JPS6318663B2 - - Google Patents
Info
- Publication number
- JPS6318663B2 JPS6318663B2 JP55120328A JP12032880A JPS6318663B2 JP S6318663 B2 JPS6318663 B2 JP S6318663B2 JP 55120328 A JP55120328 A JP 55120328A JP 12032880 A JP12032880 A JP 12032880A JP S6318663 B2 JPS6318663 B2 JP S6318663B2
- Authority
- JP
- Japan
- Prior art keywords
- corrosion
- steel
- gas
- carbon dioxide
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Rigid Pipes And Flexible Pipes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP55120328A JPS5743958A (en) | 1980-08-30 | 1980-08-30 | Steel material for line pipe with excellent carbon dioxide corrosion resistance |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP55120328A JPS5743958A (en) | 1980-08-30 | 1980-08-30 | Steel material for line pipe with excellent carbon dioxide corrosion resistance |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5743958A JPS5743958A (en) | 1982-03-12 |
| JPS6318663B2 true JPS6318663B2 (Direct) | 1988-04-19 |
Family
ID=14783531
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP55120328A Granted JPS5743958A (en) | 1980-08-30 | 1980-08-30 | Steel material for line pipe with excellent carbon dioxide corrosion resistance |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5743958A (Direct) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01269752A (ja) * | 1988-04-21 | 1989-10-27 | Mazda Motor Corp | オートテンショナ |
| JPH081197U (ja) * | 1995-10-02 | 1996-07-30 | エヌティエヌ株式会社 | オートテンショナ |
| JPH081198U (ja) * | 1995-10-02 | 1996-07-30 | エヌティエヌ株式会社 | オートテンショナ |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5401931B2 (ja) * | 2008-11-07 | 2014-01-29 | Jfeスチール株式会社 | 高圧炭酸ガスインジェクション用部材 |
| JP2010242162A (ja) * | 2009-04-06 | 2010-10-28 | Jfe Steel Corp | 超臨界圧炭酸ガスインジェクション用Cr含有鋼管 |
| CN102199729A (zh) * | 2010-03-23 | 2011-09-28 | 宝山钢铁股份有限公司 | 经济型55Ksi钢级抗CO2腐蚀油井管及其制造方法 |
| CN105648337B (zh) * | 2016-01-15 | 2017-06-23 | 宝山钢铁股份有限公司 | 一种低碳抗co2正火态无缝管线管及其制造方法 |
| CN106399862B (zh) * | 2016-09-28 | 2017-12-29 | 睿智钢业有限公司 | 一种高强防腐钢材及其制备方法和应用 |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5024244B2 (Direct) * | 1971-09-03 | 1975-08-14 | ||
| JPS531201B2 (Direct) * | 1971-10-09 | 1978-01-17 | ||
| JPS5915976B2 (ja) * | 1975-09-03 | 1984-04-12 | 住友金属工業株式会社 | 耐酸化性の優れたフエライト系ステンレス鋼 |
| JPS575846A (en) * | 1980-06-11 | 1982-01-12 | Kawasaki Steel Corp | Low-alloyed steel having sweet corrosion resistance |
| JPS575848A (en) * | 1980-06-16 | 1982-01-12 | Kawasaki Steel Corp | Low-alloyed steel having sweet corrosion resistance |
| JPS575847A (en) * | 1980-06-16 | 1982-01-12 | Kawasaki Steel Corp | Low-alloyed steel having sweet corrosion resistance |
-
1980
- 1980-08-30 JP JP55120328A patent/JPS5743958A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01269752A (ja) * | 1988-04-21 | 1989-10-27 | Mazda Motor Corp | オートテンショナ |
| JPH081197U (ja) * | 1995-10-02 | 1996-07-30 | エヌティエヌ株式会社 | オートテンショナ |
| JPH081198U (ja) * | 1995-10-02 | 1996-07-30 | エヌティエヌ株式会社 | オートテンショナ |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5743958A (en) | 1982-03-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN101415852B (zh) | 原油罐用耐腐蚀钢材及原油罐 | |
| JP4449691B2 (ja) | カーゴオイルタンク用鋼材 | |
| JPS6318663B2 (Direct) | ||
| KR101314022B1 (ko) | 내식성이 우수한 용접 이음매 및 원유 탱크 | |
| CN106435396A (zh) | 一种耐高温抗硫化氢腐蚀的压力容器用钢板及其制造方法 | |
| Kimura et al. | High Cr stainless steel OCTG with high strength and superior corrosion resistance | |
| US5417918A (en) | Austenitic nickel alloy | |
| Craig | Temperature and velocity effects in naphthenic acid corrosion | |
| US5151248A (en) | Pd-added austenitic stainless steel for use for high temperature concentrated sulfuric acid | |
| JP4243863B2 (ja) | 原油タンク用溶接継手及び原油タンク | |
| JPH0129859B2 (Direct) | ||
| JPH0114304B2 (Direct) | ||
| US6019942A (en) | Method of maintaining the corrosion resistance of a steel circulation system with a lead-containing coolant | |
| JPH07136748A (ja) | 高耐食性電縫鋼管用鋼の製造方法 | |
| JPS6032709B2 (ja) | 含p高溶接性耐食鋼 | |
| JPS6362569B2 (Direct) | ||
| RU2016130C1 (ru) | Коррозионностойкая сталь | |
| JPS60224764A (ja) | 高温用n含有オ−ステナイトステンレス鋼 | |
| JP4048874B2 (ja) | 原油タンク底板用鋼材 | |
| JPH10237601A (ja) | 耐中性塩化物腐食性オーステナイト系ステンレス鋼 | |
| CN112481440A (zh) | 一种耐点蚀钢轨及其制备方法 | |
| RU2039121C1 (ru) | Коррозионностойкая сталь | |
| JPH0534419B2 (Direct) | ||
| SU771179A1 (ru) | Ферритна сталь | |
| JPS6151022B2 (Direct) |