KR19990014598A - 균열 추종성 건물 단열용 수성도료 조성물 - Google Patents

균열 추종성 건물 단열용 수성도료 조성물 Download PDF

Info

Publication number
KR19990014598A
KR19990014598A KR1019980050837A KR19980050837A KR19990014598A KR 19990014598 A KR19990014598 A KR 19990014598A KR 1019980050837 A KR1019980050837 A KR 1019980050837A KR 19980050837 A KR19980050837 A KR 19980050837A KR 19990014598 A KR19990014598 A KR 19990014598A
Authority
KR
South Korea
Prior art keywords
condensation
building
facilities
cracks
present
Prior art date
Application number
KR1019980050837A
Other languages
English (en)
Inventor
김지태
Original Assignee
김지태
홍주환
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김지태, 홍주환 filed Critical 김지태
Priority to KR1019980050837A priority Critical patent/KR19990014598A/ko
Publication of KR19990014598A publication Critical patent/KR19990014598A/ko

Abstract

본 발명은 단열(斷熱) 성능과 탄성(彈性)을 가진 수성계 도료로서 건축물에 직접 미장 또는 도포하는 기존의 단열재가 건물자체의 균열에 적응하지 못하여 균열이 발생하고 균열부에 열손실이 발생함과 동시에 결로 발생의 원인을 제공하여 지하 창고등에 보관중인 물품이나 시설물이 습기에 피해를 보고 있는 문제점을 해결하기 위하여, 도막특성이 탄성 및 신장성이 높은 특수 아크릴 에멀젼수지를 사용하고 안료는 열전도율이 낮은 프라스틱계 PVC 파우더와 시리카, 산화아연 등을 적절하게 구성하여 도료의 도막으로서는 획기적인 0.10 Kcal/mh℃ 의 열전도율로 단열효과가 우수하다.
본 발명품으로 건축물 벽면 또는 천정에 3mm두께로 도포하여 30%정도 단열 시공을 하면 피도면과 대기의 온도 차이가 좁혀져 결로 발생을 억제할수 있으며 결로 발생으로 인한 습기 피해를 방지하고, 단열 효과에 의하여 에너지를 절감할 수 있다. 특히 수성계 이므로 작업시 화재 위험이나 유해가스의 위험이 없고 시공이 용이하다.
본 발명품은 단열 효과가 우수하므로 결로 발생으로 습기의 피해가 많은곳, 즉 지하통신시설, 탄약등 주요물품 보관시설, 냉동시설, 건물지하실등에 시공시 우수한 효과를 얻을 수 있다.

Description

균열 추종성 건물단열용 수성도료 조성물
건축물의 내 외부 단열을 목적으로 현장단열 시공을 하였을 경우 단열에 실패하는 것은 단열자재 차체의 결함도 있겠지만 건물의 진동이나 침하건조 수축에 의한 균열에 단열재료가 적응하지 못하고 건물 균열과 동시에 같이 균열이 가고 있으므로 균열 추종성 도막형 조성물을 개발한 것이다.
건축물 균열에 적응하는 단열용 수성도료 조성물 개발 본 발명은 각종 소재 특히 콘크리트나 시멘트 몰탈등으로 시공된 건축물이나 구조물의 표면에 도료를 도장하여 단열(斷熱) 효과 및 결로(結露)방지 효과를 얻을 수 있는 도료의 조성물에 관한 것으로 균열추종성(龜裂追從性)을 가진 수성계 단열도료 조성물이다.
포리우레탄폼 우레아폼 스티로폼 단열몰탈 퍼라이트몰탈등 기존단열재 대부분은 재료특성 및 시공특성상 건축물의 시공후 시일이 경과 함에따라 콘크리트의 철근 부식으로 인한 팽창으로 발생하는 균열이나, 조적벽면등의 균열에 추종성이 없어 균열 부위로 열손실이 발생하여 단열에 문제가 발생하고 단열 효과가 저하됨에 따라 외부와 내부의 온도 차이가 격심해 지기때문에 결로가 발생한다.
본 발명은 전술한 문제점을 해결하고 건물표면에 균열이 발생하더라도 도막자체의 탄성(彈性)과 신장성(伸長性)으로 도막에는 손상이 없도록 하였고, 단열재로서는 필수적인 열전도율을 낮추어 피도체 표면에 3mm두께로 도포하여 대기의 온도와 벽체표면의 온도차를 30%(1mm당10%) 이내로 유지시켜 결로점에 이르지 않게 단열효과를 줌으로서 결로발생을 억제한다.
본 발명은 유리전이온도(Tg) 약 -50℃의 탄성 및 신장성(伸長性)이 우수한 아크릴 에멀젼수지를 사용하여 균열추종성을 부여하고 난연성이 있고 열전도율이 낮은 프라스틱류의 PVC 파우더, 산화티타늄, 산화아연탄산칼슘, 시리카 등의 안료를 적정하게 배합하여 열전도율을 낮추었다.
아래에 상세한 조성물 및 실시예를 기재하는 바 실시예중 부는 중량부를 표시한다.
실시예1
아크릴 에멀젼수지 조성물
이온교환수 44.59부
유화제 3부
탄산소다 0.4부
2-에칠헥실아크레이트 42부
메칠메타크릴 레이트 3부
스티렌 4부
아크릴산 3부
과유산칼륨 0.01부
이온교환수, 유화제, 탄산소다를 혼합하여 75℃로 승온후 4종류의 혼합 모노머량의 10%를 투입하여 30분 유지후 나머지 모노머를 3시간동안 분할 투입, 80℃에서 2시간, 85℃에서 30분 반응시켜 제조한다.
실시예2
도료의 조성물
실시예1에서 제조한수지 49부
분산제(타몰731) 1부
산화티타늄 2부
산화아연 2부
탄산칼슘 14부
시리카 7부
P.V.C.파우더 20부
증점제(나트로졸2%) 5부
순서대로 투입하여 1000rpm 속도의 믹서기로 30분간 제조한다.
도료의 점도는 페이스트상이며 고형분 72%이다.
도막의 물성시험 결과는 아래와 같다.
도막물성 시험표
본 발명은 에어레스 스프레이, 붓, 로라, 미장칼로 건조도막 두께 3mm로 시공할 경우 기존의 단열재 보다 경제적이며 기존의 현장시공형 단열재가 해결하지 못하는 건물표면 자체의 균열에 대하여 균열 추종성 도막을 형성하므로 단열의 지속 효과가 에너지 절약 및 건물 내부의 결로방지에 크게 기여할 것이다. 또한 수성계 이므로 작업시 유독개스나 화재 위험성이 없고 공해를 줄일수 있는 것도 장점이다.
본발명은 단열에 실패하여 습기에 의해 손실을 보고있는 통신시설 곡물의약 탄약 등의 보관 창고에 시공시 좋은 결과가 기대된다.

Claims (1)

  1. 아크릴에멀젼(Tg-50℃∼ -60℃) 수지와 PVC 파우더를 사용한 탄성 과 신장성이 있는 단열 및 결로방지를 목적으로 하는 수성도료 조성물.
KR1019980050837A 1998-11-26 1998-11-26 균열 추종성 건물 단열용 수성도료 조성물 KR19990014598A (ko)