KR20110032233A - A metal exterior of a mobile apparatus and a method of preparing the same - Google Patents

A metal exterior of a mobile apparatus and a method of preparing the same Download PDF

Info

Publication number
KR20110032233A
KR20110032233A KR1020090089626A KR20090089626A KR20110032233A KR 20110032233 A KR20110032233 A KR 20110032233A KR 1020090089626 A KR1020090089626 A KR 1020090089626A KR 20090089626 A KR20090089626 A KR 20090089626A KR 20110032233 A KR20110032233 A KR 20110032233A
Authority
KR
South Korea
Prior art keywords
outer case
metal
portable device
plastic injection
injection molding
Prior art date
Application number
KR1020090089626A
Other languages
Korean (ko)
Other versions
KR101149177B1 (en
Inventor
김재경
김근하
엄요섭
Original Assignee
인탑스 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 인탑스 주식회사 filed Critical 인탑스 주식회사
Priority to KR1020090089626A priority Critical patent/KR101149177B1/en
Publication of KR20110032233A publication Critical patent/KR20110032233A/en
Application granted granted Critical
Publication of KR101149177B1 publication Critical patent/KR101149177B1/en

Abstract

PURPOSE: A metal exterior product of a mobile apparatus and a manufacturing method thereof are provided to easily perform the quality control of the metal exterior product by determining the positions of a coupling boss, a rib, and a hook. CONSTITUTION: A manufacturing method of a metal exterior product of a mobile apparatus is as follows. An outer case(100) and a coupling plastic molded material(200) of a metal exterior product are manufactured by processing a metal material with 150~300°C. The coupling plastic molded material is welded in the inner surface of the outer case.

Description

휴대용 기기의 금속 외장품 및 그 제조 방법{A METAL EXTERIOR OF A MOBILE APPARATUS AND A METHOD OF PREPARING THE SAME}Metal exterior of portable device and manufacturing method thereof {A METAL EXTERIOR OF A MOBILE APPARATUS AND A METHOD OF PREPARING THE SAME}

본 발명은 휴대용 기기의 금속 외장품 및 그 제조 방법에 관한 것이다. The present invention relates to a metal exterior of a portable device and a method of manufacturing the same.

근래 방송통신망 및 전자산업의 발달로 인해 휴대용 기기의 사용이 급속하게 늘고 있다. 특히 휴대용 전화기, PMP, 노트북 컴퓨터와 같이 사용시에 항상 외부로 노출되어 있어야 하며, 사용자가 손에 들고 있거나 사용자가 계속 손으로 조작하여야 하는 휴대용 기기의 경우, 휴대용 기기의 외관을 이루는 외부 케이스는 경량화, 고강도, 고신뢰성이 요구된다. 따라서 휴대용 기기 외부 케이스의 강도를 향상시키기 위해 강도가 높은 금속을 이용하는 예가 많아졌다.Recently, due to the development of broadcasting network and electronics industry, the use of portable devices is increasing rapidly. In particular, in case of a portable device such as a mobile phone, a PMP or a notebook computer, which must be exposed to the outside at all times and the user needs to keep it in hand or the user needs to operate it by hand, the external case forming the exterior of the portable device can be High strength and high reliability are required. Therefore, in order to improve the strength of the outer case of the portable device, there are many examples of using a high strength metal.

종래 금속을 이용한 휴대용 기기의 외부 케이스는 알루미늄이나 마그네슘을 다이캐스팅하여 제작되었다. 다이캐스팅을 이용하는 경우, 다른 부품을 수용할 수 있는 보스나 케이스의 다른 면과 결합을 위한 결합용 리브, 후크 등을 한 번에 형성할 수 있다는 장점이 있다. 그러나 알루미늄이나 마그네슘을 다이캐스팅하는 경우, 다이캐스팅 과정에서 기공이나 플로 마크(flow mark)가 발생하여 소재 불량이 발생하는 일이 잦고, 다이캐스팅 후에 후처리에 번거로운 작업이 필요하며, 후처리 시 가공 불량이 많아 불량품의 생산에 필요한 비용까지 산정할 경우 양산 시 고비용이 소요된다. 또한 후처리 중 생산물이 금속이므로 부식을 막기 위해 표면처리가 이루어져야 한다. The outer case of a conventional portable device using a metal is produced by die casting aluminum or magnesium. In the case of using die casting, there is an advantage in that it is possible to form a coupling rib, a hook, etc. for coupling with the other side of the boss or the case that can accommodate other components at once. However, when die-casting aluminum or magnesium, pores or flow marks occur during the die casting process, so that material defects frequently occur, and cumbersome work is required after post-casting. If the cost required for the production of defective products is estimated, mass production will be expensive. In addition, since the product is a metal during the post-treatment, surface treatment should be performed to prevent corrosion.

또한 종래 금속을 이용한 휴대용 기기의 외장품을 제작하는 다른 방법으로는, 금속 판재를 프레스 가공한 다음, 금속으로 결합용 보스, 리브, 후크 등을 외부 케이스의 내면에 용접하는 방법이 있었다. 그러나 조립을 위해 별도로 결합용 보스, 리브, 후크등을 제조하여 용접할 때, 각각의 위치를 정확히 맞추어 용접하는 것은 상당히 어려우며, 번거로운 공정이다. In addition, another method of manufacturing an exterior article of a portable device using a conventional metal was a method of pressing a metal sheet and then welding a joining boss, rib, hook, etc. with a metal to the inner surface of the outer case. However, when manufacturing separately welded bosses, ribs, hooks, etc. for assembly, it is quite difficult and cumbersome to weld each position accurately.

본 발명은 공정을 간소화하여 제조 단가를 낮출 수 있는 휴대용 기기의 외장품 및 그 제조 방법을 제공하는 것을 목적으로 한다.An object of the present invention is to provide an exterior article of a portable device and a method of manufacturing the same, which can simplify the process and lower the manufacturing cost.

또한 본 발명은 외부 케이스의 표면처리 이후 결합용 플라스틱 사출물을 부착하여, 금속 외부 케이스의 표면처리 방법을 자유롭게 선택할 수 있는 휴대용 기기의 외장품 및 그 제조 방법을 제공하는 것을 목적으로 한다.In addition, an object of the present invention is to provide an external article of the portable device and a method of manufacturing the same, by attaching a plastic injection molding for bonding after the surface treatment of the outer case, the free choice of the surface treatment method of the metal outer case.

또한 본 발명은 플라스틱 사출물과 외부 케이스가 서로 형상 결합하여 상대적인 위치가 결정됨에 따라 결합용 보스, 리브, 후크의 위치가 결정되고, 그에 따라 품질 관리가 용이한 휴대용 기기의 금속 외장품 및 그 제조 방법을 제공하는 것을 목적으로 한다. In addition, according to the present invention, as the plastic injection molding and the outer case are coupled to each other to determine a relative position, the position of the coupling boss, the rib, and the hook is determined. The purpose is to provide.

본 발명은 금속재료를 가공하여 외부 케이스 및 결합용 플라스틱 사출물을 각각 제조하는 단계 및 외부 케이스의 내면에 결합용 플라스틱 사출물을 접합하는 단계를 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법을 제공한다.The present invention is to manufacture a metal casing of a portable device, comprising the steps of manufacturing the outer case and the bonding plastic injection molding by processing a metal material, respectively, and bonding the bonding plastic injection molding to the inner surface of the outer case. Provide a method.

또한 본 발명의 다른 일 태양으로서, 금속 외장 제조 단계는, 판금 공정, 표면 후처리 공정 및 도장 공정을 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법을 제공한다.In another aspect of the present invention, the metal shell manufacturing step provides a method for manufacturing a metal shell of a portable device, comprising a sheet metal process, a surface post-treatment process and a painting process.

또한 본 발명의 다른 일 태양으로서, 판금 공정은, 금속재가 150℃ ~ 300℃ 에서 열간 프레스 성형되는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법을 제공한다.In still another aspect of the present invention, a sheet metal process provides a method of manufacturing a metal exterior part of a portable device, wherein the metal material is hot press formed at 150 ° C to 300 ° C.

또한 본 발명의 다른 일 태양으로서, 표면 후처리 공정은 비화성처리 피막(Non-chromate Anodizing)을 형성하는 공정을 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법을 제공한다.In still another aspect of the present invention, a surface post-treatment process provides a method for manufacturing a metal exterior of a portable device, the method comprising forming a non-chromate anodizing.

또한 본 발명의 다른 일 태양으로서, 표면 후처리 공정은 Ni 도금 과정을 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법을 제공한다.In another aspect of the present invention, a surface post-treatment process provides a method for manufacturing a metal enclosure of a portable device, characterized in that it comprises a Ni plating process.

또한 본 발명의 다른 일 태양으로서, 접합 단계의 전 단계에 외부 케이스를 도장하는 단계를 더 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법을 제공한다.In another aspect of the present invention, there is provided a method for manufacturing a metal exterior of a portable device, further comprising the step of painting the outer case before the bonding step.

또한 본 발명은 금속으로 제조되며, 휴대용 기기의 내장 전장품을 보호하는 외부 케이스, 외부 케이스 내면에 부착되며, 외부 케이스의 결합을 위한 결합용 리브 또는 결합용 돌기를 구비하는 결합용 플라스틱 사출물 및 외부 케이스와 결합용 플라스틱 사출물을 접합하는 접착제를 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제공한다.In addition, the present invention is made of a metal, the outer case to protect the built-in electronics of the portable device, attached to the inner surface of the outer case, the coupling plastic injection molding and the outer case having a coupling rib or coupling protrusion for the coupling of the outer case And it provides a metal exterior of the portable device comprising an adhesive for bonding the plastic injection for bonding.

또한 본 발명의 다른 일 태양으로서, 외부 케이스는, 스테인리스 스틸, 알루미늄, 두랄루민, 티타늄 및 마그네슘 중 어느 하나로 제조되는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제공한다.In still another aspect of the present invention, the outer case provides a metal enclosure of a portable device, which is made of any one of stainless steel, aluminum, duralumin, titanium, and magnesium.

또한 본 발명의 다른 일 태양으로서, 결합용 플라스틱 사출물은 외부 케이스 의 내측에 형상결합되도록 외부 케이스의 형상 및 크기에 대응하는 형상 및 크기를 가지는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제공한다.In another aspect of the present invention, the bonding plastic injection molding has a shape and a size corresponding to the shape and size of the outer case so as to be coupled to the inside of the outer case provides a metal exterior of the portable device.

본 발명이 제공하는 휴대용 기기의 금속 외장품 및 그 제조 방법은 공정을 간소화하여 제조 단가를 낮출 수 있다.The metal exterior part of the portable device provided by this invention and its manufacturing method can simplify manufacturing process, and can reduce manufacturing cost.

또한 본 발명이 제공하는 휴대용 기기의 금속 외장품 및 그 제조 방법은 외부 케이스의 표면처리 이후 결합용 플라스틱 사출물을 부착하여, 금속이 외부 케이스의 표면처리 방법을 자유롭게 선택할 수 있다.In addition, the metal exterior article of the portable device provided by the present invention and a method of manufacturing the same may be attached to the bonding plastic injection molding after the surface treatment of the outer case, the metal can freely select the surface treatment method of the outer case.

또한 본 발명이 제공하는 휴대용 기기의 금속 외장품 및 그 제조 방법은 플라스틱 사출물과 외부 케이스가 서로 형상 결합하여 상대적인 위치가 결정됨에 따라 결합용 보스, 리브, 후크의 위치가 결정되고, 그에 따라 품질 관리가 용이하다.In addition, the metal exterior of the portable device provided by the present invention and a method of manufacturing the plastic injection molded product and the outer casing shape relative to each other to determine the relative position of the coupling boss, ribs, hooks are determined, accordingly quality control Is easy.

도 1 내지 도 3은 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품이 휴대용 전화기에 적용된 모습을 도시한 도면이다. 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품은 외부 케이스(100)와 결합용 플라스틱 사출물(200)을 포함한다. 금속으로 제조된 외부 케이스(100)는 금속 판재를 프레스 가공한 다음, 도장, 표면처리 등을 거친 다음 결합용 플라스틱 사출물(200)이 접착된다. 외부 케이스(100)는 스테인리스 스틸(SUS), 두랄루민(Duralumin), 티타늄(Titanium), 마그네슘(Magnesium)결합용 플라스틱 사출물(200)에 결합용 보스(210), 리브(220), 후크(230) 등이 형성되기 때문에, 외부 케이스(100)의 내측에는 별도의 구조물이 형 성될 필요가 없다. 따라서 금속으로 외부 케이스(100)를 프레스 가공한 다음 표면처리를 할 때, 산화피막 형성(Anodizing) 비화성처리 피막 형성(Non-chromate Anodizing), UV도장, 우레탄 코팅 뿐 아니라 PVD 스퍼터링까지 표면처리 방법에 구애받지 않고 원하는 방법으로 외부 케이스(100)의 표면처리 방법을 선택하여 시행할 수 있다. 한편, 외부 케이스(100)와 결합용 플라스틱 사출물(200)은 서로 형상 결합 가능한 부분을 구비하여, 별도의 위치 선정 작업이 없이도 자연스럽게 상대적인 위치가 결정되도록 하는 것이 바람직하다. 예를 들어, 결합용 플라스틱 사출물(200)이 소정의 단차를 구비하고, 그 단차에 외부 케이스(100)의 단부가 위치됨으로써 상대적인 위치가 결정되도록 할 수 있다. 외부 케이스(100)와 결합용 플라스틱 사출물(200)은 경화용 접착제에 의해 접착된다. 경화용 접착제는 외부 케이스(100) 또는 결합용 플라스틱 사출물(200) 위에 얇게 도포된 다음, 서로 겹쳐지면서 접착된다. 1 to 3 are views illustrating a metal exterior of a portable device according to an embodiment of the present invention applied to a portable telephone. Metal exterior article of the portable device according to an embodiment of the present invention includes an outer case 100 and the coupling plastic injection molding (200). The outer case 100 made of metal is press-processed a metal plate, and then subjected to painting, surface treatment, and the like, and then the bonding plastic injection molding 200 is bonded. Outer case 100 is a stainless steel (SUS), duralumin (Duralumin), titanium (Titanium), magnesium (Magnesium) bonding plastic injection molding 200 for bonding bosses 210, ribs 220, hooks 230 Since the back is formed, it is not necessary to form a separate structure inside the outer case 100. Therefore, when surface treatment is performed after press working the outer case 100 with metal, anodizing, non-chromating anodizing, UV coating, urethane coating as well as PVD sputtering Regardless of the surface treatment method of the outer case 100 can be selected and implemented in a desired manner. On the other hand, the outer case 100 and the coupling plastic injection molding 200 is provided with a portion that can be coupled to each other, it is preferable to determine the relative position naturally without a separate positioning operation. For example, the bonding plastic injection molding 200 may have a predetermined step, and the end of the outer case 100 may be positioned at the step so that the relative position may be determined. The outer case 100 and the bonding plastic injection molding 200 are bonded by a curing adhesive. The curing adhesive is applied thinly on the outer case 100 or the bonding plastic injection molding 200, and then bonded while overlapping each other.

도 4는 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품이 노트북 컴퓨터에 적용된 예를 도시한 도면이다.4 is a diagram illustrating an example in which a metal exterior of a portable device is applied to a notebook computer according to an embodiment of the present invention.

금속으로 제조된 외부 케이스(100)의 내면에 결합용 플라스틱 사출물(200)이 접착되어 있다. 외부 케이스(100)와 결합용 플라스틱 사출물(200)은 서로 대응하는 크기 및 형상을 가져, 결합용 플라스틱 사출물(200)은 별도의 장치나 공정 없이도 쉽게 외부 케이스(100)의 내측에 정 위치에 위치시킬 수 있다. 결합용 플라스틱 사출물(200)에 노트북 컴퓨터의 LCD 패널이나 백라이트를 설치하기 위한 보스(210)나, LCD 패널을 고정하는 프레임과 외장품을 서로 고정하기 위한 리브(220)나 후 크(230) 등이 형성된다. 보스(210), 리브(220), 후크(230)은 결합용 플라스틱 사출물(200)을 사출 형성할 때, 금형의 형상에 의해 일체로 형성된다. 플라스틱 사출물(200)은 앞서 말한 것과 같이 별도의 노력을 기울이지 않아도 외부 케이스(100)의 내면에 안착되므로, 플라스틱 사출물(200)에 형성된 보스(210), 리브(220), 후크(230)의 위치도 별도의 노력없이 정 위치에 위치시킬 수 있다. 또한 결합용 플라스틱 사출물(200)은 보스(210), 리브(220), 후크(230)가 형성되는 곳을 포함하여, 외부 케이스(100) 내에 형상의 대응에 의해 용이하게 안착될 수 있도록 외부 케이스(100)의 테두리부분에 접합되도록 형성되며, 내측은 방열을 위해 중공될 수 있도록 형성된다. Bonding plastic injection molding 200 is adhered to the inner surface of the outer case 100 made of metal. The outer case 100 and the bonding plastic injection molding 200 have sizes and shapes corresponding to each other, and the bonding plastic injection molding 200 is easily positioned at the inside of the outer case 100 without a separate device or process. You can. Boss 210 for installing an LCD panel or backlight of a notebook computer, a frame 220 for fixing the LCD panel and a rib 220 or a hook 230 for fixing an external article to the plastic injection molding 200 for bonding. Is formed. The boss 210, the rib 220, and the hook 230 are integrally formed by the shape of the mold when injection molding the injection-molded plastic injection molding 200. Since the plastic injection molding 200 is seated on the inner surface of the outer case 100 without any extra effort as described above, the position of the boss 210, the rib 220, and the hook 230 formed in the plastic injection molding 200. Can also be placed in place without extra effort. In addition, the coupling plastic injection molding 200 includes a boss 210, a rib 220, and a hook 230 where the outer case is formed so that the outer case 100 can be easily seated by the correspondence of the shape. It is formed to be joined to the edge portion of the 100, the inner side is formed to be hollow for heat dissipation.

외부 케이스(100)는 알루미늄, 스테인리스 스틸(SUS), 티타늄, 마그네슘 등의 금속 판재가 정밀 프레스 가공 성형되고, PVD 스퍼터링, 산화피막 형성, 비화성처리 피막 형성 등의 고경도 표면처리를 한 다음 필요한 경우 도장 작업이 이루어진다. 결합용 플라스틱 사출물(200)은 사출성형된 다음, UV, 우레탄코팅이 이루어진다. 결합용 플라스틱 사출물(200) 역시 선택적으로 도장 작업이 이루어질 수 있다. The outer case 100 is formed by precision press forming a metal sheet such as aluminum, stainless steel (SUS), titanium, or magnesium, and subjected to high hardness surface treatment such as PVD sputtering, oxide film formation, and non-chemical treatment film formation. If painting is done. Bonding plastic injection molding 200 is injection molded, then UV, urethane coating is made. Coupling plastic injection molding 200 may also be selectively painted.

도 5는 노트북 컴퓨터에 적용된 휴대용 기기의 금속 외장품의 외부 케이스와 결합용 플라스틱 사출물을 접착하는 모습을 도시한 도면이다. 외부 케이스(100)와 결합용 플라스틱 사출물(200)의 접착을 위한 금형은 하부 금형(310)과 상부 금형(320)을 포함한다. 하부 금형(310)은 결합용 플라스틱 사출물(200)의 보스(210), 리브(220), 후크(230)를 수용할 수 있으며, 전체적인 형상이 결합용 플라스틱 사출 물(200)을 수용할 수 있도록 되어 있다. 결합용 플라스틱 사출물(200)은 보스(210), 리브(220), 후크(230) 등이 형성된 면이 하부 금형(310) 내에 수용되며 하부 금형(310)의 위에 얹혀진다. 하부 금형(310) 위에 얹혀진 결합용 플라스틱 사출물(200) 위에 경화용 접착제를 정밀하게 도포한 외부 케이스(100)를 얹고, 상부 금형(320)으로 가압하여 접착한다. FIG. 5 is a view illustrating bonding a plastic injection molded product to an outer case of a metal exterior of a portable device applied to a notebook computer. The mold for bonding the outer case 100 and the coupling plastic injection molding 200 includes a lower mold 310 and an upper mold 320. The lower mold 310 may accommodate the bosses 210, the ribs 220, and the hooks 230 of the coupling plastic injection molding 200, and the overall shape may accommodate the coupling plastic injection molding 200. It is. The coupling plastic injection molding 200 has a surface on which the boss 210, the rib 220, the hook 230, and the like are formed is accommodated in the lower mold 310 and mounted on the lower mold 310. The outer case 100, which is precisely coated with a curing adhesive, is placed on the bonding plastic injection molding 200 mounted on the lower mold 310, and pressed by the upper mold 320 to be bonded.

도 6은 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품을 제조하는 방법을 도시한 플로우 차트이다. 외부 케이스(100)를 제조하는 과정은 판금 공정(S11), 표면 후처리 공정(S12) 및 도장 공정(S13)을 포함한다. 외부 케이스(100)는 고강도 알루미늄, 두랄루민, 마그네슘, 티타늄과 같은 금속 판재를 이용하여 판금 가공한다. 특히 노트북 용 금속 외장품의 경우, 외부 케이스(100)는 0.4 ~ 0.9 mm의 전신재의 마그네슘 합금 판재를 150 ~ 300℃에서 열간 프레스 가공한다(S11). 판금 공정(S11)을 통해 성형이 이루어지면, 금속재의 표면 후처리 공정(S12)이 행해진다. 표면 후처리 공정(S12)는 비화성처리(Non-Chromate Anodizing), 산화피막 처리(Anodizing), PVD 스퍼터링, 등 외부 케이스(100)를 이루는 금속의 종류에 따라 혹은 필요에 따라 원하는 방법으로 표면 후처리 방법을 선택할 수 있다. 또한 산화피막 처리 후에 Ni 도금 등이 추가로 이루어질 수도 있다. 표면 후처리 공정(S12)이 끝나면, 필요에 따라 도장 공정(S13)을 통해 외면에 색을 입힘으로써 외관을 향상시킬 수 있다. 상기한 일련의 공정을 통해 외부 케이스(100)가 제작되는 것과 별개로, 외부 케이스(100)의 내면에 부착되어 외부 케이스(100)의 고정을 돕는 결합용 리브나 결합용 돌기, 후크 등이 형성되고, 외부 케이스(100) 내면에 다 른 부품이 안착되는 것을 안내하는 보스가 형성된 결합용 플라스틱 사출물(200)이 제조된다. 결합용 플라스틱 사출물(200)은 종래의 일반적인 플라스틱 사출 공정(S2)을 통해 사출 형성된다. 결합용 플라스틱 사출물(200)은 도 5에 도시된 것과 같은 하부 금형(310)에 안착되고, 내면에 경화형 접착제가 도포된 외부 케이스(100)가 얹혀지며, 상부 금형(320)에 의해 가압되어 결합용 플라스틱 사출물(200)과 외부 케이스(100)가 서로 접착된다(S3). 외부 케이스(100)와 결합용 플라스틱 사출물(200)은 단단히 접착되어 신뢰성을 제공한다. 이러한 공정을 통해 제조되는 노트북 용 금속 외장품은 외부 케이스(100)를 충격에 강한 금속으로 제작하는 동시에, 조립을 위해 복잡한 형상을 요구하는 결합 보스, 결합 리브, 후크 등은 별도의 결합용 플라스틱 사출물(200)에 성형하여 부착함으로써, 각 재료의 이점을 동시에 살릴 수 있다. 6 is a flow chart illustrating a method of manufacturing a metal exterior of a portable device according to an embodiment of the present invention. The process of manufacturing the outer case 100 includes a sheet metal process (S11), a surface post-treatment process (S12) and a painting process (S13). The outer case 100 is a sheet metal processing using a metal plate such as high strength aluminum, duralumin, magnesium, titanium. In particular, in the case of a metal exterior for notebooks, the outer case 100 is hot pressed to process the magnesium alloy sheet of the whole body material of 0.4 ~ 0.9 mm at 150 ~ 300 ℃ (S11). When shaping | molding is performed through sheet metal process S11, the surface post-processing process S12 of a metal material is performed. The surface post-treatment process (S12) is performed after the surface in a desired manner depending on the type of metal constituting the outer case 100, such as Non-Chromate Anodizing, Anodizing, PVD sputtering, etc. The treatment method can be selected. In addition, Ni plating may be further performed after the oxide film treatment. After the surface post-treatment step (S12) is finished, the appearance can be improved by applying color to the outer surface through the coating step (S13) as necessary. Apart from being manufactured by the outer case 100 through the series of processes described above, a coupling rib, a coupling protrusion, a hook, etc., which are attached to an inner surface of the outer case 100 to help fix the outer case 100, are formed. Then, a coupling plastic injection molding (200) having a boss for guiding the mounting of other components on the inner surface of the outer case (100) is manufactured. Bonding plastic injection molding 200 is injection molded through a conventional plastic injection process (S2). Bonding plastic injection molding 200 is seated on the lower mold 310 as shown in Figure 5, the outer case 100 is coated with a curable adhesive on the inner surface, it is pressed by the upper mold 320 and coupled Plastic injection molded product 200 and the outer case 100 are bonded to each other (S3). The outer casing 100 and the bonding plastic injection molding 200 are firmly bonded to provide reliability. The metal exterior parts for notebooks manufactured through such a process are made of a metal that is resistant to impact, and at the same time, coupling bosses, coupling ribs, hooks, etc., which require complicated shapes for assembly, have separate plastic injection molding materials ( By forming and adhering to 200, the advantages of each material can be utilized simultaneously.

도 1 내지 도 3은 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품이 휴대용 전화기에 적용된 모습을 도시한 도면,1 to 3 is a view showing a metal exterior of the portable device according to an embodiment of the present invention applied to the portable telephone,

도 4는 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품이 노트북 컴퓨터에 적용된 예를 도시한 도면,4 is a view showing an example in which a metal exterior of a portable device is applied to a notebook computer according to an embodiment of the present invention;

도 5는 노트북 컴퓨터에 적용된 휴대용 기기의 금속 외장품의 외부 케이스와 결합용 플라스틱 사출물을 접착하는 모습을 도시한 도면,5 is a view showing a state of bonding the plastic injection molding for bonding with the outer case of the metal exterior of the portable device applied to the notebook computer,

도 6은 본 발명의 일 실시예에 따른 휴대용 기기의 금속 외장품을 제조하는 방법을 도시한 플로우 차트.6 is a flow chart illustrating a method of manufacturing a metal enclosure of a portable device according to an embodiment of the present invention.

Claims (9)

금속재료를 가공하여 외부 케이스 및 결합용 플라스틱 사출물을 각각 제조하는 단계; 및Processing a metal material to manufacture an outer case and a plastic injection molding for bonding; And 외부 케이스의 내면에 결합용 플라스틱 사출물을 접합하는 단계;를 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법.Bonding the plastic injection molding product to the inner surface of the outer case; and manufacturing a metal exterior part of the portable device. 제1항에 있어서,The method of claim 1, 금속 외장 제조 단계는, 판금 공정, 표면 후처리 공정 및 도장 공정을 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법.The metal sheath manufacturing step includes a sheet metal process, a surface post-treatment process and a painting process. 제2항에 있어서,The method of claim 2, 판금 공정은, 금속재가 150℃ ~ 300℃에서 열간 프레스 성형되는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법.The sheet metal process is a method for manufacturing a metal exterior article of a portable device, characterized in that the metal material is hot press formed at 150 ℃ to 300 ℃. 제2항에 있어서,The method of claim 2, 표면 후처리 공정은 비화성처리(Non-chromate Anodizing)을 형성하는 공정을 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법.The surface post-treatment process includes a step of forming a non-chromate anodizing. 제2항에 있어서,The method of claim 2, 표면 후처리 공정은 Ni 도금 과정을 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법.And the surface post-treatment process comprises a Ni plating process. 제1항에 있어서,The method of claim 1, 접합 단계의 전 단계에 외부 케이스를 도장하는 단계;를 더 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품을 제조하는 방법.Painting the outer case prior to the bonding step; the method of manufacturing a metal exterior of a portable device further comprising. 금속으로 제조되며, 휴대용 기기의 내장 전장품을 보호하는 외부 케이스;An outer case made of metal and protecting the internal electronics of the portable device; 외부 케이스 내면에 부착되며, 외부 케이스의 결합을 위한 결합용 리브 또는 결합용 돌기를 구비하는 결합용 플라스틱 사출물; 및A coupling plastic injection molding attached to an inner surface of the outer case and having a coupling rib or coupling protrusion for coupling the outer case; And 외부 케이스와 결합용 플라스틱 사출물을 접합하는 접착제;를 포함하는 것을 특징으로 하는 휴대용 기기의 금속 외장품.Adhesive for bonding the outer case and the bonding plastic injection molding; Metal exterior article of a portable device comprising a. 제7항에 있어서,The method of claim 7, wherein 외부 케이스는, 스테인리스 스틸, 알루미늄, 두랄루민, 티타늄 및 마그네슘 중 어느 하나로 제조되는 것을 특징으로 하는 휴대용 기기의 금속 외장품.The outer case is made of any one of stainless steel, aluminum, duralumin, titanium and magnesium, the metal casing of the portable device. 제1항에 있어서,The method of claim 1, 결합용 플라스틱 사출물은 외부 케이스의 내측에 형상결합되도록 외부 케이스의 형상 및 크기에 대응하는 형상 및 크기를 가지는 것을 특징으로 하는 휴대용 기기의 금속 외장품.The plastic injection molding for joining has a shape and size corresponding to the shape and size of the outer case so as to be shape-coupled to the inside of the outer case.
KR1020090089626A 2009-09-22 2009-09-22 A metal exterior of a mobile apparatus and a method of preparing the same KR101149177B1 (en)