TW234190B - Prepare of inoganic hardenable slurry and method for solidifying wastes with the same - Google Patents

Prepare of inoganic hardenable slurry and method for solidifying wastes with the same

Info

Publication number
TW234190B
TW234190B TW82105899A TW82105899A TW234190B TW 234190 B TW234190 B TW 234190B TW 82105899 A TW82105899 A TW 82105899A TW 82105899 A TW82105899 A TW 82105899A TW 234190 B TW234190 B TW 234190B
Authority
TW
Taiwan
Prior art keywords
slurry
solidification
cement
wastes
hardenable
Prior art date
Application number
TW82105899A
Other languages
Chinese (zh)
Inventor
Ching-Tsuen Hwang
Wen-Yih Yang
Original Assignee
Inst Of Nuclear Fnergy Atomic Energy Council
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Inst Of Nuclear Fnergy Atomic Energy Council filed Critical Inst Of Nuclear Fnergy Atomic Energy Council
Priority to TW82105899A priority Critical patent/TW234190B/en
Application granted granted Critical
Publication of TW234190B publication Critical patent/TW234190B/en

Abstract

The present invention discloses a method for preparing the inorganic hardenable slurry and the use of same in the solidification of waste. In addition to water, the essential parts of the slurry are inorganic components including borates, cement-base powder and other additives such as magnesium oxide, gypsum and silica. The slurry is low in viscosity before solidification and flow freely, and within approximately 30 minutes after preparation the slurry becomes hardened into a highly solidified substance. The solidification of the slurry is resulted mainly from reaction of borate and the cement-base powder and to obtain a best result the weight of borates must be the same as that of the cement-base powder or even higher than the weight of the latter. The solidification mechanism differs entirely from the simple hydration reaction that brings about solidification of cement. The present invention also teaches a method for solidifying wastes with this hardenable slurry, i.e.to proceed solidification by admixing the various radioactive or non-radioactive dry and wet wastes with the hardenable slurry, or by burying waste pellets with the slurry. The solidified waste form thus obtained has a higher strength and the volume efficiency of the solidification is 2.5 to 10 times that of the conventional cement solidification. When applied to solidify low level radioactive wastes, the present method produces especiallya tremendous economic efficiency.
TW82105899A 1993-07-21 1993-07-21 Prepare of inoganic hardenable slurry and method for solidifying wastes with the same TW234190B (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
TW82105899A TW234190B (en) 1993-07-21 1993-07-21 Prepare of inoganic hardenable slurry and method for solidifying wastes with the same

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
TW82105899A TW234190B (en) 1993-07-21 1993-07-21 Prepare of inoganic hardenable slurry and method for solidifying wastes with the same

Publications (1)

Publication Number Publication Date
TW234190B true TW234190B (en) 1994-11-11

Family

ID=51348770

Family Applications (1)

Application Number Title Priority Date Filing Date
TW82105899A TW234190B (en) 1993-07-21 1993-07-21 Prepare of inoganic hardenable slurry and method for solidifying wastes with the same

Country Status (1)

Country Link
TW (1) TW234190B (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
TWI741802B (en) * 2020-09-21 2021-10-01 黃慶村 Method of processing liquid borate waste

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
TWI741802B (en) * 2020-09-21 2021-10-01 黃慶村 Method of processing liquid borate waste

Similar Documents

Publication Publication Date Title
CA2106747A1 (en) Preparation of Inorganic Hardenable Slurry and Method for Solidifying Wastes with the Same
CN100522854C (en) Solidifying agent for solidifying and stabilizing treatment of generated dewatered sludge in sewage plant
EG19497A (en) In-situ formation of soluble silicates from bio-genetic silica in chemical
CA2081214A1 (en) Hazardous waste disposal method and composition
KR840000045A (en) Solidification method of radioactive waste pellet
JPS60150879A (en) Conditioning method of contaminated waste by cement solidification
ES8608216A1 (en) Process for encapsulating slurries in cement.
JP2513690B2 (en) Solidifying agent for radioactive waste
TW234190B (en) Prepare of inoganic hardenable slurry and method for solidifying wastes with the same
JPS58195200A (en) Method of improving reservation of radioactive nuclide at solidifying radioactive waste
JP2781566B2 (en) Cement solidification method and solidified body of radioactive waste
JPS55149673A (en) Method for solidification treatment of impalpable powder waste containing heavy metal
JPS551865A (en) Solidification of heavy metals-containing wastes
JPS5343690A (en) Treating method for slag
JPS57180669A (en) Mildewproofing method
JP3009214B2 (en) Hydraulic solidifying material and waste disposal method
KR950012484A (en) Preparation of Inorganic Curable Slurry and Solidification of the Sludge Waste Prepared
GB2049261A (en) Method of disposal of tritium- containing water wastes
JPS55147182A (en) Solidifying treating method for waste containing heavy metal
JP2501576B2 (en) Solidifying agent for radioactive waste
EP0292307A3 (en) Compositions and methods for no mix compounds
JPS5623339A (en) Show mold
JPS62180294A (en) Shielding body to radioactivity
SU745880A1 (en) Method of producing building mortar
JPS54136000A (en) Cement solidification treating method of radioactive waste

Legal Events