JPS63102738U - - Google Patents
Info
- Publication number
- JPS63102738U JPS63102738U JP19816486U JP19816486U JPS63102738U JP S63102738 U JPS63102738 U JP S63102738U JP 19816486 U JP19816486 U JP 19816486U JP 19816486 U JP19816486 U JP 19816486U JP S63102738 U JPS63102738 U JP S63102738U
- Authority
- JP
- Japan
- Prior art keywords
- processing liquid
- tank
- processing
- silicon dioxide
- constant temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Surface Treatment Of Glass (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19816486U JPH0538016Y2 (ref) | 1986-12-23 | 1986-12-23 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19816486U JPH0538016Y2 (ref) | 1986-12-23 | 1986-12-23 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63102738U true JPS63102738U (ref) | 1988-07-04 |
| JPH0538016Y2 JPH0538016Y2 (ref) | 1993-09-27 |
Family
ID=31158604
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP19816486U Expired - Lifetime JPH0538016Y2 (ref) | 1986-12-23 | 1986-12-23 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0538016Y2 (ref) |
-
1986
- 1986-12-23 JP JP19816486U patent/JPH0538016Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0538016Y2 (ref) | 1993-09-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS63102738U (ref) | ||
| JPS60168574U (ja) | 酸化珪素被膜の製造装置 | |
| Görnert et al. | Growth rate anisotropy and kinetic coefficients of vicinal faces at LPE garnet films. II. Kinetic coefficients | |
| JPH0158631U (ref) | ||
| JPS6016427A (ja) | 酸化膜エツチング装置 | |
| JPS6378538A (ja) | 処理装置 | |
| JPH0749790Y2 (ja) | 半導体ウェーハの洗浄装置 | |
| CN102157352A (zh) | 一种微纳结构的湿法腐蚀方法及其腐蚀装置 | |
| JPH0195728U (ref) | ||
| JPS6076035U (ja) | シリコンウェファの処理装置 | |
| JPH03112806A (ja) | 二酸化珪素被膜の製造方法及び装置 | |
| JPS6012285B2 (ja) | 硫化カドミウム析出膜の製造法 | |
| US341083A (en) | Method of preparing paper for photographic printing | |
| JPS5887336U (ja) | 蝕刻装置 | |
| JPS6212870U (ref) | ||
| JPS63264115A (ja) | 処理液循環濾過方法 | |
| JPS61117249U (ref) | ||
| JPS6351638U (ref) | ||
| JP3070226B2 (ja) | 循環恒温式ウエットエッチング装置 | |
| JPS63167730U (ref) | ||
| JPS6410596B2 (ref) | ||
| JPS5348264A (en) | Heat transfer surface by ebullition | |
| JPS636729U (ref) | ||
| JPH0533863U (ja) | 塗布装置 | |
| KR19980056106A (ko) | 반도체 장치의 습식 스테이션 |