & Geological Engineering (AREA)
- Biodiversity & Conservation Biology (AREA)
- Physics & Mathematics (AREA)
- Health & Medical Sciences (AREA)
- Chemical & Material Sciences (AREA)
- Analytical Chemistry (AREA)
- Ecology (AREA)
- Biochemistry (AREA)
- Environmental Sciences (AREA)
- Immunology (AREA)
- Pathology (AREA)
- Testing Resistance To Weather, Investigating Materials By Mechanical Methods (AREA)
- Secondary Cells (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Prevention Of Electric Corrosion (AREA)
- Investigating And Analyzing Materials By Characteristic Methods (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (10)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CA002353946A CA2353946C (en) | 1998-12-10 | 1999-12-09 | Electrochemical noise technique for corrosion |
| BR9915977-5A BR9915977A (pt) | 1998-12-10 | 1999-12-09 | Método de ruìdo eletroquìmico e sistema de medição para determinar a taxa de corrosão de um artigo eletricamente condutor |
| DE69915679T DE69915679T2 (de) | 1998-12-10 | 1999-12-09 | Verfahren und system zur korrosionsmessung durch ermittlung des elektrochemischen rauschens |
| JP2000587169A JP2002532681A (ja) | 1998-12-10 | 1999-12-09 | 腐食用電気化学的ノイズ技術 |
| MXPA01005642A MXPA01005642A (es) | 1998-12-10 | 1999-12-09 | Tecnica de ruido electroquimico para corrosion. |
| AU24788/00A AU758336B2 (en) | 1998-12-10 | 1999-12-09 | Electrochemical noise technique for corrosion |
| EP99968103A EP1137926B1 (en) | 1998-12-10 | 1999-12-09 | Electrochemical noise technique for corrosion |
| DK99968103T DK1137926T3 (da) | 1998-12-10 | 1999-12-09 | Elektrokemisk stöjteknik til korrosion |
| AT99968103T ATE262169T1 (de) | 1998-12-10 | 1999-12-09 | Verfahren und system zur korrosionsmessung durch ermittlung des elektrochemischen rauschens |
| NO20012499A NO319344B1 (no) | 1998-12-10 | 2001-05-21 | Elektrokjemisk stoyteknikk for korrosjon |
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US11173598P | 1998-12-10 | 1998-12-10 | |
| US60/111,735 | 1998-12-10 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| WO2000034760A1 true WO2000034760A1 (en) | 2000-06-15 |
Family
ID=22340173
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PCT/US1999/029203 Ceased WO2000034760A1 (en) | 1998-12-10 | 1999-12-09 | Electrochemical noise technique for corrosion |
Country Status (16)
| Country | Link |
|---|---|
| US (1) | US6280603B1 (enExample) |
| EP (1) | EP1137926B1 (enExample) |
| JP (1) | JP2002532681A (enExample) |
| CN (1) | CN100385231C (enExample) |
| AT (1) | ATE262169T1 (enExample) |
| AU (1) | AU758336B2 (enExample) |
| BR (1) | BR9915977A (enExample) |
| CA (1) | CA2353946C (enExample) |
| DE (1) | DE69915679T2 (enExample) |
| DK (1) | DK1137926T3 (enExample) |
| ES (1) | ES2220142T3 (enExample) |
| ID (1) | ID28879A (enExample) |
| MX (1) | MXPA01005642A (enExample) |
| NO (1) | NO319344B1 (enExample) |
| RU (1) | RU2222001C2 (enExample) |
| WO (1) | WO2000034760A1 (enExample) |
Cited By (23)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2001098753A1 (en) * | 2000-06-23 | 2001-12-27 | Eric Atherton | Corrosion monitoring |
| WO2001098752A3 (en) * | 2000-06-22 | 2002-08-29 | United States Filter Corp | Process for real-time detection and inhibition of localized corrosion |
| WO2001098218A3 (en) * | 2000-06-22 | 2002-09-12 | United States Filter Corp | Dynamic optimization of chemical additives in a water treatment system |
| US6716359B1 (en) | 2000-08-29 | 2004-04-06 | United States Filter Corporation | Enhanced time-based proportional control |
| US6776926B2 (en) | 2001-08-09 | 2004-08-17 | United States Filter Corporation | Calcium hypochlorite of reduced reactivity |
| US6991735B2 (en) | 2002-02-26 | 2006-01-31 | Usfilter Corporation | Free radical generator and method |
| US7108781B2 (en) | 2002-02-26 | 2006-09-19 | Usfilter Corporation | Enhanced air and water purification using continuous breakpoint halogenation with free oxygen radicals |
| CN101419153B (zh) * | 2007-10-24 | 2011-05-25 | 同济大学 | 一种测量抗氯离子侵蚀能力的自动采集多通道加速腐蚀试验装置 |
| US8591730B2 (en) | 2009-07-30 | 2013-11-26 | Siemens Pte. Ltd. | Baffle plates for an ultraviolet reactor |
| US8652336B2 (en) | 2006-06-06 | 2014-02-18 | Siemens Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
| US8741155B2 (en) | 2007-04-03 | 2014-06-03 | Evoqua Water Technologies Llc | Method and system for providing ultrapure water |
| US8753522B2 (en) | 2007-04-03 | 2014-06-17 | Evoqua Water Technologies Llc | System for controlling introduction of a reducing agent to a liquid stream |
| US8877067B2 (en) | 2011-05-26 | 2014-11-04 | Evoqua Water Technologies Llc | Method and arrangement for a water treatment |
| US8961798B2 (en) | 2007-04-03 | 2015-02-24 | Evoqua Water Technologies Llc | Method for measuring a concentration of a compound in a liquid stream |
| CN104502266A (zh) * | 2014-12-31 | 2015-04-08 | 天津大学 | 一种基于熵率的电化学噪声腐蚀信号处理方法 |
| US9365435B2 (en) | 2007-04-03 | 2016-06-14 | Evoqua Water Technologies Llc | Actinic radiation reactor |
| US9365436B2 (en) | 2007-04-03 | 2016-06-14 | Evoqua Water Technologies Llc | Method of irradiating a liquid |
| US9725343B2 (en) | 2007-04-03 | 2017-08-08 | Evoqua Water Technologies Llc | System and method for measuring and treating a liquid stream |
| JP2018205124A (ja) * | 2017-06-05 | 2018-12-27 | 日本電信電話株式会社 | 腐食速度測定装置及び腐食速度測定方法 |
| US10343939B2 (en) | 2006-06-06 | 2019-07-09 | Evoqua Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
| US10494281B2 (en) | 2015-01-21 | 2019-12-03 | Evoqua Water Technologies Llc | Advanced oxidation process for ex-situ groundwater remediation |
| US11161762B2 (en) | 2015-01-21 | 2021-11-02 | Evoqua Water Technologies Llc | Advanced oxidation process for ex-situ groundwater remediation |
| US12103874B2 (en) | 2006-06-06 | 2024-10-01 | Evoqua Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
Families Citing this family (36)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3777934B2 (ja) * | 2000-01-26 | 2006-05-24 | 三菱化学株式会社 | 非水系有機液中における腐食測定方法及びその測定装置 |
| US6611151B1 (en) * | 2000-09-21 | 2003-08-26 | The United States Of America As Represented By The Secretary Of The Navy | Coating assessment system based on electrochemical noise |
| AU2002254772A1 (en) * | 2001-05-02 | 2002-11-11 | Mmfx Technologies Corporation | Determination of chloride corrosion threshold for metals embedded in cementitious material |
| JP4581306B2 (ja) * | 2001-09-03 | 2010-11-17 | 栗田工業株式会社 | 炭素鋼の局部腐食モニタリング方法及び炭素鋼の局部腐食防止方法 |
| DK200201401A (da) * | 2002-09-24 | 2004-03-25 | Guldager As | Reference-elektrode |
| US7622030B2 (en) | 2004-03-26 | 2009-11-24 | Baker Hughes Incorporated | General and localized corrosion rate measurements |
| US7368050B2 (en) * | 2004-03-26 | 2008-05-06 | Baker Hughes Incorporated | Quantitative transient analysis of localized corrosion |
| US7713405B2 (en) * | 2004-03-26 | 2010-05-11 | Baker Hughes Incorporated | Quantitative transient analysis of localized corrosion |
| GB2420856B (en) * | 2004-12-03 | 2009-07-01 | Capcis Ltd | Measurement of corrosivity |
| US20070120572A1 (en) * | 2005-11-30 | 2007-05-31 | Weiguo Chen | Smart coupon for realtime corrosion detection |
| US7388386B2 (en) * | 2006-03-31 | 2008-06-17 | General Electric Company | Method and apparatus for corrosion detection |
| US7245132B1 (en) | 2006-07-12 | 2007-07-17 | Pepperl & Fuchs, Inc. | Intrinsically safe corrosion measurement and history logging field device |
| US7239156B1 (en) | 2006-07-13 | 2007-07-03 | Pepperl & Fuchs, Inc. | Configurable corrosion measurement field device |
| US7282928B1 (en) | 2006-07-13 | 2007-10-16 | Pepperl & Fuchs, Inc. | Corrosion measurement field device with improved LPF, HDA, and ECN capability |
| JP5226975B2 (ja) * | 2007-06-28 | 2013-07-03 | 日立Geニュークリア・エナジー株式会社 | 応力腐食割れ監視方法及びその監視装置 |
| CN101144769B (zh) * | 2007-09-29 | 2010-08-18 | 哈尔滨工业大学 | 五电极钢筋锈蚀监测传感器及其制备方法 |
| US7719292B2 (en) * | 2007-10-12 | 2010-05-18 | Honeywell International Inc. | Method and apparatus for electrochemical corrosion monitoring |
| US8133383B2 (en) | 2008-01-23 | 2012-03-13 | Baker Hughes Incorporated | Localized corrosion monitoring device for limited conductivity fluids |
| CN101918822B (zh) * | 2008-03-27 | 2013-04-03 | 松下电器产业株式会社 | 测定装置、测定系统和浓度测定方法 |
| CN102132162A (zh) * | 2008-07-02 | 2011-07-20 | 倍加福公司 | 作为局部腐蚀指示器的电化学噪声 |
| CN101620062B (zh) * | 2008-07-03 | 2011-11-16 | 同济大学 | 氯盐腐蚀混凝土中钢筋加速锈蚀控制试验方法 |
| JP5421833B2 (ja) * | 2010-03-25 | 2014-02-19 | 株式会社神戸製鋼所 | 金属材料の腐食速度の推定方法 |
| CN103323520B (zh) * | 2013-05-31 | 2016-05-04 | 哈尔滨工程大学 | 利用电化学噪声技术测量材料局部腐蚀的方法及噪声探头和制法 |
| AU2015229218B2 (en) | 2014-03-14 | 2017-12-07 | Rosemount Inc. | Corrosion rate measurement |
| US10830689B2 (en) | 2014-09-30 | 2020-11-10 | Rosemount Inc. | Corrosion rate measurement using sacrificial probe |
| US9726594B2 (en) | 2014-11-18 | 2017-08-08 | Baker Hughes Incorporated | Electrochemical sensor for monitoring under-deposit corrosion |
| CN104502267A (zh) * | 2014-12-31 | 2015-04-08 | 天津大学 | 一种基于支持向量机的电化学噪声腐蚀类型判别方法 |
| CN104502265A (zh) * | 2014-12-31 | 2015-04-08 | 天津大学 | 一种常温常压下的电化学噪声实验方法 |
| US10190968B2 (en) | 2015-06-26 | 2019-01-29 | Rosemount Inc. | Corrosion rate measurement with multivariable sensor |
| CN105547988A (zh) * | 2016-01-08 | 2016-05-04 | 海南瑞泽新型建材股份有限公司 | 钢筋混凝土锈蚀试验装置及试验方法 |
| RU2695961C1 (ru) * | 2018-09-26 | 2019-07-29 | Анна Владимировна Родькина | Комплекс для исследования электрохимических характеристик корпусных конструкций судов и плавучих технических сооружений |
| RU2743885C1 (ru) * | 2020-08-05 | 2021-03-01 | Общество с ограниченной ответственностью «Техохрана» | Способ и устройство обнаружения участков перезащиты металла трубопровода |
| RU2750847C1 (ru) * | 2020-10-21 | 2021-07-05 | Общество с ограниченной ответственностью "Техохрана" | Способ и устройство стабилизации электродного потенциала безэлектролитного электрода сравнения |
| JP7558897B2 (ja) * | 2021-06-10 | 2024-10-01 | 株式会社日本製鋼所 | 試験装置および試験方法 |
| CN116046661B (zh) * | 2022-12-26 | 2025-12-02 | 中国石油大学(华东) | 一种电化学噪声测试系统以及测试方法 |
| CN119804599B (zh) * | 2024-12-12 | 2025-11-11 | 中国科学院金属研究所 | 一种混凝土中钢筋锈蚀过程监测与判别方法 |
Citations (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3716460A (en) * | 1971-06-21 | 1973-02-13 | Betz Laboratories | Method for determining corrosion rate and meter therefor |
| SU1469431A1 (ru) * | 1987-04-24 | 1989-03-30 | Предприятие П/Я А-7629 | Устройство дл регулировани потенциала электрода при электрохимических исследовани х |
| GB2218521A (en) * | 1988-05-13 | 1989-11-15 | Applied Corrosion Monitoring L | Multichannel corrosion rate measurement apparatus |
| US5139627A (en) * | 1986-05-12 | 1992-08-18 | Capcis Limited | Corrosion monitoring |
| WO1998050786A1 (en) * | 1997-05-08 | 1998-11-12 | The University Of Chicago | An in-situ process for the monitoring of localized pitting corrosion |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| SU1290147A1 (ru) * | 1984-01-02 | 1987-02-15 | Северо-Кавказский научно-исследовательский институт природных газов | Способ определени скорости коррозии углеродистой стали |
| GB2258535A (en) * | 1991-08-03 | 1993-02-10 | British Aerospace | Corrosion sensors |
| US5275704A (en) * | 1992-10-16 | 1994-01-04 | Nalco Chemical Company | Method and apparatus for measuring underdeposit localized corrosion rate or metal corrosion rate under tubercles in cooling water systems |
| CN2238433Y (zh) * | 1995-05-08 | 1996-10-23 | 中国科学院金属腐蚀与防护研究所 | 金属腐蚀速度测量仪 |
| JPH09297117A (ja) * | 1996-04-30 | 1997-11-18 | Mitsubishi Chem Corp | 金属材質の腐食測定装置 |
| RU2094773C1 (ru) * | 1996-05-23 | 1997-10-27 | Всероссийский научно-исследовательский институт природных газов и газовых технологий "ВНИИГАЗ" | Способ измерения скорости коррозии металлов и сплавов |
| JP3508430B2 (ja) * | 1996-11-22 | 2004-03-22 | 三菱化学株式会社 | 冷却塔の循環冷却水の水質管理支援装置 |
-
1999
- 1999-12-09 JP JP2000587169A patent/JP2002532681A/ja active Pending
- 1999-12-09 EP EP99968103A patent/EP1137926B1/en not_active Expired - Lifetime
- 1999-12-09 WO PCT/US1999/029203 patent/WO2000034760A1/en not_active Ceased
- 1999-12-09 ES ES99968103T patent/ES2220142T3/es not_active Expired - Lifetime
- 1999-12-09 RU RU2001119059/28A patent/RU2222001C2/ru not_active IP Right Cessation
- 1999-12-09 BR BR9915977-5A patent/BR9915977A/pt not_active Application Discontinuation
- 1999-12-09 DK DK99968103T patent/DK1137926T3/da active
- 1999-12-09 US US09/457,986 patent/US6280603B1/en not_active Expired - Lifetime
- 1999-12-09 DE DE69915679T patent/DE69915679T2/de not_active Expired - Lifetime
- 1999-12-09 MX MXPA01005642A patent/MXPA01005642A/es not_active IP Right Cessation
- 1999-12-09 CN CNB998138681A patent/CN100385231C/zh not_active Expired - Fee Related
- 1999-12-09 ID IDW00200101238A patent/ID28879A/id unknown
- 1999-12-09 AT AT99968103T patent/ATE262169T1/de active
- 1999-12-09 AU AU24788/00A patent/AU758336B2/en not_active Ceased
- 1999-12-09 CA CA002353946A patent/CA2353946C/en not_active Expired - Fee Related
-
2001
- 2001-05-21 NO NO20012499A patent/NO319344B1/no not_active IP Right Cessation
Patent Citations (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3716460A (en) * | 1971-06-21 | 1973-02-13 | Betz Laboratories | Method for determining corrosion rate and meter therefor |
| US5139627A (en) * | 1986-05-12 | 1992-08-18 | Capcis Limited | Corrosion monitoring |
| SU1469431A1 (ru) * | 1987-04-24 | 1989-03-30 | Предприятие П/Я А-7629 | Устройство дл регулировани потенциала электрода при электрохимических исследовани х |
| GB2218521A (en) * | 1988-05-13 | 1989-11-15 | Applied Corrosion Monitoring L | Multichannel corrosion rate measurement apparatus |
| WO1998050786A1 (en) * | 1997-05-08 | 1998-11-12 | The University Of Chicago | An in-situ process for the monitoring of localized pitting corrosion |
Non-Patent Citations (1)
| Title |
|---|
| DATABASE WPI WORLD PATENT INF 1 January 1900 (1900-01-01), XP002137607, Database accession no. 90-020601 * |
Cited By (27)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2001098752A3 (en) * | 2000-06-22 | 2002-08-29 | United States Filter Corp | Process for real-time detection and inhibition of localized corrosion |
| WO2001098218A3 (en) * | 2000-06-22 | 2002-09-12 | United States Filter Corp | Dynamic optimization of chemical additives in a water treatment system |
| WO2001098753A1 (en) * | 2000-06-23 | 2001-12-27 | Eric Atherton | Corrosion monitoring |
| US6776889B2 (en) | 2000-06-23 | 2004-08-17 | Eric Atherton | Corrosion monitoring |
| US6716359B1 (en) | 2000-08-29 | 2004-04-06 | United States Filter Corporation | Enhanced time-based proportional control |
| US6776926B2 (en) | 2001-08-09 | 2004-08-17 | United States Filter Corporation | Calcium hypochlorite of reduced reactivity |
| US6991735B2 (en) | 2002-02-26 | 2006-01-31 | Usfilter Corporation | Free radical generator and method |
| US7108781B2 (en) | 2002-02-26 | 2006-09-19 | Usfilter Corporation | Enhanced air and water purification using continuous breakpoint halogenation with free oxygen radicals |
| US7285223B2 (en) | 2002-02-26 | 2007-10-23 | Siemens Water Technologies Holding Corp. | Enhanced air and water purification using continuous breakpoint halogenation with free oxygen radicals |
| US12103874B2 (en) | 2006-06-06 | 2024-10-01 | Evoqua Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
| US10550020B2 (en) | 2006-06-06 | 2020-02-04 | Evoqua Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
| US8652336B2 (en) | 2006-06-06 | 2014-02-18 | Siemens Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
| US10343939B2 (en) | 2006-06-06 | 2019-07-09 | Evoqua Water Technologies Llc | Ultraviolet light activated oxidation process for the reduction of organic carbon in semiconductor process water |
| US8741155B2 (en) | 2007-04-03 | 2014-06-03 | Evoqua Water Technologies Llc | Method and system for providing ultrapure water |
| US9764968B2 (en) | 2007-04-03 | 2017-09-19 | Evoqua Water Technologies Llc | Method and system for providing ultrapure water |
| US8961798B2 (en) | 2007-04-03 | 2015-02-24 | Evoqua Water Technologies Llc | Method for measuring a concentration of a compound in a liquid stream |
| US8753522B2 (en) | 2007-04-03 | 2014-06-17 | Evoqua Water Technologies Llc | System for controlling introduction of a reducing agent to a liquid stream |
| US9365435B2 (en) | 2007-04-03 | 2016-06-14 | Evoqua Water Technologies Llc | Actinic radiation reactor |
| US9365436B2 (en) | 2007-04-03 | 2016-06-14 | Evoqua Water Technologies Llc | Method of irradiating a liquid |
| US9725343B2 (en) | 2007-04-03 | 2017-08-08 | Evoqua Water Technologies Llc | System and method for measuring and treating a liquid stream |
| CN101419153B (zh) * | 2007-10-24 | 2011-05-25 | 同济大学 | 一种测量抗氯离子侵蚀能力的自动采集多通道加速腐蚀试验装置 |
| US8591730B2 (en) | 2009-07-30 | 2013-11-26 | Siemens Pte. Ltd. | Baffle plates for an ultraviolet reactor |
| US8877067B2 (en) | 2011-05-26 | 2014-11-04 | Evoqua Water Technologies Llc | Method and arrangement for a water treatment |
| CN104502266A (zh) * | 2014-12-31 | 2015-04-08 | 天津大学 | 一种基于熵率的电化学噪声腐蚀信号处理方法 |
| US10494281B2 (en) | 2015-01-21 | 2019-12-03 | Evoqua Water Technologies Llc | Advanced oxidation process for ex-situ groundwater remediation |
| US11161762B2 (en) | 2015-01-21 | 2021-11-02 | Evoqua Water Technologies Llc | Advanced oxidation process for ex-situ groundwater remediation |
| JP2018205124A (ja) * | 2017-06-05 | 2018-12-27 | 日本電信電話株式会社 | 腐食速度測定装置及び腐食速度測定方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| AU758336B2 (en) | 2003-03-20 |
| DE69915679D1 (de) | 2004-04-22 |
| MXPA01005642A (es) | 2003-07-14 |
| ATE262169T1 (de) | 2004-04-15 |
| DK1137926T3 (da) | 2004-07-26 |
| BR9915977A (pt) | 2001-09-11 |
| US6280603B1 (en) | 2001-08-28 |
| CA2353946A1 (en) | 2000-06-15 |
| DE69915679T2 (de) | 2005-02-17 |
| ES2220142T3 (es) | 2004-12-01 |
| CA2353946C (en) | 2004-02-24 |
| NO20012499L (no) | 2001-08-02 |
| EP1137926B1 (en) | 2004-03-17 |
| ID28879A (id) | 2001-07-12 |
| CN1338043A (zh) | 2002-02-27 |
| NO319344B1 (no) | 2005-07-18 |
| NO20012499D0 (no) | 2001-05-21 |
| JP2002532681A (ja) | 2002-10-02 |
| AU2478800A (en) | 2000-06-26 |
| CN100385231C (zh) | 2008-04-30 |
| RU2222001C2 (ru) | 2004-01-20 |
| EP1137926A1 (en) | 2001-10-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA2353946C (en) | Electrochemical noise technique for corrosion | |
| US6015484A (en) | Detection of pitting corrosion | |
| Chen et al. | Electrochemical emission spectroscopy for monitoring uniform and localized corrosion | |
| Gabrielli et al. | Review of applications of impedance and noise analysis to uniform and localized corrosion | |
| US7368050B2 (en) | Quantitative transient analysis of localized corrosion | |
| CA2711951C (en) | Localized corrosion monitoring device for limited conductivity fluids | |
| US5139627A (en) | Corrosion monitoring | |
| US5448178A (en) | Transient technique to determine solution resistance for simple and accurate corrosion rate measurements | |
| US7713405B2 (en) | Quantitative transient analysis of localized corrosion | |
| Dean Jr | Electrochemical methods of corrosion testing | |
| US7520975B2 (en) | Estimation of localised corrosion penetration | |
| Scully et al. | Methods for determining aqueous corrosion reaction rates | |
| Scully¹ | Electrochemical tests | |
| GB2365977A (en) | Corrosion monitoring system for use in multiple phase solutions | |
| JPH0726935B2 (ja) | ステンレス鋼l規格材の非破壊的簡易鑑別法 | |
| Jovancicevic et al. | Controlled Potentiostatic Measurements of Electrochemical Noise | |
| Denzine et al. | An improved, rapid corrosion rate measurement technique for all process environments | |
| Britton | Introduction to corrosion measurement techniques | |
| Silverman | Types of Data | |
| JPS61223545A (ja) | 材料の耐食性の評価試験方法 | |
| JPH01267447A (ja) | 局部腐食感受性試験方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| WWE | Wipo information: entry into national phase |
Ref document number: 99813868.1 Country of ref document: CN |
|
| AK | Designated states |
Kind code of ref document: A1 Designated state(s): AE AL AM AT AU AZ BA BB BG BR BY CA CH CN CR CU CZ DE DK DM EE ES FI GB GD GE GH GM HR HU ID IL IN IS JP KE KG KP KR KZ LC LK LR LS LT LU LV MA MD MG MK MN MW MX NO NZ PL PT RO RU SD SE SG SI SK SL TJ TM TR TT TZ UA UG US UZ VN YU ZA ZW |
|
| AL | Designated countries for regional patents |
Kind code of ref document: A1 Designated state(s): GH GM KE LS MW SD SL SZ TZ UG ZW AM AZ BY KG KZ MD RU TJ TM AT BE CH CY DE DK ES FI FR GB GR IE IT LU MC NL PT SE BF BJ CF CG CI CM GA GN GW ML MR NE SN TD TG |
|
| WD | Withdrawal of designations after international publication |
Free format text: US |
|
| 121 | Ep: the epo has been informed by wipo that ep was designated in this application | ||
| DFPE | Request for preliminary examination filed prior to expiration of 19th month from priority date (pct application filed before 20040101) | ||
| WWE | Wipo information: entry into national phase |
Ref document number: 24788/00 Country of ref document: AU |
|
| WWE | Wipo information: entry into national phase |
Ref document number: 1999968103 Country of ref document: EP |
|
| ENP | Entry into the national phase |
Ref document number: 2353946 Country of ref document: CA Ref document number: 2353946 Country of ref document: CA Kind code of ref document: A |
|
| WWE | Wipo information: entry into national phase |
Ref document number: PA/a/2001/005642 Country of ref document: MX |
|
| ENP | Entry into the national phase |
Ref document number: 2000 587169 Country of ref document: JP Kind code of ref document: A |
|
| WWP | Wipo information: published in national office |
Ref document number: 1999968103 Country of ref document: EP |
|
| REG | Reference to national code |
Ref country code: DE Ref legal event code: 8642 |
|
| WWG | Wipo information: grant in national office |
Ref document number: 24788/00 Country of ref document: AU |
|
| WWG | Wipo information: grant in national office |
Ref document number: 1999968103 Country of ref document: EP |