Method of making glass with stone vein has: costing the product with a machine; heating glass material to form glass liquid at 1500 deg.C for 8-10 hours; forming base film with operating rod; adhering colored particles with base film evenly to form a complex; heating complex at high temperature of 1000 deg.C for 2 min; melting colored particles partially; placing complex in glass liquid to form a mixed layer; glass liquid on the outer layer of complex will be pressed before complex is placed in a mold, this phenomena is called the first re-location and recombination; cutting mixed layer and placing it in the mold from the top of the mold, the component produces the second re-location and recombination; applying 25 horse power of pressure in the mold to produce the thired re-location and recombination; removing the mold to obtain glass product.
TW83100120A1994-01-071994-01-07Method of making glass with stone vein