Г1ре:дл:агаемый способ получени шлаковых путем затворени вОДой измельченного остывшего доменного шлака с последуюшей формовкой, сушкой и обжигом изделий отличаетс от известных тем, что обжиг ведут при температуре 800-950° с последующим медлеННым охлаждением до температуры 100-50°.G1re: for: a method for producing slag by mixing with water a chopped, cooled blast furnace slag followed by molding, drying and burning products differs from the known ones by burning at 800-950 ° C, followed by slow cooling to 100-50 ° C.
Остывший доменный шлак разма;1ывает : до фракции 0,05 мм, касса увлажн етс до 10-15% и формуетс в издели . Отформованные издели подвергаютс просушиванию при температуре 60- 120° в течение 24-30 час. ПослеThe cooled blast furnace slag stretches; 1waste: to a fraction of 0.05 mm, the cash register is moistened to 10-15% and molded into articles. Molded products are dried at a temperature of 60-120 ° for 24-30 hours. After
просушивани издели подвергают обжигу при температуре 800-950° и выдержке их в течение 24-30 час., затем медленному охлаждению до температуры 100-50°.drying the product is fired at a temperature of 800-950 ° and holding them for 24-30 hours, then slowly cooling to a temperature of 100-50 °.
Предмет изобретени Subject invention
Способ изготовлени шлаковых изделий путем затворени водой изме тьченного гранулированного доменного шлака с последующей формовкой, сушкой и обжигом изделий , отличающийс тем, что обжиг ведут при температуре 800-950° с последующим медленным охлаждением до температуры 100-50°.A method of making slag products by mixing with water a measured granulated blast furnace slag followed by molding, drying and burning of products, characterized in that the calcination is carried out at a temperature of 800-950 ° C, followed by slow cooling to a temperature of 100-50 °.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU22197A SU61030A1 (en) | 1939-03-02 | 1939-03-02 | Method of making slag products |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU22197A SU61030A1 (en) | 1939-03-02 | 1939-03-02 | Method of making slag products |
Publications (1)
Publication Number | Publication Date |
---|---|
SU61030A1 true SU61030A1 (en) | 1941-11-30 |
Family
ID=48242548
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SU22197A SU61030A1 (en) | 1939-03-02 | 1939-03-02 | Method of making slag products |
Country Status (1)
Country | Link |
---|---|
SU (1) | SU61030A1 (en) |
-
1939
- 1939-03-02 SU SU22197A patent/SU61030A1/en active
Similar Documents
Publication | Publication Date | Title |
---|---|---|
SU61030A1 (en) | Method of making slag products | |
AT322849B (en) | COMPOSITIONS FOR PRODUCTS WITH IMPACT RESISTANCE AND WEAR RESISTANCE AT HIGH TEMPERATURE AND PRODUCTION OF THESE PRODUCTS | |
ES388628A1 (en) | Treatment of cement raw materials | |
ES300068A1 (en) | Procedure for preparing a refractory (Machine-translation by Google Translate, not legally binding) | |
GB717520A (en) | Process of forming a ceramic body | |
ES340602A1 (en) | A method of Converting a Finely-Grained Material to a more Coarsely-Grained Material | |
ES452488A1 (en) | Production of cement by a dry process | |
SU464564A1 (en) | Refractory mass | |
SU386870A1 (en) | METHOD OF MANUFACTURING OF FARFORO-FAYANS PRODUCTS | |
SU94756A1 (en) | Method for continuous cooking of crushed raw materials | |
SU95400A1 (en) | The method of lining furnaces for the continuous production of sodium sulfide using graphite | |
GB783755A (en) | Improvements in and relating to the manufacture of shaped articles | |
SU373290A1 (en) | INSTALLATION FOR OBTAINING A FORMED COKE | |
SU92420A1 (en) | The method of manufacturing products of basalt | |
ES436956A1 (en) | Process for manufacturing ceramic products | |
ES333377A1 (en) | A procedure to manufacture a basque refractory brass agglomerated with fish. (Machine-translation by Google Translate, not legally binding) | |
FR1012197A (en) | Process for manufacturing elements for heat exchangers, and resulting products | |
SU50783A1 (en) | Method of making shaped parts from stone casting with holes of small diameter | |
SU53612A1 (en) | Method of making dolomite refractory brick | |
SU100217A1 (en) | Method for the production of carbon refractories | |
US2043640A (en) | Manufacture of refractory articles | |
FR63620E (en) | Process for the discoloration of plasticizers and the improvement of their thermal stability | |
GB679452A (en) | Improvements in the production of high quality silico-aluminous refractories | |
GB831769A (en) | Improvements in tunnel kilns | |
ES408067A1 (en) | Cast iron shot |