JPS6331435B2 - - Google Patents
Info
- Publication number
- JPS6331435B2 JPS6331435B2 JP54121012A JP12101279A JPS6331435B2 JP S6331435 B2 JPS6331435 B2 JP S6331435B2 JP 54121012 A JP54121012 A JP 54121012A JP 12101279 A JP12101279 A JP 12101279A JP S6331435 B2 JPS6331435 B2 JP S6331435B2
- Authority
- JP
- Japan
- Prior art keywords
- fluidity
- repair material
- adhesion
- frit
- resin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Ceramic Products (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP12101279A JPS5645867A (en) | 1979-09-19 | 1979-09-19 | Thermally repairing material |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP12101279A JPS5645867A (en) | 1979-09-19 | 1979-09-19 | Thermally repairing material |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5645867A JPS5645867A (en) | 1981-04-25 |
| JPS6331435B2 true JPS6331435B2 (enExample) | 1988-06-23 |
Family
ID=14800609
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP12101279A Granted JPS5645867A (en) | 1979-09-19 | 1979-09-19 | Thermally repairing material |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5645867A (enExample) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS58181769A (ja) * | 1982-04-20 | 1983-10-24 | タイホ−工業株式会社 | 工業用炉の補修方法 |
| JPS59137336A (ja) * | 1983-01-21 | 1984-08-07 | Sumitomo Electric Ind Ltd | 円柱状石英ガラスと石英パイプの溶着法 |
| US5346942A (en) * | 1989-10-11 | 1994-09-13 | Shinagawa Refractories Co., Ltd. | Monolithic refractories |
| EP0447562B1 (en) * | 1989-10-11 | 1995-05-24 | Shinagawa Refractories Co., Ltd. | Amorphous refractory material |
| JP2556418B2 (ja) * | 1992-07-14 | 1996-11-20 | 大光炉材株式会社 | 不定形耐火材 |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59471B2 (ja) * | 1976-08-30 | 1984-01-06 | 黒崎窯業株式会社 | 熱間補修用不定形耐火材 |
| JPS603035B2 (ja) * | 1977-06-25 | 1985-01-25 | 住友金属工業株式会社 | 低温硬化性高炉用圧入材組成物 |
| JPS5542218A (en) * | 1978-09-13 | 1980-03-25 | Kurosaki Refractories Co | Refractory for spray |
-
1979
- 1979-09-19 JP JP12101279A patent/JPS5645867A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5645867A (en) | 1981-04-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0007646B1 (en) | Coke oven patching and sealing material, method of patching and sealing cracks in coke ovens | |
| CA2255322A1 (en) | Repairing material for bricks of carbonizing chamber in coke oven and repairing method | |
| CN108017376A (zh) | 一种镁碳砖及其生产方法 | |
| CN101913893A (zh) | 一种转炉大面热态修补料 | |
| CN103687828A (zh) | 不定形耐火物 | |
| CN106995309A (zh) | 耐火衬体裂缝补缝料 | |
| US3303031A (en) | Carbonaceous ramming paste | |
| JPS6331435B2 (enExample) | ||
| JPS63156081A (ja) | 熱間投入補修材 | |
| US4436678A (en) | Method for hot repairing the inside of a furnace | |
| JP3222709B2 (ja) | 粉末状焼付け補修材 | |
| JP3037625B2 (ja) | 焼付け補修材 | |
| JPS6220476B2 (enExample) | ||
| JPS61242962A (ja) | 窯炉の炉壁熱間補修材 | |
| JPS6154746B2 (enExample) | ||
| CN102115336A (zh) | 干式喷补料 | |
| JPS59137368A (ja) | 補修用不定形耐火物 | |
| JPH09278556A (ja) | 目地用成形体 | |
| JPS60145968A (ja) | 溶融金属容器の内張り目地充填材 | |
| JP2010235340A (ja) | 熱間補修用水系吹付材 | |
| JP2644404B2 (ja) | 目地用成形体 | |
| JPS5915115B2 (ja) | アルミナ−クロム系振動成形材 | |
| JPH08134380A (ja) | 炭素含有煉瓦用被覆材 | |
| JPS62176963A (ja) | 流し込み施工される高炉出銑孔周り充填材 | |
| JPS5869782A (ja) | 不定形耐火物 |