WO1996035249A1 - Discharge tube with coated discharge surface - Google Patents
Discharge tube with coated discharge surface Download PDFInfo
- Publication number
- WO1996035249A1 WO1996035249A1 PCT/JP1996/001200 JP9601200W WO9635249A1 WO 1996035249 A1 WO1996035249 A1 WO 1996035249A1 JP 9601200 W JP9601200 W JP 9601200W WO 9635249 A1 WO9635249 A1 WO 9635249A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- discharge
- weight
- voltage
- discharge tube
- coating agent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01T—SPARK GAPS; OVERVOLTAGE ARRESTERS USING SPARK GAPS; SPARKING PLUGS; CORONA DEVICES; GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES
- H01T1/00—Details of spark gaps
- H01T1/20—Means for starting arc or facilitating ignition of spark gap
- H01T1/22—Means for starting arc or facilitating ignition of spark gap by the shape or the composition of the electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01T—SPARK GAPS; OVERVOLTAGE ARRESTERS USING SPARK GAPS; SPARKING PLUGS; CORONA DEVICES; GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES
- H01T4/00—Overvoltage arresters using spark gaps
- H01T4/10—Overvoltage arresters using spark gaps having a single gap or a plurality of gaps in parallel
- H01T4/12—Overvoltage arresters using spark gaps having a single gap or a plurality of gaps in parallel hermetically sealed
Definitions
- the present invention relates to a discharge tube suitable for use in a lightning arrester, a spark gap for supplying a constant voltage to a spark plug, a high-pressure discharge lamp, or the like.
- the present invention relates to a discharge tube having a discharge surface coated with a coating agent.
- a lightning arrester attached to the equipment's commercial power supply line to prevent a single surge voltage generated by lightning from entering the equipment, or ignition of a vehicle ignition plug or high-pressure discharge lamp
- spark gaps for continuously supplying a high constant voltage for use in applications.
- the initial discharge starting voltage with respect to the surge voltage is kept as low as possible.
- the discharge surface of the electrode is Various coating agents are applied. It should be noted that since a spark gap has a function of reducing the discharge voltage to approximately a predetermined voltage or less, it can be naturally used as a lightning arrester.
- the most common coating agents known in the past include sodium silicate, 2-nitrocellulose and silicone as a fixing agent using water as a solvent, and improved surge withstand capability.
- barium titanate or aluminum oxide is added.
- a first object of the present invention is to provide a discharge tube capable of obtaining a stable discharge voltage even with a surge pulse having a short rise time. It is in.
- a second object of the present invention is to provide a discharge tube capable of obtaining a stable discharge voltage even when a continuous discharge is performed.
- the present invention has the following configuration to achieve the above object.
- the discharge tube in the discharge tube according to the present invention, two electrodes are arranged to face each other with an insulator interposed therebetween, and a discharge is generated in a gap formed between the facing discharge surfaces of these electrodes.
- at least one of potassium bromide, potassium fluoride, and sodium fluoride was used on the discharge surfaces of the two electrodes at a weight of 0.01 to 60% by weight. % Is applied.
- the content of the one kind of alkali metal salt in the coating composition is preferably 5 to 30% by weight, and particularly preferably 10 to 20% by weight.
- the content of sodium silicate in the coating agent is preferably 0.5 to 10% by weight, and particularly preferably 1 to 2.5% by weight.
- FIG. 1 is a sectional view of a discharge tube according to the present invention.
- FIG. 2 is a graph showing a one-hour voltage characteristic of a discharge tube (using a coating agent mixed with potassium bromide) according to the first embodiment of the present invention.
- Fig. 3 is a graph showing the continuous discharge characteristics when a high-voltage pulse is continuously applied to the discharge tube in Fig. 2 (showing the upper and lower limits of the wave).
- FIG. 4 is a graph showing voltage-time characteristics in a discharge tube (using a coating material in which sodium silicate and potassium bromide are mixed) according to the second embodiment of the present invention.
- Fig. 5 is a graph showing the continuous discharge characteristics when a high-voltage pulse is continuously applied to the discharge tube in Fig. 4 (showing the upper and lower limits of the wave).
- Fig. 6 is a graph showing the continuous discharge characteristics when the high voltage pulse is continuously applied again to the discharge tube of Fig. 4 after the high voltage pulse is continuously applied (showing the upper and lower limits of the wave). '
- FIG. 7 is a graph showing continuous discharge characteristics when a high-voltage pulse is applied to the discharge tube according to the third embodiment of the present invention.
- FIG. 8 is a graph showing continuous discharge characteristics when a high-voltage pulse is applied to the discharge tube of the fourth embodiment (showing upper and lower limits of waves).
- FIG. 9 is a sectional view showing the shape of another embodiment of the electrode portion of the discharge tube of the present invention.
- FIG. 10 is a graph showing voltage-hour characteristics when a high-voltage pulse is applied to a conventional discharge tube.
- Fig. 11 is a graph showing the continuous discharge characteristics of a discharge tube coated with 25 wt% sodium silicate and 5 wt% barium titanate as an example of a conventional discharge tube (upper / lower limit of wave). Is shown).
- Fig. 12 is a graph showing the continuous discharge characteristics of a discharge tube coated with a coating material of 6% by weight of sodium silicate and 3.5% by weight of barium titanate as an example of a conventional discharge tube. (Shows the upper and lower limits of the wave).
- FIG. 10 is a graph showing, as an example, a one-hour voltage characteristic of a discharge tube in which a coating material containing sodium silicate and barium titanate is applied to a discharge surface.
- the voltage on the vertical axis indicates the discharge starting voltage when the surge pulse voltage is applied
- the time on the horizontal axis indicates the pulse width of the applied surge pulse.
- the rise time of the surge pulse (unit: voltage Z time) is also shown.
- This graph shows a change in the actual discharge start voltage with respect to a change in the pulse width and the rise time of the surge pulse of the discharge tube designed in advance to a predetermined discharge start voltage.
- the discharge starting voltage is 600 volts
- Fig. 11 shows a high-voltage pulse of 5 ms ec applied to a discharge tube coated with a coating material containing 25% by weight of sodium silicate and 5% by weight of barium titanate.
- Fig. 12 shows the initial discharge characteristics (continuous discharge characteristics) when voltage was applied.
- Fig. 12 shows the discharge time of 5 ms ec on a discharge tube coated with a 6% by weight of sodium silicate and 3.5% by weight of barium titanate.
- the initial discharge characteristics (continuous discharge characteristics) when a high voltage pulse is applied are shown, but no stable continuous discharge starting voltage was obtained in any case.
- FIG. 1 is a sectional view showing an example of the discharge tube 10.
- Numeral 12 is a cylindrical insulator made of ceramics such as alumina, etc. Electrodes 14a and 14b are fixed to the openings of both ends of the cylindrical insulator 12 with silver brazes facing each other and sealed.
- the insulator 12 is filled with a low-pressure inert gas such as argon.
- Carbon trigger wires (not shown) are formed at appropriate places on the inner wall of the insulator 12 to stabilize the initial discharge.
- Electrodes 14a and 14b made of iron-nickel alloy, iron-nickel-cobalt alloy or copper have discharge surfaces 17a and 17b, respectively, and are provided between these opposed discharge surfaces 17a and 17b. Discharge occurs at gap 20.
- the coating agent 16 is applied on the facing discharge surfaces 17a and 17b.
- the coating agent 16 uses water (pure water) as a solvent, and is a known coating agent using barium titanate, and is an alkali metal salt with respect to the solvent 1. Contains 0.01 to 60% by weight of potassium bromide. The coating agent 16 is dried after being applied to the discharge surface.
- FIG. 2 shows a specific example of the first embodiment (a discharge tube in which an application agent containing 10% by weight of potassium bromide was applied to an application agent containing barium titanate as a main component). Voltage It is a graph which shows one hour characteristic.
- the conventional example uses a 200-volt discharge tube.
- the discharge starting voltage rises and exceeds 2000 volts in 10 kV Z mic mouth seconds. This means that even if a 200-volt discharge tube is installed as a lightning arrester on the device to be protected, an abnormal voltage exceeding 2000 volts will enter the device, preventing reliable protection of the device and damaging the device. May occur. Looking at Figure 10, it is clear that abnormal voltages exceeding 200 volts can be reliably removed for surges with rise times of about 200 volts Zmsec to 400 volts Zmsec.
- the discharge starting voltage does not rise steeply as compared with the comparative example, and is 10 kV Z microsecond.
- the discharge starting voltage does not rise steeply as compared with the comparative example, and is 10 kV Z microsecond.
- it operates at about 430 volts and exhibits excellent characteristics as a lightning arrester. Therefore, the equipment can be reliably protected, and the occurrence rate of the equipment being damaged can be reduced.
- potassium bromide directly affects the stability of the discharge voltage, it can be used in the range of 0.01 to 60% by weight. The stability is preferably high at around% by weight.
- other alkali metal salts for example, potassium fluoride and sodium fluoride, may be used, and at least one of these three alkali metal salts is contained. You may make it do.
- the discharge tube 10 As shown in FIG. 3, the discharge tube 10 according to the first embodiment has a constant discharge characteristic (continuous discharge characteristic) when a high-voltage pulse of 5 ms ec or less is continuously applied. Because the voltage cannot be maintained stably, there is no possibility of using it as a spark gap. (Second embodiment)
- the mechanical structure of the discharge tube 10 is the same as the structure shown in FIG.
- the second embodiment is characterized in that the coating agent contains sodium silicate as a fixing agent.
- the coating agent 16 uses water (pure water) as a solvent.
- the sodium silicate is 0.01 to 50% by weight and the potassium bromide is 0.01 to 60% by weight based on the solvent 1. %.
- the coating agent 16 is dried after being applied to the discharge surface. The effect is exhibited from about 0.01% by weight of sodium silicate added, and the discharge characteristics are most stable in the range of 1 to 1.5% by weight. 2. When the content is more than 5% by weight, the stability of the discharge characteristics gradually decreases, and when the content exceeds 40% by weight, the continuation discharge becomes more likely to occur. The effect lasts up to the solubility limit in water of 50% by weight.
- FIG. 4 is a graph showing voltage-time characteristics in a specific example of the second embodiment (sodium silicate: 2.5% by weight, potassium bromide: 10% by weight).
- the voltage-hour characteristic of the discharge tube 10 according to the second embodiment is similar to that of the discharge agent containing potassium bromide. Even in the case of a short time, as in the first embodiment, an increase in the discharge start voltage is suppressed, and a good discharge start voltage can be obtained.
- Fig. 5 shows the preparation of a coating agent containing 2.5% by weight of sodium silicate and 15% by weight of potassium bromide.
- a high voltage pulse of 5 ms ec or less was applied to the spark gap applied to the discharge surface.
- 5 shows the initial discharge characteristics in the case.
- the potassium bromide but also the sodium silicate contained not only the voltage-hour characteristics shown in Fig. 4 but also the initial discharge characteristics (continuous discharge characteristics). When the starting voltage is around 1000 volts Can be stabilized.
- the discharge tube can be used not only as a lightning arrester but also as a spark gap.
- Figure 6 shows the discharge characteristics after the operation of applying a high-voltage pulse of 5 ms e or less for 1 sec to the same discharge tube as described above was performed 20 000 times. As is evident from the figure, the discharge starting voltage was maintained at 1000 volts even when used for a long time, showing stable discharge characteristics.
- the configuration of the discharge tube according to the third embodiment is substantially the same as that of the discharge tube 10 described with reference to FIG. 1, except that the components of the coating agent 16 are different.
- the coating agent 16 uses water as a solvent and contains 0.01 to 50% by weight of sodium silicate and 0.01 to 60% by weight of calcium fluoride. The coating agent 16 is dried after being applied to the discharge surface.
- the content of sodium silicate is the same as that described in the second embodiment, and a description thereof will be omitted.
- Fluidizing force has a direct effect on the stability of the discharge voltage, and can be used in the range of 0.01 to 60% by weight, but the discharge characteristics are stable in the range of 5 to 30% by weight, especially 10 to 20%
- the stability is preferably high at around% by weight.
- Fig. 7 shows the preparation of a coating agent containing 2.5% by weight of sodium silicate and 15% by weight of potassium fluoride, and application of a high-voltage pulse of 5 ms ec or less to the spark gap applied to the discharge surface. It shows the initial discharge characteristics (continuous discharge characteristics) in the case of the above. As is clear from the figure, the firing voltage is stable around 1000 volts.
- a high voltage pulse of 5 ms ec or less is applied to this discharge tube for 1 sec.
- the discharge characteristics after 20,000 operations are not shown, the discharge starting voltage is maintained at 1000 volts even when the discharge tube is used for a long period of time, as in the discharge tube of the second embodiment, and is stable. Discharge characteristics were shown.
- the voltage-hour characteristic is not shown, it has substantially the same characteristics as those of the second embodiment.
- the configuration of the discharge tube according to the fourth embodiment is substantially the same as the discharge tube 10 described in the first embodiment, except for the components of the coating agent 16.
- the coating agent 16 uses water as a solvent and contains 0.01 to 50% by weight of sodium silicate and 0.01 to 60% by weight of sodium fluoride. The coating agent 16 is dried after being applied to the discharge surface.
- the content of sodium silicate is the same as that described in the second embodiment, and a description thereof will be omitted.
- the sodium fluoride directly affects the stability of the discharge voltage, and can be used in the range of 0.01 to 60% by weight, but the discharge characteristics are stable in the range of 5 to 30% by weight. A stability of about 10 to 20% by weight is high and is suitable.
- Fig. 8 shows that a coating agent 16 containing 2.5% by weight of sodium silicate and 15% by weight of sodium fluoride was prepared, and a high-voltage pulse of 5 ms ec or less was applied to the discharge tube applied to the discharge surface.
- 7 shows initial discharge characteristics when voltage is applied.
- the discharge starting voltage is stable around 1000 volts.
- the discharge characteristics after 20,000 times of applying a high-voltage pulse of 5 ms ec or less to the discharge tube for 1 sec are not shown, the discharge characteristics are similar to those of the discharge tube of the first embodiment. Even when used continuously, the discharge starting voltage was maintained at 1000 volts, showing stable discharge characteristics.
- the voltage-hour characteristic is not shown, it has substantially the same characteristics as those of the second embodiment.
- the alkali metal salts to be included in the coating agent 16 together with the sodium silicate include potassium bromide, sodium fluoride, and sodium fluoride. Used one of them, but two kinds of potassium bromide and potassium fluoride, two kinds of potassium bromide and sodium fluoride, and two kinds of potassium fluoride and sodium fluoride.
- the coating agent 16 contains a mixture of multiple alkali metal salts, such as two types of thorium and three types of potassium bromide, potassium fluoride, and sodium fluoride. Even in this case, good characteristics can be obtained.
- the content of each alkali metal salt contained in the coating agent 16 can be used in the range of 0.01 to 60% by weight, as in the case of one kind, but 5 to 30% by weight.
- the discharge characteristics are stable, especially 10 ⁇ 20 weight
- the above alkali metal salts as one example, potassium bromide and potassium fluoride
- 2.5% by weight of sodium silicate and bromide are used. It may be adjusted to a coating agent 16 containing 15% by weight of potassium and 15% by weight of potassium fluoride.
- the above three kinds of aluminum salts are used.
- 2.5% by weight of sodium silicate, 15% by weight of potassium bromide, 15% by weight of sodium fluoride, 15% by weight of sodium fluoride What is necessary is just to adjust to the coating agent 16 containing the weight%.
- the coating agent of the present invention may be applied to a triode discharge tube or the like.
- the shape of the discharge surface of the electrode of the discharge tube 10 may be replaced with the flat shape of FIG. 1 and a concave portion 18 may be provided on the discharge surface as shown in FIG. By adopting this configuration, the surface area can be increased, and the discharge life is extended.
- ADVANTAGE OF THE INVENTION According to the discharge tube according to the present invention, even when the rise time of the surge voltage becomes short, a stable discharge starting voltage can be obtained, and the device can be prevented from being damaged by being used as a lightning arrester. Can be.
- Ignition plug It has a remarkable effect that it can have good characteristics even as a spark gap used for ignition of a high pressure discharge lamp.
Landscapes
- Vessels And Coating Films For Discharge Lamps (AREA)
- Paints Or Removers (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| EP96912300A EP0769832A4 (en) | 1995-05-02 | 1996-05-01 | DISCHARGE TUBE WITH COATED DISCHARGE SURFACE |
Applications Claiming Priority (4)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7/108464 | 1995-05-02 | ||
| JP10846495 | 1995-05-02 | ||
| JP06754296A JP3749754B2 (ja) | 1995-05-02 | 1996-03-25 | 放電管 |
| JP8/67542 | 1996-03-25 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| WO1996035249A1 true WO1996035249A1 (en) | 1996-11-07 |
Family
ID=26408765
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PCT/JP1996/001200 Ceased WO1996035249A1 (en) | 1995-05-02 | 1996-05-01 | Discharge tube with coated discharge surface |
Country Status (5)
| Country | Link |
|---|---|
| EP (1) | EP0769832A4 (enExample) |
| JP (1) | JP3749754B2 (enExample) |
| KR (1) | KR100206035B1 (enExample) |
| CA (1) | CA2194212A1 (enExample) |
| WO (1) | WO1996035249A1 (enExample) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6194820B1 (en) * | 1998-02-20 | 2001-02-27 | Shinko Electric Industries Co., Ltd. | Discharge tube having switching spark gap |
| FR2907865B1 (fr) | 2006-10-30 | 2009-06-05 | Valeo Embrayages | Embrayage pour vehicules automobiles a moyens de centrage du cordon rampe sur le plateau de pression |
| CN103594304A (zh) * | 2013-11-21 | 2014-02-19 | 四川天微电子有限责任公司 | 放电管点火装置 |
| US20240182726A1 (en) * | 2021-03-29 | 2024-06-06 | The Regents Of The University Of California | Sprayable cool white coating based on ceramic microspheres |
Citations (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5537709A (en) * | 1978-09-07 | 1980-03-15 | Shiroyama Seisakusho Kk | Communication atmospheric discharge arrester |
| JPS6313290A (ja) * | 1986-06-25 | 1988-01-20 | シ−メンス、アクチエンゲゼルシヤフト | ガス放電避雷器 |
| JPS6359513B2 (enExample) * | 1977-08-09 | 1988-11-18 | ||
| JPH0223996B2 (enExample) * | 1983-09-30 | 1990-05-28 | Siemens Ag | |
| JPH0633388U (ja) * | 1992-10-06 | 1994-04-28 | 矢崎総業株式会社 | 放電管 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE2537964C3 (de) * | 1975-08-26 | 1978-03-30 | Siemens Ag, 1000 Berlin Und 8000 Muenchen | Überspannungsableiter mit einer Gasfüllung |
-
1996
- 1996-03-25 JP JP06754296A patent/JP3749754B2/ja not_active Expired - Fee Related
- 1996-05-01 EP EP96912300A patent/EP0769832A4/en not_active Withdrawn
- 1996-05-01 WO PCT/JP1996/001200 patent/WO1996035249A1/ja not_active Ceased
- 1996-05-01 CA CA002194212A patent/CA2194212A1/en not_active Abandoned
- 1996-05-02 KR KR1019960014240A patent/KR100206035B1/ko not_active Expired - Lifetime
Patent Citations (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6359513B2 (enExample) * | 1977-08-09 | 1988-11-18 | ||
| JPS5537709A (en) * | 1978-09-07 | 1980-03-15 | Shiroyama Seisakusho Kk | Communication atmospheric discharge arrester |
| JPH0223996B2 (enExample) * | 1983-09-30 | 1990-05-28 | Siemens Ag | |
| JPS6313290A (ja) * | 1986-06-25 | 1988-01-20 | シ−メンス、アクチエンゲゼルシヤフト | ガス放電避雷器 |
| JPH0633388U (ja) * | 1992-10-06 | 1994-04-28 | 矢崎総業株式会社 | 放電管 |
Non-Patent Citations (1)
| Title |
|---|
| See also references of EP0769832A4 * |
Also Published As
| Publication number | Publication date |
|---|---|
| KR100206035B1 (ko) | 1999-07-01 |
| KR960042810A (ko) | 1996-12-21 |
| EP0769832A1 (en) | 1997-04-23 |
| EP0769832A4 (en) | 1998-07-15 |
| CA2194212A1 (en) | 1996-11-07 |
| JP3749754B2 (ja) | 2006-03-01 |
| JPH0922769A (ja) | 1997-01-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4433354A (en) | Gas-discharge surge arrester | |
| CA1214508A (en) | Gas filled surge arrester | |
| US4769736A (en) | Gas discharge surge arrester | |
| US5336970A (en) | Gas tube protector | |
| US6788519B2 (en) | Pressure-resistant encapsulated air-gap arrangement for the draining off of damaging perturbances due to overvoltages | |
| JP2001516943A (ja) | ガス充填形放電路 | |
| US4009422A (en) | Lightning arrester construction | |
| JP3749754B2 (ja) | 放電管 | |
| US6362945B1 (en) | Gas-filled surge arrester wIth an activating compound formed of a plurality of components | |
| JPH056797B2 (enExample) | ||
| CA1124317A (en) | Surge arrester with improved impulse ratio | |
| JP3378583B2 (ja) | ガス充填形放電ギャップ | |
| EP0060530B1 (en) | Electrical circuit protector | |
| GB1468677A (en) | Duplex surge arrestors | |
| JP2002508580A (ja) | ガスを充填した放電ギャップ | |
| GB2181887A (en) | Electrode of surge arrester | |
| US4924347A (en) | Gas lightning arrester containing a mineral addition agent | |
| JP2573908Y2 (ja) | 放電管 | |
| USH60H (en) | Long-life triggered spark gap | |
| US20010026432A1 (en) | Protector device | |
| JP2002289317A (ja) | 通信用避雷器 | |
| GB2046009A (en) | Excess voltage arrester | |
| JPH05283141A (ja) | ギャップ型サージアブソーバ | |
| JP3536592B2 (ja) | 放電管型サージアブソーバ | |
| JPH0658592U (ja) | 放電管 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| AK | Designated states |
Kind code of ref document: A1 Designated state(s): CA US |
|
| AL | Designated countries for regional patents |
Kind code of ref document: A1 Designated state(s): AT BE CH DE DK ES FI FR GB GR IE IT LU MC NL PT SE |
|
| ENP | Entry into the national phase |
Ref document number: 1996 765631 Country of ref document: US Date of ref document: 19961227 Kind code of ref document: A |
|
| WWE | Wipo information: entry into national phase |
Ref document number: 2194212 Country of ref document: CA |
|
| WWE | Wipo information: entry into national phase |
Ref document number: 1996912300 Country of ref document: EP |
|
| 121 | Ep: the epo has been informed by wipo that ep was designated in this application | ||
| WWP | Wipo information: published in national office |
Ref document number: 1996912300 Country of ref document: EP |
|
| WWW | Wipo information: withdrawn in national office |
Ref document number: 1996912300 Country of ref document: EP |