SU455151A1 - Method of tanning leather - Google Patents
Method of tanning leatherInfo
- Publication number
- SU455151A1 SU455151A1 SU1721437A SU1721437A SU455151A1 SU 455151 A1 SU455151 A1 SU 455151A1 SU 1721437 A SU1721437 A SU 1721437A SU 1721437 A SU1721437 A SU 1721437A SU 455151 A1 SU455151 A1 SU 455151A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- tanning leather
- formaldehyde
- tanning
- skin
- carried out
- Prior art date
Description
1one
Изобретение относитс к кожевенной промышленности .The invention relates to the leather industry.
Известно дубление кож лигносульфоновыми дуб щими сульфитспиртовой барды, но при этом наблюдаетс незначительное повышение температуры сваривани , кожа приобретает некоторую жестеобразность и способность к короблению.Leather tanning with lignosulfone tanning sulfite-alcohol stillage is known, but a slight increase in the welding temperature is observed, and the skin acquires some stiffness and warping ability.
Цель изобретени - улучшение качества кожи.The purpose of the invention is to improve the quality of the skin.
Это достигаетс за счет того, что обработку сульфитспиртовой бардой .ведут в присутствии формальдегида с последующим добавлением в раствор -сернокислой соли, а в качестве последней используют сульфат хрома или алюмини .This is achieved due to the fact that the treatment with sulfite alcohol barda will be carried out in the presence of formaldehyde and then added to the solution of sulfuric acid salt, and chromium or aluminum sulfate is used as the latter.
Способ осуществл етс следующим образом.The method is carried out as follows.
Голье после пикелевани или частичного хромировани обрабатывают сульфитспиртовой бардой в присутствии формальдегида при температуре 35-40°С, рН 7,0-7,2 в течение 20-24 час. Количество формальдегида составл ет ) 0,8-2% от веса голь .After pickleing or partial chrome plating, the scorch is treated with sulfite-alcohol barda in the presence of formaldehyde at a temperature of 35-40 ° C, pH 7.0-7.2 for 20-24 hours. The amount of formaldehyde is 0.8-2% by weight mole.
По истечении этого времени добавл ют сульфат хрома или алюмини в количестве 0,6- 3% от веса голь в пересчете на СггОз.After this time, chromium or aluminum sulphate in an amount of 0.6-3% by weight mole in terms of CrO2 is added.
Через 2 час корректируют величину рН (в зависимости от назначени кожи), обработку продолжают 15-20 час, после чего ввод т кальцинированную соду (0,4-0,5%) и дальнейшую обработку производ т известным способом .After 2 hours, the pH value is adjusted (depending on the purpose of the skin), the treatment is continued for 15-20 hours, after which the soda ash (0.4-0.5%) is introduced and further processing is carried out in a known manner.
10ten
Предмет изобретени Subject invention
Claims (2)