JPWO2022237727A5 - - Google Patents
Info
- Publication number
- JPWO2022237727A5 JPWO2022237727A5 JP2023569898A JP2023569898A JPWO2022237727A5 JP WO2022237727 A5 JPWO2022237727 A5 JP WO2022237727A5 JP 2023569898 A JP2023569898 A JP 2023569898A JP 2023569898 A JP2023569898 A JP 2023569898A JP WO2022237727 A5 JPWO2022237727 A5 JP WO2022237727A5
- Authority
- JP
- Japan
- Prior art keywords
- refractory material
- corundum
- fine powder
- aggregate
- hot
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CN202110507564.4 | 2021-05-10 | ||
| CN202110507564.4A CN115321966A (zh) | 2021-05-10 | 2021-05-10 | 耐蚀损性耐火材料、制备方法及其应用 |
| PCT/CN2022/091728 WO2022237727A1 (zh) | 2021-05-10 | 2022-05-09 | 耐蚀损性耐火材料、制备方法及其应用 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2024522455A JP2024522455A (ja) | 2024-06-21 |
| JPWO2022237727A5 true JPWO2022237727A5 (enrdf_load_stackoverflow) | 2025-09-26 |
Family
ID=83912610
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2023569898A Pending JP2024522455A (ja) | 2021-05-10 | 2022-05-09 | 耐溶損性耐火材、製造方法及びその使用 |
Country Status (6)
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN116239370A (zh) * | 2023-04-03 | 2023-06-09 | 宜兴金君耐火炉料有限公司 | 用于低氧铜杆生产中延长流槽寿命的99浇注料及制备方法 |
| CN116655360B (zh) * | 2023-05-23 | 2025-02-18 | 北京科技大学 | 一种rh精炼炉用复合耐火材料及其制备方法 |
| CN116835977B (zh) * | 2023-05-24 | 2024-09-17 | 无锡市南方耐材有限公司 | 钢包上水口砖及其制备方法 |
| CN116751067A (zh) * | 2023-06-21 | 2023-09-15 | 武汉科技大学 | 一种转炉用水系大面料及其制备方法 |
| CN117447192B (zh) * | 2023-11-02 | 2024-05-03 | 衡水兆星复合材料有限公司 | 一种挡渣塞及其制备方法 |
| CN117720358A (zh) * | 2023-11-30 | 2024-03-19 | 广西北港新材料有限公司 | 红土镍矿回转窑用耐火砖及其制备方法和应用 |
Family Cites Families (13)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0777980B2 (ja) * | 1989-11-27 | 1995-08-23 | 東芝セラミックス株式会社 | 鋳造用耐火物の製造方法 |
| JPH08208317A (ja) * | 1995-01-31 | 1996-08-13 | Kyocera Corp | アルミナ質焼結体およびその製造方法 |
| EP1178023A1 (en) * | 2000-08-04 | 2002-02-06 | Alcoa Chemie GmbH | High density refractory material containing calcium hexaluminate |
| CN102531555B (zh) * | 2012-03-15 | 2013-07-03 | 福州大学 | 利用铝厂污泥和牡蛎壳原位合成六铝酸钙/刚玉复相材料 |
| CN102718514B (zh) * | 2012-06-28 | 2015-05-20 | 江苏晶鑫高温材料有限公司 | 一种微孔高强刚玉-六铝酸钙复合耐火原料及其制备方法 |
| CN105585314B (zh) | 2015-12-22 | 2018-07-06 | 辽宁科技学院 | 一种致密六铝酸钙耐火熟料及其制备方法 |
| CN106431430A (zh) * | 2016-08-31 | 2017-02-22 | 浙江正豪耐火材料有限公司 | 一种高强防渗耐腐蚀浇注料 |
| CN107500747A (zh) | 2017-09-15 | 2017-12-22 | 武汉威林科技股份有限公司 | 一种致密的六铝酸钙浇注料及其制备方法 |
| CN107602136A (zh) * | 2017-09-15 | 2018-01-19 | 武汉威林科技股份有限公司 | 一种用于中间包的耐火材料衬体及其制备方法 |
| CN108178639A (zh) * | 2017-12-20 | 2018-06-19 | 北京科技大学 | 一种高纯Ca2Mg2Al28O46材料及其制备方法 |
| CN108147826A (zh) * | 2017-12-20 | 2018-06-12 | 北京科技大学 | 一种高纯cm2a8材料及其制备方法 |
| CN110171980A (zh) | 2019-04-10 | 2019-08-27 | 辽宁科技学院 | 一种致密六铝酸钙耐火熟料的制备方法 |
| CN112125651B (zh) * | 2020-09-03 | 2023-02-17 | 武汉理工大学 | 一种致密六铝酸钙-刚玉复相陶瓷的制备方法 |
-
2021
- 2021-05-10 CN CN202110507564.4A patent/CN115321966A/zh active Pending
-
2022
- 2022-05-09 JP JP2023569898A patent/JP2024522455A/ja active Pending
- 2022-05-09 EP EP22806690.8A patent/EP4339175A4/en active Pending
- 2022-05-09 KR KR1020237042548A patent/KR20240051885A/ko active Pending
- 2022-05-09 WO PCT/CN2022/091728 patent/WO2022237727A1/zh not_active Ceased
- 2022-05-09 US US18/290,388 patent/US20240246862A1/en active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2024522455A (ja) | 耐溶損性耐火材、製造方法及びその使用 | |
| Ewais | Carbon based refractories | |
| US20240254051A1 (en) | High-purity compact calcium hexa-aluminate-based refractory material and preparation method therefor | |
| Lee et al. | Refractories: Controlled microstructure composites for extreme environments | |
| US20070203013A1 (en) | Ceramic Batch And Associated Product For Fireproof Applications | |
| Ghasemi-Kahrizsangi et al. | A Review on Recent Advances on Magnesia-Doloma Refractories by Nano-Technology. | |
| US20240261851A1 (en) | Refractory material with function of cleaning molten steel, preparation method therefor and use thereof | |
| JP4310277B2 (ja) | 重セラミック成形品、その製造方法および使用 | |
| US20240246861A1 (en) | Ca6-based refractory material with medium volume density, preparation method therefor, and use thereof | |
| JP2002241182A (ja) | 不定形耐火組成物 | |
| Tomšů et al. | Refractory monolithics versus shaped refractory products | |
| JPWO2022237727A5 (enrdf_load_stackoverflow) | ||
| CN1298465C (zh) | 一种大型钢包包底耐火材料 | |
| Aksel et al. | Investigation of parameters affecting grain growth of sintered magnesite refractories | |
| JP2001270781A (ja) | 炭酸マグネシウムをマグネシア源とするアルミナ−マグネシア質キャスタブル耐火物 | |
| Biswas et al. | Refractories for Iron and Steel Plant | |
| CN115321974A (zh) | 六铝酸钙系耐火材料、纳米隔热板、复合耐火材料衬体结构体、制法及其应用 | |
| JP3212856B2 (ja) | 不定形流し込み耐火物及びその成形体 | |
| Kalpaklı | Comparative study for physical properties and corrosion mechanism of synthetic and in situ MgAl2O4 spinel formation zero cement refractory castables | |
| Banerjee | Thermal and Corrosion Properties of Monolithic Refractories for Iron and Steel Applications | |
| Feifang et al. | Innovative Lining of Unburnt Al2O3-MgO Brick for 300t Steel Ladle in Baosteel | |
| Feifang et al. | Insulating Permanent Lining of Calcium Hexaluminate Based Castable for 300t Ladle in Baosteel | |
| KR20250069871A (ko) | 시멘트 조성물 및 시멘트 요소 생산 방법 | |
| JP2004307293A (ja) | 不定形耐火組成物 | |
| Nourbakhsh | Development of MgO refractories by using synthesized spinel for application in steel industries |