KR910012390A - 방향족-지방족 폴리아미드 혼성섬유의 제조방법 - Google Patents
방향족-지방족 폴리아미드 혼성섬유의 제조방법 Download PDFInfo
- Publication number
- KR910012390A KR910012390A KR1019890019716A KR890019716A KR910012390A KR 910012390 A KR910012390 A KR 910012390A KR 1019890019716 A KR1019890019716 A KR 1019890019716A KR 890019716 A KR890019716 A KR 890019716A KR 910012390 A KR910012390 A KR 910012390A
- Authority
- KR
- South Korea
- Prior art keywords
- hybrid fiber
- aliphatic polyamide
- spinning
- producing aromatic
- dope
- Prior art date
Abstract
내용 없음
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
Claims (1)
- 방향족 폴리아미드와 지방족 폴리아미드를 혼용하여 방사도우프를 제조한 다음, 이를 응고욕으로 방사도우프를 제조한 다음, 이를 응고욕으로 방사시켜 응고시키면서 권취하고 수세, 건조 및 열처리하여서 방향족-지방족 폴리아미드 혼성섬유를 제조하는데 있어서, 다음 일반식(Ⅰ)로 표시되고 고유점도가 2.0 내지 3.0인 예비중합체용액 90 내지 97중량%와, 통상의 용융중합에 의하여 얻어진 다음 일반식(Ⅱ)로 표시되고 고유점도가 0.7이상인 지방족 폴리아미드 중합체 용액 3 내지 10중량%를 혼련하여 단일상의 액정도우프를 제조하고, 습식방사법을 이용하여 3급아민으로 이루어진 응고욕으로 방사하여 접촉시켜서 되는 것임을 특징으로 하는 방향족-지방족 폴리아미드 혼성섬유의 제조방법.윗 식에서, n은 20 내지 40이고, m은 500이상이다.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.