SU83281A1 - The method of strengthening of steel and cast iron parts - Google Patents
The method of strengthening of steel and cast iron partsInfo
- Publication number
- SU83281A1 SU83281A1 SU395103A SU395103A SU83281A1 SU 83281 A1 SU83281 A1 SU 83281A1 SU 395103 A SU395103 A SU 395103A SU 395103 A SU395103 A SU 395103A SU 83281 A1 SU83281 A1 SU 83281A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- cast iron
- steel
- iron parts
- strengthening
- electric
- Prior art date
Description
Известны различные способы упрочнени стальных и чугунных деталей нанесением твердого сплава на поверхность издели , например, электроискровым методом. Издели после наплавки твердого сплава подвергаютс термообработке путем нагрева их в печи и последующего охлаждени .There are various methods of hardening steel and cast iron parts by applying a solid alloy on the surface of the product, for example, by the electric-spark method. The products after hard metal surfacing are subjected to heat treatment by heating them in a furnace and subsequent cooling.
Предлагаемый способ упрочнени стальных и чугунных деталей предусматривает нанесение твердого сплава на поверхность издели электроискровым методом, с помощью электровибратора, но с последующей термической обработкой издели пламенем электрической дуги от того же прибора, которым производилось покрытие поверхности твердым сплавом.The proposed method of hardening steel and cast iron parts involves applying a hard alloy to the surface of the product using an electric-spark method using an electrovibrator, but with subsequent thermal treatment of the product with an electric arc flame from the same device that was used to coat the surface with a hard alloy.
Режим покрыти поверхности издели твердым сплавом осущеставл етс напр жением 200-250 в, с силой тока 8-10 а. Термическа обработка наплавленной поверхности производитс на том же электровибраторе при том же дуговом разр де посредством отключени емкости от электроискровой установки.The mode of coating the surface of the product with a hard alloy is realized with a voltage of 200-250 V, with a current strength of 8-10 a. Thermal treatment of the weld surface is performed on the same electric vibrator at the same arc discharge by disconnecting the capacitance from the electric-spark installation.
Предмет изобретени Subject invention
Способ упрочнени стальных и чугунных деталей, о т л п ч а ю щ и йс тем, что, с целью повыщени прочности детали, нанесенный электроискровым методом слой твердого сплава подвергаетс кратковременной термической обработке вольтовой дугой, получаемой на TONT же электровибраторе.The method of hardening steel and cast iron parts is about the fact that, in order to increase the strength of the part, the layer of hard alloy applied by the electric-spark method undergoes a short-term heat treatment with a volt arc obtained on a TONT electrovibrator.