KR930013153A - 스테인레스강 정련로 슬래그의 분화방지방법 - Google Patents

스테인레스강 정련로 슬래그의 분화방지방법 Download PDF

Info

Publication number
KR930013153A
KR930013153A KR1019910025129A KR910025129A KR930013153A KR 930013153 A KR930013153 A KR 930013153A KR 1019910025129 A KR1019910025129 A KR 1019910025129A KR 910025129 A KR910025129 A KR 910025129A KR 930013153 A KR930013153 A KR 930013153A
Authority
KR
South Korea
Prior art keywords
stainless steel
slag
differentiation
refining furnace
refining
Prior art date
Application number
KR1019910025129A
Other languages
English (en)
Other versions
KR940004820B1 (ko
Inventor
송효석
신영길
유병돈
윤석근
Original Assignee
정명식
포항종합제철 주식회사
백덕현
재단법인 산업과학기술연구소
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 정명식, 포항종합제철 주식회사, 백덕현, 재단법인 산업과학기술연구소 filed Critical 정명식
Priority to KR1019910025129A priority Critical patent/KR940004820B1/ko
Publication of KR930013153A publication Critical patent/KR930013153A/ko
Application granted granted Critical
Publication of KR940004820B1 publication Critical patent/KR940004820B1/ko

Abstract

본 발명은 스테인레스강 정련로 슬래그의 분화방지방법에 관한 것으로서, 최종제품의 [B]농도를 규제하는 스테인레스강 제조시에 사용할 수 있을 뿐만 아니라 스테인레스강 정련시 발생하는 슬래그의 분화를 효과적으로 방지할 수 있는 향상된 스테인레스강 정련로 슬래그의 분화방지방법을 제공하고자 하는데, 그 목적이 있다.
본 발명은 최종제품의 [B]농도를 규제하는 스테인레스강 제조방방법에 있어서, 정련후 발생하는 슬래그 중량에 대하여 3.5-5.0중량%의 세레스 타이트를 정련과정중 산화단계에서 정련로내에 투입하여 슬래그 분화를 방지하는 스테인레스강 정련로 슬래그의 분화방지방법에 관한 것이다.

Description

스테인레스강 정련로 슬래그의 분화방지방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 슬래그의 중량을 기준으로 하는 분화방지제 첨가율의 변화에 따른 슬래그분화율 변화를 나타내는 그래프.

Claims (1)

  1. 최종제품의 붕소 [B] 농도를 규제하는 스테인레스강 제조방법에 있어서, 정련후 발생하는 슬래그 중량에 대하여 3.5-5.0중량%의 세레스타이트를 정련과정중 산화단계에서 정련로내에 투입하여 슬래그 분화를 방지하는 스테인레스강 정련로 슬래그의 분화방지방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019910025129A 1991-12-30 1991-12-30 스테인레스강 정련로 슬래그의 분화방지방법 KR940004820B1 (ko)