JPS6475620A - Method for removing metal in molten metal vessel - Google Patents
Method for removing metal in molten metal vesselInfo
- Publication number
- JPS6475620A JPS6475620A JP23207687A JP23207687A JPS6475620A JP S6475620 A JPS6475620 A JP S6475620A JP 23207687 A JP23207687 A JP 23207687A JP 23207687 A JP23207687 A JP 23207687A JP S6475620 A JPS6475620 A JP S6475620A
- Authority
- JP
- Japan
- Prior art keywords
- metal
- flame
- high pressure
- water
- pressure water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To easily and surely remove stuck metal in a molten metal vessel without any damage to the lining by combining energies of high pressure water and high temp. flame. CONSTITUTION:To the metal 2 sticking to an opening part or internal side wall, etc., in the above vessel of converter, etc., an injection nozzle forming the high temp. flame burner 10 of LPG flame, etc., at center part and the high pressure water nozzle 13 around the burner 10 at the equal interval so as to concentrate the high pressure water to the tip of the flame, is used. At the same time of detaching the metal with the high temp. flame from the burner 10 by colliding the high pressure water, the firmly stuck metal 2 layer is effectively detached and removed by cooling effect with the water and by inducing a kind of steam explosion caused by quick volume expansion from the water to the steam. Further, by regulating the water pressure of the high pressure water to lower level, only the metal 2 layer is selectively removed and the damage of the refractory 15 can be avoided.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23207687A JPS6475620A (en) | 1987-09-18 | 1987-09-18 | Method for removing metal in molten metal vessel |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23207687A JPS6475620A (en) | 1987-09-18 | 1987-09-18 | Method for removing metal in molten metal vessel |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS6475620A true JPS6475620A (en) | 1989-03-22 |
Family
ID=16933615
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP23207687A Pending JPS6475620A (en) | 1987-09-18 | 1987-09-18 | Method for removing metal in molten metal vessel |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6475620A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2012229480A (en) * | 2011-04-27 | 2012-11-22 | Nisshin Steel Co Ltd | Method for melting and removing slag and base metal deposited on refractory vessel |
JP2014169834A (en) * | 2013-03-04 | 2014-09-18 | Nippon Steel & Sumitomo Metal | Removal method of metal deposit and removal device of metal deposit |
-
1987
- 1987-09-18 JP JP23207687A patent/JPS6475620A/en active Pending
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2012229480A (en) * | 2011-04-27 | 2012-11-22 | Nisshin Steel Co Ltd | Method for melting and removing slag and base metal deposited on refractory vessel |
JP2014169834A (en) * | 2013-03-04 | 2014-09-18 | Nippon Steel & Sumitomo Metal | Removal method of metal deposit and removal device of metal deposit |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES454771A1 (en) | Lance for desulphurizing cast iron or steel | |
DE3672275D1 (en) | INJECTING DEVICE FOR METALLURGICAL VESSELS. | |
CA2003133A1 (en) | Air cooled gas injection lance | |
JPS6475620A (en) | Method for removing metal in molten metal vessel | |
DE59903163D1 (en) | METHOD FOR GRANULATING LIQUID SLAG MOLDS AND DEVICE FOR CARRYING OUT THIS METHOD | |
SE8503515L (en) | METAL MELTOR RINSE TREATMENT PROCEDURE | |
JPS5785940A (en) | Tuyere for refining molten metal | |
JPS54125106A (en) | Reducing blowing out method for blast furnace | |
JPS5732310A (en) | Method for repairing wall of blast furnace | |
JPS64217A (en) | Vacuum refining method for molten steel | |
GB500938A (en) | Method of cleaning out slag or cinder pockets of open hearth combustion furnaces | |
JPS53115692A (en) | Method for treating blast furnace slags | |
JPS5611159A (en) | Construction of dummy bar head in continuous horizontal casting machine | |
JPS5791842A (en) | Horizontal and continuous casting method of deformed cast iron piece | |
JPS6475617A (en) | Melting and refining method for scrap | |
JPS51121407A (en) | Method of cooling tuyeres in bottom-blowing refining furnace | |
GB1354016A (en) | Method of and vacuum treatment apparatus for refining molten metal or alloy | |
Higuchi et al. | Blow-In and Empty Blow-Out Operation of the NKK Blast Furnaces | |
JPS5693814A (en) | Method of supplying cooling medium to oxygen blowing part of bottom blown refining furnace | |
JPS54141309A (en) | Reducing blow out method for blast furnace | |
JPS57155312A (en) | Repairing method of bottom-blow converter | |
JPS6451489A (en) | Method of repairing wall of coke oven | |
Omel'yanenko et al. | Further Development of Equipment for the After-Furnace Treatment of Iron | |
JPS5390105A (en) | Removing apparatus for scum | |
Pan et al. | A Mathematical Model Study on Bottom Gas Flow of Combined Blown Converters |