SE505141C2 - Syrgasdelignifiering av massa i två steg med hög satsning av alkali och syrgas och temperatur under 90 C i första steget - Google Patents

Syrgasdelignifiering av massa i två steg med hög satsning av alkali och syrgas och temperatur under 90 C i första steget

Info

Publication number
SE505141C2
SE505141C2 SE9503720A SE9503720A SE505141C2 SE 505141 C2 SE505141 C2 SE 505141C2 SE 9503720 A SE9503720 A SE 9503720A SE 9503720 A SE9503720 A SE 9503720A SE 505141 C2 SE505141 C2 SE 505141C2
Authority
SE
Sweden
Prior art keywords
pulp
oxygen
delignification
temperature
alkali
Prior art date
Application number
SE9503720A
Other languages
English (en)
Other versions
SE9503720D0 (sv
SE9503720L (sv
Inventor
Monica Bokstroem
Pia Mellander
Solveig Norden
Original Assignee
Sunds Defibrator Ind Ab
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=20399927&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=SE505141(C2) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Application filed by Sunds Defibrator Ind Ab filed Critical Sunds Defibrator Ind Ab
Priority to SE9503720A priority Critical patent/SE505141C2/sv
Publication of SE9503720D0 publication Critical patent/SE9503720D0/sv
Priority to DE69630803T priority patent/DE69630803T2/de
Priority to JP51652197A priority patent/JP3459072B2/ja
Priority to CN96197756A priority patent/CN1072743C/zh
Priority to PCT/SE1996/001154 priority patent/WO1997015715A1/en
Priority to AU73483/96A priority patent/AU691132B2/en
Priority to CA002231048A priority patent/CA2231048C/en
Priority to ES96935649T priority patent/ES2206598T3/es
Priority to NZ320687A priority patent/NZ320687A/en
Priority to AT96935649T priority patent/ATE254687T1/de
Priority to EP96935649A priority patent/EP0857231B1/en
Priority to BR9611243A priority patent/BR9611243A/pt
Priority to RU98109942A priority patent/RU2148118C1/ru
Priority to PT96935649T priority patent/PT857231E/pt
Priority to ZA967932A priority patent/ZA967932B/xx
Priority to MYPI96003947A priority patent/MY117900A/en
Publication of SE9503720L publication Critical patent/SE9503720L/sv
Publication of SE505141C2 publication Critical patent/SE505141C2/sv
Priority to US08/927,925 priority patent/US6221206B1/en
Priority to NO19981794A priority patent/NO324111B1/no
Priority to US09/759,032 priority patent/US6319357B1/en
Priority to US09/886,913 priority patent/US6454900B2/en

Description

505 141 2 Förfarandet innebär således att delignifieringen utföres i två på varandra följande steg. I den första mixern 2 görs såväl en hög alkalitillsats som en hög syrgastillsats.
Detta innebär en satsning av 25-50 kg alkali (NaOH) per ton massa, företrädesvis 25-35 kg/ton. Eventuellt kan denna erfor- derliga alkalisats delvis erhållas genom överbäring från brunmassatvätten. Satsningen i mixern 2 kan då minskas i motsvarande grad. Syrgassatsningen skall vara 25-50 kg/ton I massa, företrädesvis 30-40 kg/ton.
Temperaturen på massan vid inmatningen i reaktorn 3 skall vara under 90°C, företrädesvis 75-90°C. Detta innebär att reaktionen i det första steget i reaktorn 3 kan utföras vid den temperatur massan har från brunmassatvätten. Uppehållstiden i reaktorn 3 skall vara relativt kort, 10-30 min, företrädesvis 15-25 min.
I den första reaktorn 3 skall trycket vara 4-10 bar.
Tillsammans med massans höga alkalitet och den höga syrgassats- ningen medför det höga trycket en hög delignifieringshastighet.
Samtidigt hålls hastigheten för cellulosanedbrytningen på låg nivå genom den relativt låga temperaturen och korta uppehålls- tiden.
Efter det första delignifieringssteget i den första reaktorn 3 förs massan till det andra delignifieringssteget i den andra reaktorn 6. Temperaturn i den andra reaktorn 6 skall vara över 90°C, dvs högre än i den första reaktorn 3. Tempera- turskillnaden skall dock vara mindre än 20°C, företrädesvis 10-15°C. För att åstadkomma den erforderliga temperaturhöjning- en tillförs ånga i den andra mixern 5.
Trycket i den andra reaktorn 6 skall vara 2-5 bar och lägre än i den första reaktorn 3. Uppehållstiden bör vara relativt lång, 45-180 min, företrädesvis 60-120 min.
Det andra delignifieringssteget är främst ett långt extraktionssteg där, i förhållande till första steget, den förhöjda temperaturen och den förlängda uppehållstiden ger förlängd delignifiering. Vid temperaturer över 90°C erhålles således god extraktion/lakningshastighet.
Genom att ingen ytterligare alkalisats görs i det andra steget, inte ens för att kompensera förbrukningen i det första steget, kan massans alkalitet hållas relativt låg i det andra - 505 141 J steget. Därigenom undviks huvudsakligen cellulosanedbrytning trots hög temperatur och lång uppehållstid.
I den andra mixern 5 kan eventuellt en liten mängd syrgas tillsättas. Satsningen kan vara upp till 5 kg/ton massa.
Därigenom kan syrgassatsningen i det första steget kompletteras för att höja syrgasens partialtryck.
Uppehàllstiden i det andra steget bestäms relativt temperaturen för att uppnå bästa resultat, dvs avsedd förlängd delignifiering utan försämring av massaegenskaperna. Högre temperatur innebär således kortare uppehàllstid.
Uppfinningen är givetvis inte begränsad till beskrivna utföranden utan kan varieras inom ramen för uppfinningstanken.

Claims (4)

505 141 4 Patentkrav
1. Förfarande för syrgasdelignifiering av massa av ligno- cellulosahaltigt material vid medelkoncentration i två steg, k ä n n e t e c k n a t av att en förlängd delignifiering àstadkommes genom att temperaturen i det första steget hålls under 90°C och i det andra steget över 90°C varvid temperatur- skillnaden mellan stegen understiger 20°C, att trycket i det första steget är 4-10 bar och i det andra steget 2-5 bar varvid trycket i det första steget år högre än i det andra steget, att syrgastillsatsen till det första steget år hög, 25-50 kg/ton massa, att alkali tillsätts enbart till det första steget för att uppnå en hög alkalitet i massan, 25-50 kg alkali per ton massa, samt att uppehàllstiden i det första steget är 10-30 min och i det andra steget 45-180 min.
2. Förfarande enligt kravet 1, k ä n n e t e c k n a t av att temperaturhöjningen mellan de båda syrgasstegen är 10-l5°C.
3. Förfarande enligt något av föregående krav, k ä n n e t e c k n a t av att massans uppehållstid i det första steget är 15-25 min och i det andra steget 60-120 min.
4. Förfarande enligt något av föregående krav, k ä n n e t e c k n a t av att ytterligare syrgas satsas i en mängd av 0-5 kg/ton massa till det andra steget
SE9503720A 1995-10-23 1995-10-23 Syrgasdelignifiering av massa i två steg med hög satsning av alkali och syrgas och temperatur under 90 C i första steget SE505141C2 (sv)