- JPS6366374B2 JPS6366374B2 JP54101935A JP10193579A JPS6366374B2 JP S6366374 B2 JPS6366374 B2 JP S6366374B2 JP 54101935 A JP54101935 A JP 54101935A JP 10193579 A JP10193579 A JP 10193579A JP S6366374 B2 JPS6366374 B2 JP S6366374B2
- Authority
- JP
- Japan
- Prior art keywords
- ductility
- alloy
- added
- phase
- brittle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Manufacture Of Alloys Or Alloy Compounds (AREA)
Priority Applications (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10193579A JPS5625947A (en) | 1979-08-10 | 1979-08-10 | Ni3al alloy having improved ordinary temperature ductility and strength |
GB7936682A GB2037322B (en) | 1978-10-24 | 1979-10-23 | Super heat reistant alloys having high ductility at room temperature and high strength at high temperatures |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10193579A JPS5625947A (en) | 1979-08-10 | 1979-08-10 | Ni3al alloy having improved ordinary temperature ductility and strength |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5625947A JPS5625947A (en) | 1981-03-12 |
JPS6366374B2 true JPS6366374B2 (enrdf_load_stackoverflow) | 1988-12-20 |
Family
ID=14313762
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10193579A Granted JPS5625947A (en) | 1978-10-24 | 1979-08-10 | Ni3al alloy having improved ordinary temperature ductility and strength |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5625947A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2006158737A (ja) * | 2004-12-08 | 2006-06-22 | Terumo Corp | ガイドワイヤ |
-
1979
- 1979-08-10 JP JP10193579A patent/JPS5625947A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2006158737A (ja) * | 2004-12-08 | 2006-06-22 | Terumo Corp | ガイドワイヤ |
Also Published As
Publication number | Publication date |
---|---|
JPS5625947A (en) | 1981-03-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN110317990B (zh) | 一种Ni-Co-Al-Cr-Fe系单晶高熵高温合金及其制备方法 | |
JP5582532B2 (ja) | Co基合金 | |
US4879092A (en) | Titanium aluminum alloys modified by chromium and niobium and method of preparation | |
JP3027200B2 (ja) | 耐酸化性低膨張合金 | |
EP1900835A1 (en) | Cobalt-chromium-iron-nickel alloys amenable to nitride strengthening | |
JP2635804B2 (ja) | 炭素、クロムおよびニオブで改変されたγ‐チタン‐アルミニウム合金 | |
JPH03104833A (ja) | クロムとタンタルで改変されたγ‐チタン‐アルミニウム合金およびその製造方法 | |
JP5127144B2 (ja) | 2重複相組織からなるVおよびTiを含有するNi3Al基金属間化合物及びその製造方法,耐熱構造材 | |
US5076858A (en) | Method of processing titanium aluminum alloys modified by chromium and niobium | |
JPH03274238A (ja) | 加工性に優れた高強度チタン合金およびその合金材の製造方法ならびにその超塑性加工法 | |
JPH0730419B2 (ja) | クロムとケイ素で改変されたγ‐チタン‐アルミニウム合金およびその製造方法 | |
JP6660042B2 (ja) | Ni基超耐熱合金押出材の製造方法およびNi基超耐熱合金押出材 | |
US5167732A (en) | Nickel aluminide base single crystal alloys | |
JP4264411B2 (ja) | 高強度α+β型チタン合金 | |
GB2037322A (en) | Super heat resistant alloys having high ductility at room temperature and high strength at high temperatures | |
JPH05255781A (ja) | クロム、ホウ素およびニオブで改良されている加工されたガンマ‐アルミニウム化チタン合金 | |
JPH01255632A (ja) | 常温靭性を有するTi―Al系金属間化合物型鋳造合金 | |
JPH04501440A (ja) | 高温構造材用の改良ニッケルアルミニド合金 | |
US5304344A (en) | Gamma titanium aluminum alloys modified by chromium and tungsten and method of preparation | |
JPH0441641A (ja) | 金型用ニッケル基超耐熱合金 | |
JPH05255782A (ja) | クロム、ニオブおよびケイ素で改良された鋳造ガンマ‐チタン・アルミニウム合金ならびにその製法 | |
JPS6366374B2 (enrdf_load_stackoverflow) | ||
JPH0218374B2 (enrdf_load_stackoverflow) | ||
JPS6323257B2 (enrdf_load_stackoverflow) | ||
US5725691A (en) | Nickel aluminide alloy suitable for structural applications |