PL431928A1 - Composition of the low-cement grout - Google Patents

Composition of the low-cement grout

Info

Publication number
PL431928A1
PL431928A1 PL431928A PL43192819A PL431928A1 PL 431928 A1 PL431928 A1 PL 431928A1 PL 431928 A PL431928 A PL 431928A PL 43192819 A PL43192819 A PL 43192819A PL 431928 A1 PL431928 A1 PL 431928A1
Authority
PL
Poland
Prior art keywords
parts
composition
low
cement
cement grout
Prior art date
Application number
PL431928A
Other languages
Polish (pl)
Inventor
Marcian Kremieniewski
Marcin Rzepka
Miłosz Kędzierski
Ewa Kątna
Szczepan Filip
Łukasz Kut
Original Assignee
Instytut Nafty I Gazu - Państwowy Instytut Badawczy
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Instytut Nafty I Gazu - Państwowy Instytut Badawczy filed Critical Instytut Nafty I Gazu - Państwowy Instytut Badawczy
Priority to PL431928A priority Critical patent/PL431928A1/en
Publication of PL431928A1 publication Critical patent/PL431928A1/en

Abstract

Przedmiotem zgłoszenia jest kompozycja zaczynu niskocementowego na bazie wody zarobowej, cementu oraz krzemionki, która charakteryzuje się tym, że zawiera w stosunku do ilości wody zarobowej 100 cz. wag. Mieszaniny, składającej się z 50 – 75% cementu i 25 - 50 mączki krzemionkowej oraz od 0,8 do 1,2 cz. wag. rozdrobnionej glinki bentonitowej oraz od 0,8 do 1,2 cz. wag. Dyspersji koloidalnej krzemionki, a także od 0,8 do 1,2 cz. wag. wodorotlenku sodu i od 0,2 do 0,4 cz. wag. Eteru polikarboksylowego.The subject of the application is a composition of a low-cement slurry based on make-up water, cement and silica, which is characterized by the fact that it contains 100 parts in relation to the amount of make-up water. wt. A mixture consisting of 50 - 75% cement and 25 - 50 silica flour and from 0.8 to 1.2 parts. wt. ground bentonite clay and from 0.8 to 1.2 parts. wt. Colloidal silica dispersion, as well as from 0.8 to 1.2 parts wt. sodium hydroxide and from 0.2 to 0.4 parts wt. Polycarboxylic ether.

PL431928A 2019-11-25 2019-11-25 Composition of the low-cement grout PL431928A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL431928A PL431928A1 (en) 2019-11-25 2019-11-25 Composition of the low-cement grout

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL431928A PL431928A1 (en) 2019-11-25 2019-11-25 Composition of the low-cement grout

Publications (1)

Publication Number Publication Date
PL431928A1 true PL431928A1 (en) 2021-05-31

Family

ID=76132961

Family Applications (1)

Application Number Title Priority Date Filing Date
PL431928A PL431928A1 (en) 2019-11-25 2019-11-25 Composition of the low-cement grout

Country Status (1)

Country Link
PL (1) PL431928A1 (en)

Similar Documents

Publication Publication Date Title
EA201991989A1 (en) CARBONIZABLE CEMENTS AND CONCRETES BASED ON CALCIUM SILICATE, CONTAINING MINERAL ADDITIVES AND THEIR METHODS
MX2016014254A (en) Concrete materials with modified rheology, methods of making, and uses thereof.
NZ630005A (en) Settable compositions comprising unexpanded perlite and methods of cementing in subterranean formations
EP2085368A3 (en) Joint mortar especially for shaped clinker bricks
JP6404629B2 (en) High fluidity retention type underwater non-separable grout composition
BR112016029622A2 (en) ultra high performance non-self-consolidating concrete
RU2013139856A (en) HYDRAULIC BINDER WITH LOW CONTENT OF CLINKER
KR101354249B1 (en) A composite of hauyne cement by using fly ash of fluidize-bed boiler and manufacturing method thereof
PL431928A1 (en) Composition of the low-cement grout
JP6306973B2 (en) High fluidity retention type low exothermic grout composition
CN104743997A (en) Quick and high-efficiency leaking stoppage agent
RU2553667C1 (en) Preparation method of portland cement binding agent with addition of high-lime ash of thermal power plants
CN106082726A (en) Environment protecting cement formula
PL426989A1 (en) Composition of ultra-lightweight cement slurry
PL421250A1 (en) Composition of the low-settling cement-latex grout with water-glass addition
CN109180045A (en) A kind of mineral admixture
PL422054A1 (en) Hydraulic road binder and method for producing it and the cementitious hydraulic binder and method for producing it
KR20150022189A (en) Concrete binder and Process thereof
PL418792A1 (en) Protective plaster mortar
PL430180A1 (en) Composition of aluminium sealing grout
PL421676A1 (en) Composition of non-fractionating cement grout
PL420758A1 (en) Composition of sedimentation high-stability cement grout
CN105198245A (en) Alkali-activated slag cement
CN109912268A (en) Intumescent mortar formula
PL432018A1 (en) Self-hardening suspension based on phosphogypsum for applications in hydrotechnical construction and method for its production