JPS6462410A - Method for adjusting components in molten pig iron and molten slag - Google Patents

Method for adjusting components in molten pig iron and molten slag

Info

Publication number
JPS6462410A
JPS6462410A JP21586087A JP21586087A JPS6462410A JP S6462410 A JPS6462410 A JP S6462410A JP 21586087 A JP21586087 A JP 21586087A JP 21586087 A JP21586087 A JP 21586087A JP S6462410 A JPS6462410 A JP S6462410A
Authority
JP
Japan
Prior art keywords
molten
pig iron
flow
molten pig
molten slag
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP21586087A
Other languages
Japanese (ja)
Inventor
Yoshiyuki Matsui
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kobe Steel Ltd
Original Assignee
Kobe Steel Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kobe Steel Ltd filed Critical Kobe Steel Ltd
Priority to JP21586087A priority Critical patent/JPS6462410A/en
Publication of JPS6462410A publication Critical patent/JPS6462410A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To effectively execute adjustment of components in molten pig iron and molten slag and to improve the yield of component adjusting material by pouring the fine particle component adjusting material at the dropping position in a molten pig iron trough or a molten slag trough to the molten pig iron flow or the molten slag flow at the specific ratio. CONSTITUTION:To the molten pig iron flow 3 or the molten slag flow or mixing flow of the molten pig iron and the molten slag flow discharged from molten pig iron tapping hole 2 or molten slag tapping hole in the blast furnace 1, the fine grain component adjusting material is injected at the dropping position in the molten pig iron trough 4 or the molten slag trough. This component adjusting material having <=5mm grain size is used at max. 50kg/T.P. ratio. The above component adjusting material is stirred by dropping energy of the pouring and the molten pig iron flow, etc., and free degree of the additional quantity can be improved. Further, the poured component adjusting material gives the effect at high yield without any spattering. By this method, the molten pig iron flow 9 effectively executing the desulfurization, etc., is recovered in a runner 12 through a skimmer 11 or the molten slag flow 8 improving basicity, etc., is recovered from the slag-off hole 10.
JP21586087A 1987-08-29 1987-08-29 Method for adjusting components in molten pig iron and molten slag Pending JPS6462410A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP21586087A JPS6462410A (en) 1987-08-29 1987-08-29 Method for adjusting components in molten pig iron and molten slag

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP21586087A JPS6462410A (en) 1987-08-29 1987-08-29 Method for adjusting components in molten pig iron and molten slag

Publications (1)

Publication Number Publication Date
JPS6462410A true JPS6462410A (en) 1989-03-08

Family

ID=16679472

Family Applications (1)

Application Number Title Priority Date Filing Date
JP21586087A Pending JPS6462410A (en) 1987-08-29 1987-08-29 Method for adjusting components in molten pig iron and molten slag

Country Status (1)

Country Link
JP (1) JPS6462410A (en)

Similar Documents

Publication Publication Date Title
BG60214B2 (en) Method for steel-making
JPS6462410A (en) Method for adjusting components in molten pig iron and molten slag
MXPA99011501A (en) Process for making expanded slag.
JPS54151503A (en) Quality reforming converter slag
JPS563610A (en) Molten iron pretreating method
JPS6465223A (en) Charging method for desiliconization
SU1401053A1 (en) Method of producing metallurgical flux
JPS54139819A (en) Stabilization treating method for impurities in hot iron to low level
Kolsi Hot Metal Desulphurization at Koverhar Steel Works
JPS62247015A (en) Desiliconizing agent for molten iron
Hiraga et al. Reduction behavior of manganese ore in injection into hot metal
Gvamberiya et al. After-Furnace Desulphurization of Tube Steel by Slag-Forming Mixtures
Palchetti et al. Hot Metal Techniques for Mass Production of Clean Steel
JPS6455315A (en) Method for pretreating molten iron by converter slag
SU1497222A1 (en) Method of separating liquid products of blast-furnace smelting
JPS648214A (en) Steel making method in converter
JPS54127819A (en) Desulfurinzing molten iron
JPS60238407A (en) Casting bed desiliconizing method of molten iron
JPS54107496A (en) Property improvement of molten pig iron soda ash desulfurized slag
JPS6439313A (en) Refining method using ferro-silicon alloy coated by carbonic material
Jones Lime Based Slag Forming Materials for the Treatment of Iron and Steel
JPS55122652A (en) Cast iron inoculation method
JPH0517809A (en) Hearth desulfurization method for blast furnace
Gurov et al. Determining the Volume of Resources of Graphite and Graphite-Bearing Discards From Iron and Steel Works and the Effectiveness of Their Utilization
Chuiko et al. Refining Steel on a High Output Level by Means of Slag Mixtures in the Ladle at Tapping