WO1997007377A2 - Vehicule blinde leger perfectionne et procede de fabrication correspondant - Google Patents

Vehicule blinde leger perfectionne et procede de fabrication correspondant Download PDF

Info

Publication number
WO1997007377A2
WO1997007377A2 PCT/US1996/013337 US9613337W WO9707377A2 WO 1997007377 A2 WO1997007377 A2 WO 1997007377A2 US 9613337 W US9613337 W US 9613337W WO 9707377 A2 WO9707377 A2 WO 9707377A2
Authority
WO
WIPO (PCT)
Prior art keywords
window
armored
armor
vehicle
curved
Prior art date
Application number
PCT/US1996/013337
Other languages
English (en)
Other versions
WO1997007377A3 (fr
Inventor
Richard C. Medlin
James E. Munn
Daniel T. Medlin
Melvin W. Floyd
Joe I. Wolfe
Original Assignee
Medlin Richard C
Munn James E
Medlin Daniel T
Floyd Melvin W
Wolfe Joe I
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Medlin Richard C, Munn James E, Medlin Daniel T, Floyd Melvin W, Wolfe Joe I filed Critical Medlin Richard C
Priority to AU70081/96A priority Critical patent/AU7008196A/en
Publication of WO1997007377A2 publication Critical patent/WO1997007377A2/fr
Publication of WO1997007377A3 publication Critical patent/WO1997007377A3/fr

Abstract

Cette invention concerne un véhicule blindé léger perfectionné (1) ainsi qu'un procédé d'un bon rapport efficacité/coût qui permet d'équiper a posteriori des automobiles standards pour les transformer en véhicules blindés légers. Des garnitures (133) et des tiges métalliques profilées, qui sont installées autour des vitres (131) en verre feuilleté pour protéger les bords du verre feuilleté des contraintes, de l'humidité et des éléments atmosphériques, peuvent être adaptées à un encadrement (135) de vitre d'une automobile standard. Des vitres (179) d'un autre type, en verre feuilleté, à l'épreuve des effractions, peuvent être adaptées à des encadrements des vitres d'origine d'une automobile standard. Un blindage opaque (11, 13, 15, 17, 19, 21, 205, 207) de faible poids, préfabriqué et formé rigidement, est moulé pour pouvoir être ajusté précisément à ladite automobile standard. En outre, on utilise de petites pièces d'acier (440, 446, 442, 444, 448, 450) antiprojectiles pour renforcer le blindage et l'intégrité structurale en différents points du véhicule blindé. De manière générale, le blindage est conçu pour permettre une fabrication sur site des composants d'un bon rapport efficacité/coût ainsi que pour permettre des procédures d'installation d'un bon rapport efficacité/coût, cela dans le but de produire un véhicule blindé léger d'un prix abordable.
PCT/US1996/013337 1995-08-14 1996-08-14 Vehicule blinde leger perfectionne et procede de fabrication correspondant WO1997007377A2 (fr)

Priority Applications (1)

Application Number Priority Date Filing Date Title
AU70081/96A AU7008196A (en) 1995-08-14 1996-08-14 Improved lightweight armored vehicle and method of making same

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US229295P 1995-08-14 1995-08-14
US60/002,292 1995-08-14

Publications (2)

Publication Number Publication Date
WO1997007377A2 true WO1997007377A2 (fr) 1997-02-27
WO1997007377A3 WO1997007377A3 (fr) 1997-04-24

Family

ID=21700106

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/US1996/013337 WO1997007377A2 (fr) 1995-08-14 1996-08-14 Vehicule blinde leger perfectionne et procede de fabrication correspondant

Country Status (3)

Country Link
CN (1) CN1172526A (fr)
AU (1) AU7008196A (fr)
WO (1) WO1997007377A2 (fr)

Cited By (16)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
EP0915315A3 (fr) * 1997-10-13 1999-07-28 Isoclima GmbH Vitre blindée munie d'un insert d'une feuille métallique
EP0971197A3 (fr) * 1998-07-07 2001-03-14 Ressenig-Fahrzeugbau Gesellschaft m.b.H. Méthode pour monter une couche blindée dans la carrosserie d'une voiture
DE10002447A1 (de) * 2000-01-21 2001-08-16 Daimler Chrysler Ag Gepanzerte Fahrzeugtüre
DE10002449A1 (de) * 2000-01-21 2001-08-16 Daimler Chrysler Ag Gepanzerte Fahrzeugtüre
US6276100B1 (en) 1998-11-27 2001-08-21 Isoclima Gmbh Bulletproof glass window for use as a windscreen in a motor vehicle
US6280826B1 (en) 1998-12-16 2001-08-28 Isoclima Gmbh Bulletproof glass window for a motor vehicle
EP1916496A1 (fr) * 2006-10-25 2008-04-30 Krauss-Maffei Wegmann GmbH & Co. KG Véhicule automobile protégé contre les effets d'explosions extérieures, en particulier véhicule automobile militaire
JP2009281722A (ja) * 1997-06-18 2009-12-03 Saint Gobain Vitrage 特に自動車用の固定式または可動式の側面装甲窓ガラス
DE19803435C5 (de) * 1998-01-29 2010-06-24 Volkswagen Ag Sicherheitsglasaufbau für Sicherheitskraftfahrzeuge
RU2502037C2 (ru) * 2011-10-05 2013-12-20 Закрытое акционерное общество Корпорация "Защита" Автомобиль скрытого бронирования
RU2520865C1 (ru) * 2012-11-28 2014-06-27 Геннадий Юрьевич Яворский Способ установки стекол при бронировании автомобиля
DE102011055687B4 (de) * 2011-11-24 2014-09-25 Benteler Defense Gmbh & Co. Kg Splitterschutzanordnung sowie Abschirmelement für eine Splitterschutzanordnung
WO2019008466A1 (fr) * 2017-07-02 2019-01-10 Agp America S.A. Stratifié multicouche et procédé de production
EP3384227A4 (fr) * 2015-11-30 2019-08-21 Equipment Armor, Inc. Écrans de protection
CZ309481B6 (cs) * 2021-12-07 2023-02-15 J.P.D. GROUP, s.r.o Ohnivzdorný osobní vůz se spalovacím motorem pro únik z životu nebezpečných situací
US11993914B2 (en) 2022-09-23 2024-05-28 Equipment Armor, Inc. Protective shields

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
FR3029454B1 (fr) * 2014-12-04 2020-09-25 Saint Gobain Vitrage blinde fabrique a partir de constituants de vitrages feuilletes de grande serie
CN106482583B (zh) * 2015-09-01 2018-05-04 中国航天科工集团第四研究院指挥自动化技术研发与应用中心 一种伪装防弹防护组件
CN114659556B (zh) * 2022-03-03 2024-03-12 中国科学院计算技术研究所 一种面向巡视器的可分离式星表材质识别方法及系统

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3855898A (en) * 1972-12-12 1974-12-24 Goodyear Aerospace Corp Protective panel for a vehicle door
US4316404A (en) * 1978-06-30 1982-02-23 Medlin Richard C Lightweight armored vehicle and method of making same

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3855898A (en) * 1972-12-12 1974-12-24 Goodyear Aerospace Corp Protective panel for a vehicle door
US4316404A (en) * 1978-06-30 1982-02-23 Medlin Richard C Lightweight armored vehicle and method of making same

Cited By (19)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2009281722A (ja) * 1997-06-18 2009-12-03 Saint Gobain Vitrage 特に自動車用の固定式または可動式の側面装甲窓ガラス
EP0918629B2 (fr) 1997-06-18 2012-05-09 Saint-Gobain Glass France Vitrage blinde, notamment lateral fixe ou mobile pour vehicule automobile
EP0915315A3 (fr) * 1997-10-13 1999-07-28 Isoclima GmbH Vitre blindée munie d'un insert d'une feuille métallique
DE19803435C5 (de) * 1998-01-29 2010-06-24 Volkswagen Ag Sicherheitsglasaufbau für Sicherheitskraftfahrzeuge
EP0971197A3 (fr) * 1998-07-07 2001-03-14 Ressenig-Fahrzeugbau Gesellschaft m.b.H. Méthode pour monter une couche blindée dans la carrosserie d'une voiture
US6276100B1 (en) 1998-11-27 2001-08-21 Isoclima Gmbh Bulletproof glass window for use as a windscreen in a motor vehicle
US6280826B1 (en) 1998-12-16 2001-08-28 Isoclima Gmbh Bulletproof glass window for a motor vehicle
DE10002449A1 (de) * 2000-01-21 2001-08-16 Daimler Chrysler Ag Gepanzerte Fahrzeugtüre
DE10002447A1 (de) * 2000-01-21 2001-08-16 Daimler Chrysler Ag Gepanzerte Fahrzeugtüre
DE10002447C2 (de) * 2000-01-21 2003-11-06 Daimler Chrysler Ag Gepanzerte Fahrzeugtüre
EP1916496A1 (fr) * 2006-10-25 2008-04-30 Krauss-Maffei Wegmann GmbH & Co. KG Véhicule automobile protégé contre les effets d'explosions extérieures, en particulier véhicule automobile militaire
RU2502037C2 (ru) * 2011-10-05 2013-12-20 Закрытое акционерное общество Корпорация "Защита" Автомобиль скрытого бронирования
DE102011055687B4 (de) * 2011-11-24 2014-09-25 Benteler Defense Gmbh & Co. Kg Splitterschutzanordnung sowie Abschirmelement für eine Splitterschutzanordnung
RU2520865C1 (ru) * 2012-11-28 2014-06-27 Геннадий Юрьевич Яворский Способ установки стекол при бронировании автомобиля
EP3384227A4 (fr) * 2015-11-30 2019-08-21 Equipment Armor, Inc. Écrans de protection
US11486114B2 (en) 2015-11-30 2022-11-01 Equipment Armor, Inc. Protective shields
WO2019008466A1 (fr) * 2017-07-02 2019-01-10 Agp America S.A. Stratifié multicouche et procédé de production
CZ309481B6 (cs) * 2021-12-07 2023-02-15 J.P.D. GROUP, s.r.o Ohnivzdorný osobní vůz se spalovacím motorem pro únik z životu nebezpečných situací
US11993914B2 (en) 2022-09-23 2024-05-28 Equipment Armor, Inc. Protective shields

Also Published As

Publication number Publication date
AU7008196A (en) 1997-03-12
CN1172526A (zh) 1998-02-04
WO1997007377A3 (fr) 1997-04-24

Similar Documents

Publication Publication Date Title
US6327954B1 (en) Lightweight armored vehicle and method of making same
WO1997007377A2 (fr) Vehicule blinde leger perfectionne et procede de fabrication correspondant
US5820201A (en) High impact barrier for automobile body exterior components
EP0676996B1 (fr) Procede de fabrication d' une feuille stratifiee cintree de verre de securite
US6276100B1 (en) Bulletproof glass window for use as a windscreen in a motor vehicle
JPS6166645A (ja) 窓材アセンブリ及びその製造方法
US4336644A (en) Method of installing bulletproof windows in an armored automobile
US20150000511A1 (en) Bullet-Proof Glass Pane and Associated Bullet-Resistant Appartus
JP2003503296A (ja) 車両用強化積層窓ガラス
US20110024564A1 (en) Injection-molded window panel and related methods
US6041689A (en) Vehicle armoring assembly
US11034136B2 (en) Intrusion resistant laminated automotive glazing
KR930011145B1 (ko) 유리에 파손 방지용 플라스틱층을 붙이는 방법
US20050081464A1 (en) Stabilized window structure and method of stabilizing window structures entirely or substantially entirely devoid of glass
MXPA97002743A (en) Armored vehicle of improved light weight, and method to make my
US11584199B2 (en) Passenger retention system and method
US20200282705A1 (en) Opaque laminated vehicle roof with panoramic glazed appearance
RU96104344A (ru) Усовершенствованное легкое бронированное транспортное средство и способ его изготовления
WO2023170609A1 (fr) Verre blindé présentant une esthétique et une ouverture de lumière du jour améliorées
WO2017095847A1 (fr) Écrans de protection
CN110895123A (zh) 一种防弹玻璃窗格
JP2000001345A (ja) 異層合せガラス板
MXPA99010780A (en) Bulletproof glass window for use as a windscreen in a motor vehicle
IL108237A (en) Concave, unbreakable laminated glass and method of manufacture
CN107003100A (zh) 由大规模生产的层压窗玻璃组件制造的装甲玻璃

Legal Events

Date Code Title Description
WWE Wipo information: entry into national phase

Ref document number: 96191071.2

Country of ref document: CN

AK Designated states

Kind code of ref document: A2

Designated state(s): AL AM AT AU AZ BB BG BR BY CA CH CN CU CZ DE DK EE ES FI GB GE HU IL IS JP KE KG KP KR KZ LK LR LS LT LU LV MD MG MK MN MW MX NO NZ PL PT RO RU SD SE SG SI SK TJ TM TR TT UA UG US UZ VN AM AZ BY KG KZ MD RU TJ TM

AL Designated countries for regional patents

Kind code of ref document: A2

Designated state(s): KE LS MW SD SZ UG AT BE CH DE DK ES FI FR GB GR IE IT LU MC NL PT SE BF BJ CF CG CI CM

WWE Wipo information: entry into national phase

Ref document number: PA/a/1997/002743

Country of ref document: MX

ENP Entry into the national phase in:

Ref document number: 1997 817370

Country of ref document: US

Date of ref document: 19970506

Kind code of ref document: A

121 Ep: the epo has been informed by wipo that ep was designated in this application
REG Reference to national code

Ref country code: DE

Ref legal event code: 8642

122 Ep: pct application non-entry in european phase
NENP Non-entry into the national phase in:

Ref country code: CA