SU126205A1 - Surface hardening method - Google Patents

Surface hardening method

Info

Publication number
SU126205A1
SU126205A1 SU366267A SU366267A SU126205A1 SU 126205 A1 SU126205 A1 SU 126205A1 SU 366267 A SU366267 A SU 366267A SU 366267 A SU366267 A SU 366267A SU 126205 A1 SU126205 A1 SU 126205A1
Authority
SU
USSR - Soviet Union
Prior art keywords
hardened
heating
surface hardening
inductor
teeth
Prior art date
Application number
SU366267A
Other languages
Russian (ru)
Inventor
А.С. Борщева
Original Assignee
А.С. Борщева
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.С. Борщева filed Critical А.С. Борщева
Priority to SU366267A priority Critical patent/SU126205A1/en
Application granted granted Critical
Publication of SU126205A1 publication Critical patent/SU126205A1/en

Description

Известен способ поверхностной закалкп стальных деталей токами высокой частоты, перемещаемых относительно нагревательного индуктора с последовательным нагревам участков закаливаемой поверхности с применением жидких охладителей.The known method of surface hardening of steel parts by high-frequency currents moving relative to the heating inductor with sequential heating of the areas of the hardened surface using liquid coolers.

Описываемый способ поверхностной закалки стальных деталей токами высокой частоты отличаетс  от известных тем, что закалка производитс  без охлаждающей жидкости за счет отдачи тепла от нагретых участков .детали - не нагретым участкам.The described method of surface hardening of steel parts by high-frequency currents differs from the known ones in that quenching is performed without a coolant due to the release of heat from the heated sections. The parts to the non-heated sections.

Перемеща  закаливаемую деталь со скоростью, обеспечивающей необходимый нагрев детали под индуктором и теплоотдачу остальной массе закаливаемой детали по выходе из-под индуктора.Moving the hardened part at a speed that provides the necessary heating of the part under the inductor and heat transfer to the rest of the mass of the hardened part as it leaves the inductor.

С целью регулировани  теплоотдачи нагреваемой детали примен етс  или искусственное охлаждение стола, на котором устанавливаетс  закаливаема  деталь, или теплова  изол ци  среды, или подогрев детали.In order to regulate the heat transfer of the heated part, either artificial cooling of the table on which the part is being hardened, or thermal insulation of the medium, or heating the part is used.

Поверхностна  закалка зубьев шестерен производитс  при помощи петлевого индуктора, а нагрев зубьев производ т поочередно через каждые два-три зуба.The surface hardening of the gear teeth is done using a loop inductor, and the teeth are heated alternately every two to three teeth.

Скорость перемещени  закаливаемой детали определ ют по цветам побежалости, а глубину сло  поверхностной закалки - по ширине дорожек цветов побежалости.The speed of movement of the hardened part is determined by the colors of the tint, and the depth of the layer of surface hardening is determined by the width of the paths of the colors of the tint.

Предложение практически проверено в производственной практике и может быть широко применено в различных отрасл х промьппленности .The offer has been practically tested in production practice and can be widely applied in various industries.

. Предмет изобретени . Subject invention

Claims (4)

1. Способ поверхностной закалки стальных деталей, перемещаемых относительно нагревательного индуктора, с последовательным нагревом участков закаливаемой поверхности, отличающийс  тем, что, с целью упрощени  технологии закалки, повышени  качества и расшиМ 126205- 2 рени  возможностей ее применени , производ т закалку без охлаждающей жидкости, перемеща  закаливаемую деталь с такой скоростью, чтобы обеспечить необходимый нагрев закаливаемой детали под индуктором и теплоотдачу остальной массе закаливаемой детали по выходе из-под индуктора.1. The method of surface hardening of steel parts moving relative to the heating inductor, with sequential heating of the areas of the hardened surface, characterized in that, in order to simplify the hardening technology, improve the quality and expand its application possibilities, quenching is performed without coolant, moving the hardened part at such a rate as to provide the necessary heating of the hardened part under the inductor and heat transfer to the rest of the mass of the hardened part as it leaves the inductive part a. 2.Прием выполнени  по п. 1, отличающийс  тем, что, с целью регулировки теплоотдачи нагреваемой детали, примен ют или искусственное охлаждение стола, на котором установлена деталь, или тепловую изол цию среды, или подогрев детали.2. A method according to claim 1, characterized in that, in order to adjust the heat transfer of the heated part, either artificial cooling of the table on which the part is installed, or thermal insulation of the medium, or heating the part is used. 3.Прием выполнени  способа по п. Л, о,т,лл  аю щи и с   тем, что при поверхностной закалке шестерен без охлажд-ающей жидкости, нагрев зубьев производ т поочередно через каждые, два-три зуба при помощи петлевого индуктора.3. Acceptance of the method according to p. L, o, t, l ay shchi and the fact that during the surface hardening of gears without a cooling liquid, the teeth are heated alternately after every two or three teeth with the help of a loop inductor. 4.Прием выполнени  способа по п. 1, отличающийс  тем, что скорость движени  закаливаемой детали определ ют по цветам побежалости , а глубину сло  поверхностной закалки - по гпирине дорожек цветов побежа,пости.4. A method according to claim 1, characterized in that the speed of movement of the hardened part is determined by the colors of tinge, and the depth of the surface hardening layer is determined by the width of the paths of the colors of the run, post.
SU366267A 1948-12-23 1948-12-23 Surface hardening method SU126205A1 (en)