US20010054693A1 - Method and apparatus for inspection of a substrate by use of a ring illuminator - Google Patents
Method and apparatus for inspection of a substrate by use of a ring illuminator Download PDFInfo
- Publication number
- US20010054693A1 US20010054693A1 US09/821,426 US82142601A US2001054693A1 US 20010054693 A1 US20010054693 A1 US 20010054693A1 US 82142601 A US82142601 A US 82142601A US 2001054693 A1 US2001054693 A1 US 2001054693A1
- Authority
- US
- United States
- Prior art keywords
- substrate
- image
- incident angle
- defect
- infrared light
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
- The present invention relates generally to inspection devices, and more particularly to an device which can perform inspections of a substrate by an infrared imaging technique.
- Cracks or defects in a substrate can result in substrate failures or failures in the system in which the substrate is placed. When the substrate is used as a solar cell, the crack or defect has the potential to severely limit the power output of the solar panel which contains the defective solar cell. Once a crack has begun, it is highly probable that it will propagate over time to develop into a more significant crack; therefore, it is important to detect not only large but also small cracks. Flight program specifications typically require few or zero cracks in solar panels many square meters in size.
- A well-known method for inspecting solar cells involves illuminating the solar cell from the side with a tungsten halogen lamp and imaging the returned light with an infrared camera. Since this technique requires illuminating the solar cell from one side, it typically results in one side of the solar cell being too bright and the other side being too dim such that the solar cell is not uniformly illuminated. This lack of uniform illumination can mask small cracks, thereby leaving them undetected.
- This prior art method also typically requires operating the tungsten halogen lamp at a relatively high intensity level in order to provide sufficient illumination of the entire solar cell. Because a tungsten halogen lamp has a quartz envelope, it strongly absorbs energy in the 2 to 5 micron wavelength range of interest. To compensate for such absorption losses, a tungsten halogen lamp often operates at a relatively high temperature resulting in a large fraction of the light output power having shorter wavelengths. The shorter wavelength radiation, especially in the 1.0 to 2.0 micron range can result in glare due to strong reflections of the solar cell cover glass in the 1.0 to 2.0 micron wavelength range. Additionally, this high intensity level adds heat to the solar cell, which can result in thermal expansion of the cell, closing cracks temporarily during the inspection process such that those cracks avoid detection. Excessive heating of the solar cell can also result in ambiguous cell crack detection since the cell re-radiates the heat which is then imaged by the camera. Features in the image can appear as cracks even though no cracks exist.
- In addition, the current method cannot objectively and definitively differentiate surface anomalies from substrate cracks. Surface anomalies are mainly caused by the presence of contaminants, such as solvent stains, on the surface of the substrate. The contaminant is generally not harmful to solar cell performance and typically does not result in a rejection of the solar cell. For the current method, the image of a surface anomaly is typically more diffuse that the image of a cell crack; however, in many cases it is difficult to distinguish between a cell crack and a surface anomaly based solely on the appearance of the image. As a result, reinspection of the cell to distinguish between a crack and a surface anomaly is typically required, resulting in increased inspection time and cost. It is desirable to distinguish surface anomalies from cell cracks to avoid any unnecessary rejection of good cells or unnecessary rework of an otherwise good cell.
- What is needed therefore is an apparatus and method for detecting defects in a substrate such as a solar cell which provides consistent detection of defects such as cracks, differentiates between types of defects, and, does not excessively heat the substrate.
- The preceding and other shortcomings of the prior art are addressed and overcome by the present invention which provides an apparatus for detecting a defect in a substrate which includes an infrared radiating source spaced from the substrate and positioned to substantially uniformly illuminate the substrate with infrared light, an infrared camera with a lens positioned to collect the reflected infrared light from the substrate and means for creating an image from the reflected light, the image which including indicia representative of the defect.
- In a second aspect, the present invention provides a method for detecting a defect in a substrate, including the steps of illuminating the substrate with an infrared light source in an substantially uniform manner, collecting reflected infrared light from the substrate, producing an image from the reflected infrared light and examining the image for indicia of a defect.
- In still another aspect, the present invention provides an apparatus for detecting defects in a substrate and determining the type of each defect which includes an infrared radiating source spaced from the substrate and positioned to substantially uniformly illuminate the substrate with infrared light at an incident angle, an infrared camera with a lens positioned to collect the reflected infrared light from the substrate, means for creating an image from the collected light which includes indicia representative of the defect and means for varying the incident angle.
- The foregoing and additional features and advantage of this invention will become apparent from the detailed description and accompanying drawing figures below. In the figures and the written description, numerals indicate the various features of the invention, like numerals referring to like features throughout for both the drawing figures and the written description.
- Reference is now made to the detailed description of the preferred embodiments illustrated in the accompanying drawings, in which:
- FIG. 1 is a side view of the inspection device in accordance with the preferred embodiment of the present invention;
- FIG. 2 is a detailed end view of the ring illuminator illustrated in FIG. 1; and, FIG. 3 is a diagram showing an image of a solar cell using the present invention, illustrating an image indicia of defects.
- Referring to FIG. 1, an
inspection device 10 for inspecting asubstrate 12 and detecting defects such as cracks and surface anomalies is illustrated. Theinspection device 10 of the present invention is preferably utilized to inspectsolar cells 12 because it provides consistent, accurate detection of cracks and accurate differentiation between cracks, surface anomalies and delamination type defects. - The present invention is not limited to detecting cracks, surface anomalies and delamination type defects in a solar cells, but may also be utilized to detect defects in other substrates such as silicon, gallium arsinide, germanium and other substrates used in integrated circuits or energy collecting devices.
- As is illustrated in FIGS. 1 and 2, the
inspection device 10 includes an infrared radiatingsource 14 andinfrared camera 16. The infrared radiatingsource 14 producesinfrared energy 18 which is utilized to illuminate thesubstrate 12. Thesource 14 can be anyradiating source 14 which provides uniform illumination of asubstrate 12, but it is preferred that thesource 14 be aring illuminator 14 which is a radiating source in the shape of an annulus or a ring. A ring configuration provides a symmetrical radiation pattern such that thesubstrate 12 is uniformly illuminated from a constant θ angle. As shown in FIG. 2, for the preferred embodiment of the invention, thering illuminator 14 is comprised of a small diameter heater wire of a material such as nickel/chromium, which is spirally coiled and formed into an annular ring of afirst diameter 20. A 14 centimeterfirst diameter 20 is preferred for ease in handling and for providing good uniform illumination at both a far and a near distance from the substrate 12 (FIG. 1). However, the present invention is not limited to a 14 centimeter first diameter 20 (FIG. 2) but may be practiced with differentsize ring illuminators 14 having a variety offirst diameters 20. - Referring to FIGS. 1 & 2, for the preferred embodiment of the invention, the
ring illuminator 14 is supported by aninsulator 24. Theinsulator 24 can be formed from any material that has low thermal conductivity and can withstand the temperatures associated with thering illuminator 14, however, it is preferred that theinsulator 24 be fabricated of a transite material. Thering illuminator 14 can be fastened to theinsulator 24 by use of ceramic standoffs (not shown); however, it is preferred that theinsulator 24 contain agroove 25 in which thering illuminator 14 is placed. Thering illuminator 14 can be secured into thegroove 25 byseveral fasteners 26 which are preferably fabricated of a ceramic material. Anopening 28 is provided in theinsulator 24 such that thecamera 16 can view thesubstrate 12 through theopening 28. -
Infrared radiation 18 emitted from thering illuminator 14, is incident on thesubstrate 12 at an angle θ, and illuminates thesubstrate 12. Thesubstrate 12 in turn reflects the incidentinfrared radiation 18 in all directions. Thelens 30 of aninfrared camera 16 views thesubstrate 12 through the opening 28 in theinsulator 24. A portion of the reflected radiation is incident on the lens of thecamera 16 and is captured and collected by thecamera 16. Thecamera 16 provides the means to create animage 32 from the collected reflected infrared light. Thelens 30 of thecamera 16 is positioned along anaxis 34 approximately normal to thesubstrate 12 such that a substantial amount of surface area of thesubstrate 12 can be focused within the field of view of thecamera 16. Thecamera 16 preferably has a spectral response that matches the spectral outputs of thering illuminator 14. Onesuch camera 16 is a platinum-silicideinfrared camera 16 such as an Infracam™ made by Inframatrics Inc., located in North Billerica, Mass. The Infracam has a spectral response from a wavelength of 1 to 5 microns. Thelens 30 is preferably a close-uplens 30 which can be used to view a portion of thesubstrate 12 or theentire substrate 12. -
Many substrates 12 such assolar cells 12 include acover glass 36 with a coating that reflects strongly in the 1 to 2.0 micron wavelength range. For suchsolar cells 12, a long-pass filter 38 may be added to thecamera 16 to block the light reflected from thecover glass 36 and reduce any glare from such reflected light. Alternatively, thelens 30 can be made of a germanium material which acts as a filter to block radiation below a 2.0 micron wavelength. - For the preferred embodiment of the invention, a
light shield 40 is placed between thelens 30 of thecamera 16 and theinsulator 24 to shield thecamera 16 from any radiation from thering illuminator 14 and theinsulator 24. Thelight shield 40 can be formed integral with theinsulator 24 or as a separate unit. Preferably, thelight shield 40 is a tube of polyvinyl chloride material having aninterior surface 42 which is non-reflective to infrared light. - For the preferred embodiment of the invention, the
camera 16 provides the means to create animage 32 from the collected reflected infrared light. A separate processor, computer, or the like can also provide the means to create and record animage 32. Theimage 32 is preferably displayed on amonitor 44. If thesubstrate 12 is asolar cell 12 which is free of cracks and surface anomalies, theimage 32 will be uniform in appearance except for thegrid structure 46 inherent in the solar cell structure. If thesubstrate 12 includes defects, theimage 32 will displayindicia - When inspecting a
solar cell 12, for a large distance d and a small incident angle θ, the indicia of both cell cracks 48 andsurface anomalies 50 are displayed as dark images. To distinguish between asurface anomaly 50 and acell crack 48, thering illuminator 14 is repositioned closer to thesolar cell 12 along theaxis 34, thereby decreasing the distance d and increasing the incident angle θ. Theimage 32 is monitored during the movement of thering illuminator 14. Acell crack 44 will appear dark regardless of the distance and the incident angle θ. On the other hand, asurface anomaly 50 will be displayed as a dark image when thering illuminator 14 is positioned at a significant distance from thecell 12 such that thecell 12 is illuminated at a small θ angle. Theimage 50 fades away as thering illuminator 14 is repositioned closer to thesolar cell 12 and the θ angle increases. Theimage 50 eventually reappears as a bright image as thering illuminator 14 is further repositioned closer to thesolar cell 12 illuminating thesolar cell 12 at an even greater θ angle. Theimage 32 of thesurface anomaly 50 appears dark at a θ angle between approximately 20 and 40 degrees, the image fades away at about 45 to 46 degrees and becomes distinctly brighter at about 58 degrees. The present invention thus differentiatessurface anomalies 50 from cell cracks 48 and provides excellent, repeatable results when applied tosolar cells 12 having textured surface structures, such as high efficiency silicon cells, and can be used for inspection of baresolar cells 12 orsolar cells 12 having acover glass 36. - In addition, the present invention does not excessively heat the
substrate 12. A power input (not shown) into the coiled heater wire of thering illuminator 14 of about 35 Watts typically provides a level ofinfrared radiation 18 which adequately illuminates asolar cell 12 without acover glass 36, and, a power input of about 45 Watts typically provides a level ofinfrared radiation 18 which adequately illuminates asolar cell 12 with acover glass 36. These power input levels translate to temperatures of thering illuminator 14 of approximately 325 to 375 degrees Celsius respectively which is significantly lower than the prior art tungsten halogen lamp such that heating of thesolar cell 12 is reduced. Therefore, acell crack 48 can now be detected more consistently with minimal excess heating. - The present invention also allows for a large surface area of a
substrate 12 to be illuminated substantially more uniformly when compared to that achieved in the prior art because the present invention provides symmetrical radiation at a constant incident angle θ from all directions resulting in a uniformly illuminatedsubstrate 12. - In addition, the present invention provides a method to differentiate
cell cracks 48 fromsurface anomalies 50. However, the present invention is not limited to detection of cell cracks 48 andsurface anomalies 50 but can also detect other types of defects insubstrates 12 including delaminations between thesubstrate 12 and a second material, such as a metallized material, bonded to thesubstrate 12. Delaminations are displayed as bright images and remain bright with changes in illumination angle θ whereas substrate cracks 48 are displayed as dark images and remain dark with changes in illumination angle θ,surface anomalies 50 are displayed as a dark image which changes to a bright image with increases in illumination angle θ. - It will be appreciated by persons skilled in the art that the present invention is not limited to what has been shown and described hereinabove, nor the dimensions of sizes of the physical implementation described immediately above. The scope of invention is limited solely by the claims which follows.
Claims (22)