SU85598A1 - Method of making shark skins for felt production - Google Patents

Method of making shark skins for felt production

Info

Publication number
SU85598A1
SU85598A1 SU407892A SU407892A SU85598A1 SU 85598 A1 SU85598 A1 SU 85598A1 SU 407892 A SU407892 A SU 407892A SU 407892 A SU407892 A SU 407892A SU 85598 A1 SU85598 A1 SU 85598A1
Authority
SU
USSR - Soviet Union
Prior art keywords
skins
felt production
shark
making
hours
Prior art date
Application number
SU407892A
Other languages
Russian (ru)
Inventor
М.Н. Селезнев
Original Assignee
М.Н. Селезнев
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by М.Н. Селезнев filed Critical М.Н. Селезнев
Priority to SU407892A priority Critical patent/SU85598A1/en
Application granted granted Critical
Publication of SU85598A1 publication Critical patent/SU85598A1/en

Description

Предметом изобретени   вл ете  способ выделки шкуры черноморской акулы и шкуры северной сельдевой акулы, примеи емых в фетровом производстве дл  начеса шл п.The subject of the invention is the method of dressing the skins of the Black Sea shark and the skins of the northern herring shark, used in the felt production for combing wool.

Особенность способа заключаетс  в том, что шкуры акул, отмочеиные в растворе формалина и сульфата аммоии , иодвергают после мездреии  и промывки дублению, вначале в растворе формалина, а затем памазью хромовым экстрактом по бахтарме. Способ позвол ет получать выделанные шкуры необходимой прочности с полной сохранностью чешуек на лицевой стороне. Дл  этого шкуры акул мокро-соленогс консервировани  подвергают .отмочке в чане при ЖК-1:4 и температуре 16-22° с добавлением в отмочную воду 40-60 г/л сульфата аммоии  и 40%-ного раствора формалина из расчета 4% веса мокро-соленых шкур. Процесс ведут 18-24 час. с переборками через каждые 4-6шс-После отмочки шкуры подвергают мездрению до удалени  прирезей м са. Мездрение ведут вручную на колоде, нослечего шкуры промывают 10- 20 мин. чистой водой, имеюшей температуру 18-20°, с добавкой 0,5 г/л кальцинированной соды. При этом особое внимание обран,ают на отмывку загр знений лицевого чешуйчатого сло  шкуры. После этих операций шкуры подвергают дублению. Дубление в растворе формалина ведут при ЖК-1:4 и температуре 18-20°. В ванну внос т 40%-ный раствор формалина в ко.личестве 6% веса шкур и поваренную соль в количестве 6-7%, веса шкур. (Процесс ведут 20-24 час- с переборками через каждые 2-3 час. Хромовое дубление ведут намазью хромовым экстрактом ио бахтарме , после чего шкуры подвергают 8-12-часовой пролежке, нейтрализуют путем обработки водой с добавкой соды, затем промывают чистой водой и снова пролеживают при 20-25° в течепие 2-3 час. Обработанные таким образом шкуры набивают иа рамы, а шкуры черноА% 85598- 2 -The peculiarity of the method is that the shark skins, dyed in formalin solution and ammonium sulphate, are removed after washing and tanning, first in formalin solution, and then with chromium extract with chromium. The method allows to obtain tanned skins of the necessary strength with complete safety of the flakes on the front side. For this, shark skins wet-salt canning is subjected to a soaking in a vat at 1: 4 LCD and a temperature of 16-22 ° with 40-60 g / l of ammonium sulphate and 40% formalin at the rate of 4% by weight wet-salted skins. The process is 18-24 hours. with bulkheads every 4-6s-After-soaking, the skins are subject to shredding until the meat is removed. Fleshing is done by hand on a deck, and the skins are washed for 10-20 minutes. pure water having a temperature of 18-20 °, with the addition of 0.5 g / l of soda ash. At the same time, special attention has been given to the washing of soils of the facial scaly layer of the skin. After these operations, the skins are tanned. Tanning in formalin solution is carried out at LCD 1: 4 and a temperature of 18-20 °. A 40% formalin solution in a co-mixture of 6% by weight of hides and salt in an amount of 6-7%, the weight of hides, is introduced into the bath. (The process is carried out for 20-24 hours - with bulkheads every 2-3 hours. Chrome tanning is carried out with namazju chrome extract and bahtarme, after which the skins are subjected to 8-12 hours soaking, neutralized by treatment with water with soda, then washed with clean water lie again at 20–25 ° for 2–3 hours. The skins thus treated are stuffed with frames, and the black skins% 85598–2

морской мелкой акулы еще наклеивают на текстиль и сушат прл 25-30 в течение 24 час., после чего снимают/с рам и сортируют.the sea shallow shark is also glued to textiles and dried at 25-30 for 24 hours, after which it is removed / s frame and sorted.

Предмет изобретеии Subject of invention

Способ выделки шкур акулы дл  фетрового производства, отличающийс  тем, что шкуры черноморских акул и северных сельдевых , отмоченные в растворе формалина и сульфата аммоии , подвергают после мездрени  и промывки дублению :вначале в растворе формалила , а затем намазью хромовым экстрактом по бахтарме,The method of dressing shark skins for felt production, characterized in that the skins of the Black Sea sharks and northern herring, soaked in a solution of formalin and ammonium sulfate, are subjected after mezzanine and washing with tanning:

SU407892A 1949-11-28 1949-11-28 Method of making shark skins for felt production SU85598A1 (en)