RU97102229A - Способ получения шинного регенерата - Google Patents
Способ получения шинного регенератаInfo
- Publication number
- RU97102229A RU97102229A RU97102229/04A RU97102229A RU97102229A RU 97102229 A RU97102229 A RU 97102229A RU 97102229/04 A RU97102229/04 A RU 97102229/04A RU 97102229 A RU97102229 A RU 97102229A RU 97102229 A RU97102229 A RU 97102229A
- Authority
- RU
- Russia
- Prior art keywords
- mixing
- crumb
- rubber
- ingredients
- devulcanization
- Prior art date
Links
- 229920001971 elastomer Polymers 0.000 claims 6
- KHPCPRHQVVSZAH-HUOMCSJISA-N Rosin Natural products O(C/C=C/c1ccccc1)[C@H]1[C@H](O)[C@@H](O)[C@@H](O)[C@@H](CO)O1 KHPCPRHQVVSZAH-HUOMCSJISA-N 0.000 claims 4
- 239000012190 activator Substances 0.000 claims 4
- 239000004615 ingredient Substances 0.000 claims 4
- 239000010426 asphalt Substances 0.000 claims 2
- 238000002844 melting Methods 0.000 claims 2
- 239000000203 mixture Substances 0.000 claims 2
- 229920002209 Crumb rubber Polymers 0.000 claims 1
- 238000004140 cleaning Methods 0.000 claims 1
- 238000007670 refining Methods 0.000 claims 1
Claims (2)
1. Способ получения шинного регенератора, включающий смешение ингредиентов с резиновой шинной крошкой и девулканизацию механодеструкцией в присутствии активаторов с последующей очисткой регенерата на рафинирующих вальцах, отличающийся тем, что смешение резиновой шинной крошки с ингредиентами и активаторами производят в смесителе для сыпучих компонентов при температуре 25 ± 10oC; усреднение смеси, плавление тугоплавких компонентов и частичную девулканизацию производят в кулачковом экструдере при температуре 70-100oC, девулканизацию заканчивают на регенератно-смесительных, смесительно-листовальных вальцах при температуре 30-60oC или смешение резиновой крошки с ингредиентами и активаторами, усреднение смеси, плавление тугоплавких компонентов и девулканизацию производят на регенератно-смесительных, смесительно-листовальных вальцах при температуре 30-60oC.
2. Способ получения шинного регенерата по п. 1, отличающийся тем, что в качестве резиновой шинной крошки используют резиновую крошку, полученную бародеструкционным измельчением шин, при этом в качестве ингредиентов при смешении с резиновой крошкой используют канифоль и битум при следующем соотношении компонентов, мас.ч.:
Резиновая шинная крошка - 100,0
Активатор - 0,3 - 0,5
Канифоль - 2,0 - 6,0
Битум - 5,0 - 15,0
Резиновая шинная крошка - 100,0
Активатор - 0,3 - 0,5
Канифоль - 2,0 - 6,0
Битум - 5,0 - 15,0