JPS6358696B2 - - Google Patents
Info
- Publication number
- JPS6358696B2 JPS6358696B2 JP55060364A JP6036480A JPS6358696B2 JP S6358696 B2 JPS6358696 B2 JP S6358696B2 JP 55060364 A JP55060364 A JP 55060364A JP 6036480 A JP6036480 A JP 6036480A JP S6358696 B2 JPS6358696 B2 JP S6358696B2
- Authority
- JP
- Japan
- Prior art keywords
- rubber
- molded
- minutes
- sputter etching
- sample
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Treatments Of Macromolecular Shaped Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6036480A JPS56157336A (en) | 1980-05-07 | 1980-05-07 | Surface treatment of rubber |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6036480A JPS56157336A (en) | 1980-05-07 | 1980-05-07 | Surface treatment of rubber |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS56157336A JPS56157336A (en) | 1981-12-04 |
| JPS6358696B2 true JPS6358696B2 (cg-RX-API-DMAC7.html) | 1988-11-16 |
Family
ID=13140004
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6036480A Granted JPS56157336A (en) | 1980-05-07 | 1980-05-07 | Surface treatment of rubber |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS56157336A (cg-RX-API-DMAC7.html) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100517430B1 (ko) * | 2002-11-22 | 2005-09-29 | 한국타이어 주식회사 | 내부 박리를 방지하기 위한 타이어 가류 브래더 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5930730B2 (ja) * | 1976-08-19 | 1984-07-28 | 積水化学工業株式会社 | ブロツキング性の改善されたポリビニルブチラ−ルシ−トの製造方法 |
| JPS5513753A (en) * | 1978-07-18 | 1980-01-30 | Achilles Corp | Production of molded plastic product freed from the migration of additive |
-
1980
- 1980-05-07 JP JP6036480A patent/JPS56157336A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS56157336A (en) | 1981-12-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR100743409B1 (ko) | 탈착성이 우수한 불소함유 엘라스토머 성형품 및 그 제조방법 | |
| Kang et al. | Surface modifications of polyaniline films by graft copolymerization | |
| JP3594884B2 (ja) | 複合材の製法およびそれによって得られる複合材 | |
| JPS6393650A (ja) | ワイパブレ−ド用ゴム | |
| JP3661723B2 (ja) | ゴム系複合材料の製造方法 | |
| JP2003268533A (ja) | 冷却およびエアコンディショニングにおける使用のための金属表面のプラズマ重合による改良 | |
| JPS6358696B2 (cg-RX-API-DMAC7.html) | ||
| Cho et al. | Improvement of paint adhesion to a polypropylene bumper by plasma treatment | |
| US4349403A (en) | Method for bonding elastomers to steel | |
| JP3232643B2 (ja) | ゴム系複合材料の製造方法 | |
| CN1245547C (zh) | 一种对高分子纤维材料表面改性的方法 | |
| KR100438941B1 (ko) | 플라즈마를 이용한 내식성 및 친수성을 가지는 다층막형성방법 | |
| CN1858091A (zh) | 真空射频等离子体极化处理氟橡胶的方法 | |
| JPS5973673A (ja) | リ−ドバルブ | |
| US20070173179A1 (en) | Method of changing the surface wettability of polymer materials | |
| JP2000129015A (ja) | フッ素樹脂成形物の表面改質方法 | |
| JPS6241232A (ja) | 加硫ゴムと他材料との接着方法 | |
| JPS5971336A (ja) | 成形ゴム材料の表面処理方法 | |
| JP3146647B2 (ja) | 加硫ゴムの表面処理方法 | |
| CN116836443B (zh) | 一种增强聚四氟乙烯材料表面粘接性能的两步等离子体处理方法 | |
| JPH0730183B2 (ja) | 加硫ゴムと他材料との接着方法 | |
| CN223083114U (zh) | 一种pe片材涂覆装置 | |
| JPH07102090A (ja) | 弗素樹脂製チューブの表面改質法 | |
| JPH0260939A (ja) | ゴム材料の表面導電化法 | |
| JPS59190576A (ja) | 低トルクシ−ル |