JPS639005B2 - - Google Patents
Info
- Publication number
- JPS639005B2 JPS639005B2 JP15872681A JP15872681A JPS639005B2 JP S639005 B2 JPS639005 B2 JP S639005B2 JP 15872681 A JP15872681 A JP 15872681A JP 15872681 A JP15872681 A JP 15872681A JP S639005 B2 JPS639005 B2 JP S639005B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- temperature
- cooling
- less
- strength
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15872681A JPS5861221A (ja) | 1981-10-07 | 1981-10-07 | 高強度高靭性鋼の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15872681A JPS5861221A (ja) | 1981-10-07 | 1981-10-07 | 高強度高靭性鋼の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5861221A JPS5861221A (ja) | 1983-04-12 |
JPS639005B2 true JPS639005B2 (enrdf_load_stackoverflow) | 1988-02-25 |
Family
ID=15677989
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15872681A Granted JPS5861221A (ja) | 1981-10-07 | 1981-10-07 | 高強度高靭性鋼の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5861221A (enrdf_load_stackoverflow) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0774379B2 (ja) * | 1989-09-16 | 1995-08-09 | 新日本製鐵株式会社 | 靭性の優れた低降伏比高張力鋼板の製造方法 |
-
1981
- 1981-10-07 JP JP15872681A patent/JPS5861221A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS5861221A (ja) | 1983-04-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP2013533384A (ja) | 超高強度鉄筋及びその製造方法 | |
JP2938101B2 (ja) | 冷間鍛造用鋼の製造方法 | |
JPS61104022A (ja) | 高温構造用鋼の製造方法 | |
KR20210108002A (ko) | 냉간압조용 선재 및 그 제조방법에 있어 열처리생략 | |
JPH0250916A (ja) | 細粒化組織の低合金高張力シームレス鋼管の製造法 | |
RU2430978C1 (ru) | Способ производства листового проката | |
JPS6250411A (ja) | 均質性にすぐれた圧延鋼材の製造方法 | |
JPH01319629A (ja) | 靭性の優れたCr−Mo鋼板の製造方法 | |
JPH0112815B2 (enrdf_load_stackoverflow) | ||
JPS639005B2 (enrdf_load_stackoverflow) | ||
JPH0257634A (ja) | 高強度鋼板の製造方法及びその加工品の熱処理方法 | |
JPH0570685B2 (enrdf_load_stackoverflow) | ||
JP2706159B2 (ja) | 溶接性の良好な低降伏比高張力鋼の製造方法 | |
JPS6156268A (ja) | 高靭性高張力鋼およびその製造法 | |
JPS62139821A (ja) | 高延性高強度冷延鋼板の製造方法 | |
JPS5952207B2 (ja) | 低降伏比、高靭性、高張力鋼板の製造方法 | |
JP2767254B2 (ja) | Cr−Mo肌焼鋼の製造方法 | |
JPH04358026A (ja) | 細粒化組織の低合金シームレス鋼管の製造法 | |
JPS6124454B2 (enrdf_load_stackoverflow) | ||
JP2564425B2 (ja) | 耐ssc性の優れた高靭性40キロ級鋼管の製造法 | |
JP3544625B2 (ja) | 熱間圧延直接焼入れ棒鋼とその製造方法 | |
JPH0670249B2 (ja) | 靭性に優れた調質型高張力鋼板の製造方法 | |
JPH0368715A (ja) | 強度・靭性に優れた構造用鋼板の製造方法 | |
JPS6056017A (ja) | 低温靭性の優れた厚鋼板の製造法 | |
CN116240456A (zh) | 核电站关键设备支撑用马氏体不锈钢板及其制造方法 |