SU600213A1 - Method of protecting magnesium electrolyzer anodes from destruction - Google Patents

Method of protecting magnesium electrolyzer anodes from destruction

Info

Publication number
SU600213A1
SU600213A1 SU752191814A SU2191814A SU600213A1 SU 600213 A1 SU600213 A1 SU 600213A1 SU 752191814 A SU752191814 A SU 752191814A SU 2191814 A SU2191814 A SU 2191814A SU 600213 A1 SU600213 A1 SU 600213A1
Authority
SU
USSR - Soviet Union
Prior art keywords
anodes
destruction
electrolyzer
poured
overlapping
Prior art date
Application number
SU752191814A
Other languages
Russian (ru)
Inventor
Валерий Афанасьевич Колесников
Константин Дмитриевич Мужжавлев
Вячеслав Васильевич Башкатов
Анатолий Афанасьевич Щелконогов
Петр Александрович Донских
Леонид Федорович Земляных
Юрий Константинович Попов
Original Assignee
Предприятие П/Я Р -6919
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я Р -6919 filed Critical Предприятие П/Я Р -6919
Priority to SU752191814A priority Critical patent/SU600213A1/en
Application granted granted Critical
Publication of SU600213A1 publication Critical patent/SU600213A1/en

Description

фита и повысить срок анодов магниевых электролизеров. Все это приводит к снижению расхода графита, электроэнергии и трудозатрат при производстве магни .fit and increase the life of the anodes of magnesium electrolyzers. All this leads to a decrease in the consumption of graphite, electricity and labor costs in the production of magnesium.

Claims (2)

1. Способ защиты анодов магниевых электролизеров от разрушени , включаюш;ий уплотнение зазоров между анодами и перекрытием асбестовым шнуром и засыпку пространства между анодами и перекрытием сыпучим веществом перед пуском электролизера, отличающийс  тем, что, с целью увеличени 1. A method of protecting anodes of magnesium electrolysis cells from destruction, including sealing of the gaps between the anodes and the overlapping with asbestos cord and filling the space between the anodes and the overlapping of the bulk before starting the electrolyzer, characterized in that срока службы анодов, засыпают тонкомолотый фтористый кальций, а после пуска электролизера на фтористый, кальций заливают расплавленный материал о температурой плавлени  300-450° С.the life of the anodes, poured finely ground calcium fluoride, and after the start of the electrolyzer on the fluoride, calcium pour molten material about the melting point of 300-450 ° C. 2. Способ по п. 1, отличающийс  тем, что заливают безводный карналлит с содержанием в нем хлористого натри  5-20%.2. A method according to claim 1, characterized in that anhydrous carnallite is poured in with sodium chloride content of 5-20%. Источники информации, прин тые во внимание при экспертизе Sources of information taken into account in the examination 1.Авторское свидетельство СССР № 259397, кл. С 25С 3/04, 1968.1. USSR author's certificate No. 259397, cl. C 25 C 3/04, 1968. 2.Авторское свидетельство СССР № 492593, кл. С 25С 3/04, 1974.2. USSR author's certificate number 492593, cl. C 25 C 3/04, 1974.
SU752191814A 1975-11-18 1975-11-18 Method of protecting magnesium electrolyzer anodes from destruction SU600213A1 (en)