JPS6412298B2 - - Google Patents
Info
- Publication number
- JPS6412298B2 JPS6412298B2 JP56161674A JP16167481A JPS6412298B2 JP S6412298 B2 JPS6412298 B2 JP S6412298B2 JP 56161674 A JP56161674 A JP 56161674A JP 16167481 A JP16167481 A JP 16167481A JP S6412298 B2 JPS6412298 B2 JP S6412298B2
- Authority
- JP
- Japan
- Prior art keywords
- water
- polymer electrolyte
- film
- molded product
- soluble
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02A—TECHNOLOGIES FOR ADAPTATION TO CLIMATE CHANGE
- Y02A40/00—Adaptation technologies in agriculture, forestry, livestock or agroalimentary production
- Y02A40/10—Adaptation technologies in agriculture, forestry, livestock or agroalimentary production in agriculture
- Y02A40/25—Greenhouse technology, e.g. cooling systems therefor
Landscapes
- Surface Treatment Of Optical Elements (AREA)
- Coating Of Shaped Articles Made Of Macromolecular Substances (AREA)
- Greenhouses (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56161674A JPS5863727A (ja) | 1981-10-09 | 1981-10-09 | 表面を改質した樹脂成形品の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56161674A JPS5863727A (ja) | 1981-10-09 | 1981-10-09 | 表面を改質した樹脂成形品の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5863727A JPS5863727A (ja) | 1983-04-15 |
| JPS6412298B2 true JPS6412298B2 (enExample) | 1989-02-28 |
Family
ID=15739681
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56161674A Granted JPS5863727A (ja) | 1981-10-09 | 1981-10-09 | 表面を改質した樹脂成形品の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5863727A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100439580B1 (ko) * | 2001-11-05 | 2004-07-12 | 학교법인 포항공과대학교 | 소수성 기재의 표면을 친수성으로 개질하는 방법 |
-
1981
- 1981-10-09 JP JP56161674A patent/JPS5863727A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5863727A (ja) | 1983-04-15 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| NO794250L (no) | Fremgangsmaate til fremstilling av en polymerblanding, formede produkter derav, samt polymer-legering | |
| US5674934A (en) | Reversible and irreversible water-based coatings | |
| WO1992014785A1 (fr) | Dispersion aqueuse et materiau de base recouvert de cette dispersion | |
| JPH07508059A (ja) | 防曇性を有する親水性組成物 | |
| US4898908A (en) | Anionic polymer hydrogels and a process for making the same | |
| CN103649214A (zh) | 配制品 | |
| NL8002335A (nl) | Waterabsorberend mengsel. | |
| JPS6412300B2 (enExample) | ||
| JPS6412298B2 (enExample) | ||
| JPS62246984A (ja) | 防曇剤組成物 | |
| JPH0218357B2 (enExample) | ||
| JPS6412297B2 (enExample) | ||
| JPH06502358A (ja) | 親水性相互浸透性ネットワークの被覆 | |
| JPS6412299B2 (enExample) | ||
| JPS6412295B2 (enExample) | ||
| JPH0463095B2 (enExample) | ||
| JPS6412296B2 (enExample) | ||
| JPH0455616B2 (enExample) | ||
| JPH0478670B2 (enExample) | ||
| JPH01249343A (ja) | 表面被覆されたポリビニルアルコール系フイルム及びその製造方法 | |
| JP3580907B2 (ja) | アイオノマー組成物及びその薄膜ならびにその被膜が形成された成形品 | |
| JP3212044B2 (ja) | 多層構造体の製法 | |
| JP4205768B2 (ja) | 帯電防止剤 | |
| KR20070003246A (ko) | 대전방지용 수분산 코팅액 및 이를 이용하여 제조된대전방지성 폴리에스테르 필름 | |
| JP3426635B2 (ja) | 変性エチレン−ビニルアルコール系共重合体、分散安定剤および水性分散液 |