SU378544A1 - METHOD OF ELECTROLYTIC DEPOSITION OF ZINCAL ALLOYS21Avooh-known: b-alloying of alloys; w • zinc; pH = 7—10, a temperature of 20 + 5 ° C and a current density of 01–30 a / dm ^. Long equilibrium allows to obtain an alloy of cnc – kashmiy – gnickel – jo, balt, which, compared to the known, has an increase in hardness and iznostoy, bone. The proposed apasob differs from the well-known in that the electrolyte "water alt sulphate in determining the content kom1ponento1v. - Google Patents

METHOD OF ELECTROLYTIC DEPOSITION OF ZINCAL ALLOYS21Avooh-known: b-alloying of alloys; w • zinc; pH = 7—10, a temperature of 20 + 5 ° C and a current density of 01–30 a / dm ^. Long equilibrium allows to obtain an alloy of cnc – kashmiy – gnickel – jo, balt, which, compared to the known, has an increase in hardness and iznostoy, bone. The proposed apasob differs from the well-known in that the electrolyte "water alt sulphate in determining the content kom1ponento1v.

Info

Publication number
SU378544A1
SU378544A1 SU1332543A SU1332543A SU378544A1 SU 378544 A1 SU378544 A1 SU 378544A1 SU 1332543 A SU1332543 A SU 1332543A SU 1332543 A SU1332543 A SU 1332543A SU 378544 A1 SU378544 A1 SU 378544A1
Authority
SU
USSR - Soviet Union
Prior art keywords
zincal
kashmiy
iznostoy
gnickel
apasob
Prior art date
Application number
SU1332543A
Other languages
Russian (ru)
Inventor
что осаждение сплава цинк дмий никель кобальт производ элвкт ролите содержащем Цинк сернокислый Кадмий сернокислый Никель сернокислый Ний серно ислый Полиэтиленполиамин Кобальт сернокислый гори температуре плотности тока При осуществлении способа исттользуют аноды сплава цинк Способ состоит том
Original Assignee
Способ эле ктр лити чеакого осаждени сплавов цинка электролите, сскдержащем сернокислые соли цинка, кадими , никел лиэтиленполиамин, аммюиий сернокислый при , плотности тока отличающийс тем, что, целью получени оцла кад мий никель бальт, электролит ввод кобальт сернокис
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Способ эле ктр лити чеакого осаждени сплавов цинка электролите, сскдержащем сернокислые соли цинка, кадими , никел лиэтиленполиамин, аммюиий сернокислый при , плотности тока отличающийс тем, что, целью получени оцла кад мий никель бальт, электролит ввод кобальт сернокис filed Critical Способ эле ктр лити чеакого осаждени сплавов цинка электролите, сскдержащем сернокислые соли цинка, кадими , никел лиэтиленполиамин, аммюиий сернокислый при , плотности тока отличающийс тем, что, целью получени оцла кад мий никель бальт, электролит ввод кобальт сернокис
Priority to SU1332543A priority Critical patent/SU378544A1/en
Application granted granted Critical
Publication of SU378544A1 publication Critical patent/SU378544A1/en

Description

лый при следующем садаржании компонентов в г1л: Ци к сериакЕслый100-150 Кадмий сернокислый10-18 Никель сернокислый3-5 Аммоний сбрнокислый200-250 Полиэтилввполиамин150-200 Кобальт сернокислый2-3The following components are boiled down into g1l: Qi to shiakEslyy100-150 Cadmium sulphate 10-18 Nickel sulphate3-5 Ammonium sulphate200-250 Polyethylene in polyamine 150-200 Cobalt sulphate2-3

SU1332543A 1969-05-19 1969-05-19 METHOD OF ELECTROLYTIC DEPOSITION OF ZINCAL ALLOYS21Avooh-known: b-alloying of alloys; w • zinc; pH = 7—10, a temperature of 20 + 5 ° C and a current density of 01–30 a / dm ^. Long equilibrium allows to obtain an alloy of cnc – kashmiy – gnickel – jo, balt, which, compared to the known, has an increase in hardness and iznostoy, bone. The proposed apasob differs from the well-known in that the electrolyte "water alt sulphate in determining the content kom1ponento1v. SU378544A1 (en)