SU464926A1 - The method of mixing the electrolyte in the battery - Google Patents

The method of mixing the electrolyte in the battery

Info

Publication number
SU464926A1
SU464926A1 SU1927658A SU1927658A SU464926A1 SU 464926 A1 SU464926 A1 SU 464926A1 SU 1927658 A SU1927658 A SU 1927658A SU 1927658 A SU1927658 A SU 1927658A SU 464926 A1 SU464926 A1 SU 464926A1
Authority
SU
USSR - Soviet Union
Prior art keywords
electrolyte
battery
mixing
air
bubbles
Prior art date
Application number
SU1927658A
Other languages
Russian (ru)
Inventor
Рудольф Сергеевич Лепилин
Сергей Викторович Волков
Алексей Иванович Русин
Original Assignee
Куйбышевский политехнический институт им. В.В. Куйбышева
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Куйбышевский политехнический институт им. В.В. Куйбышева filed Critical Куйбышевский политехнический институт им. В.В. Куйбышева
Priority to SU1927658A priority Critical patent/SU464926A1/en
Application granted granted Critical
Publication of SU464926A1 publication Critical patent/SU464926A1/en

Description

1one

Изобретение относитс  к электротехнике.The invention relates to electrical engineering.

В крупногабаритных аккумул торах при их работе происходит расслоение электролита , в результате чего плотность его по высоте аккумул тора оказываетс  неодинаковой. Это приводит к ухудшению электрических характеристик аккумул торов.In large-sized batteries, during their work, electrolyte separation occurs, as a result of which its density along the height of the battery is uneven. This leads to a deterioration in the electrical characteristics of the batteries.

Дл  предотвращени  расслоени  электролита его перемешивают путем пропускани  воздуха снизу вверх. Поднимающиес  пузырьки воздуха перемешивают электролит.To prevent separation of the electrolyte, it is stirred by passing air from the bottom up. Rising air bubbles mix electrolyte.

Однако при использовании известного способа объем электролита насыщаетс  пузырьками воздуха, что приводит к увеличению внутреннего сопротивлени  аккумул тора, т. е. к ухудшению его характеристик. Кроме того, пузырьки оказывают механическое воздействие на электроды, вызыва  ускоренное оплывание активной массы, что сокращает срок службы аккумул тора.However, when using a known method, the electrolyte volume is saturated with air bubbles, which leads to an increase in the internal resistance of the battery, i.e., to a deterioration of its characteristics. In addition, bubbles have a mechanical effect on the electrodes, causing accelerated discharging of the active mass, which shortens the life of the battery.

Целью изобретени   вл етс  снижение внутреннего сопротивлени  и повышение срока службы аккумул тора.The aim of the invention is to reduce internal resistance and increase battery life.

Дл  этого воздух пропускают внутри вертикальной трубки, расположенной в электролите . Воздух подвод т в нижнюю часть вертикальной трубки, начинающейс  у дна аккумул тора . Двига сь по трубке в виде пузырей, воздух поднимает наход щийс  между нузыр ми электролит в верхнюю часть аккумул тора . Таким образом исключаетс  попаданиеFor this, air is passed inside a vertical tube located in the electrolyte. Air is introduced into the lower part of the vertical tube, starting at the bottom of the battery. Moving through the tube in the form of bubbles, the air lifts the electrolyte between the bubbles to the top of the battery. This prevents the entry

пузырьков воздуха в электролит и мехаиическое воздействие их на электроды.air bubbles in the electrolyte and their mechanical effect on the electrodes.

Предмет изобретени Subject invention

Способ перемешивани  электролита в аккумул торе путем пропускани  воздуха снизу вверх, отличающийс  тем, что, с целью снижени  внутреннего сопротивлени  и повышени  срока службы, воздуТс пропускают внутри вертикальной трубки, расположенной в электролите.The method of mixing the electrolyte in the battery by passing air from the bottom up, characterized in that, in order to reduce internal resistance and increase the service life, air is passed inside a vertical tube located in the electrolyte.

SU1927658A 1973-06-04 1973-06-04 The method of mixing the electrolyte in the battery SU464926A1 (en)