JPS629185B2 - - Google Patents
Info
- Publication number
- JPS629185B2 JPS629185B2 JP57223319A JP22331982A JPS629185B2 JP S629185 B2 JPS629185 B2 JP S629185B2 JP 57223319 A JP57223319 A JP 57223319A JP 22331982 A JP22331982 A JP 22331982A JP S629185 B2 JPS629185 B2 JP S629185B2
- Authority
- JP
- Japan
- Prior art keywords
- temperature
- alloy
- transformation
- heat treatment
- concentration
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Nonferrous Metals Or Alloys (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22331982A JPS59113167A (ja) | 1982-12-20 | 1982-12-20 | チタン・ニツケル形状記憶合金の熱処理方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22331982A JPS59113167A (ja) | 1982-12-20 | 1982-12-20 | チタン・ニツケル形状記憶合金の熱処理方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59113167A JPS59113167A (ja) | 1984-06-29 |
| JPS629185B2 true JPS629185B2 (cs) | 1987-02-26 |
Family
ID=16796284
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP22331982A Granted JPS59113167A (ja) | 1982-12-20 | 1982-12-20 | チタン・ニツケル形状記憶合金の熱処理方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59113167A (cs) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6106642A (en) | 1998-02-19 | 2000-08-22 | Boston Scientific Limited | Process for the improved ductility of nitinol |
| WO2004092431A1 (en) * | 2003-04-18 | 2004-10-28 | The University Of Hong Kong | Shape memory material and method of making the same |
| US8714976B2 (en) * | 2009-11-17 | 2014-05-06 | William B. Johnson | Fatigue-resistant Nitinol instrument |
| CN107475652B (zh) * | 2017-08-22 | 2019-03-05 | 哈尔滨工程大学 | 一种调控TiNi基记忆合金中R相存在区间的方法 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5123428A (en) * | 1974-08-21 | 1976-02-25 | Matsushita Electric Industrial Co Ltd | Nitsukeruchitangokinno seizokakohoho |
-
1982
- 1982-12-20 JP JP22331982A patent/JPS59113167A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS59113167A (ja) | 1984-06-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US7083687B2 (en) | Super-elastic titanium alloy for medical uses | |
| JP3521253B2 (ja) | 生体用形状記憶合金 | |
| JP3753380B2 (ja) | 生体用超弾性チタン合金の製造方法及び生体用超弾性チタン合金 | |
| JPS6214619B2 (cs) | ||
| JP2000328158A (ja) | プレス打抜き性が優れた銅合金板 | |
| JPS635465B2 (cs) | ||
| JPH0762472A (ja) | 高加工性銅系形状記憶合金とその製造方法 | |
| JPS629185B2 (cs) | ||
| JPS58157935A (ja) | 形状記憶合金 | |
| JP2004197112A (ja) | 生体用超弾性チタン合金の製造方法 | |
| JPS6361377B2 (cs) | ||
| WO2004055222A1 (ja) | NbC添加Fe−Mn−Si系形状記憶合金の加工熱処理方法 | |
| US6319340B1 (en) | Ti-V-A1 based superelasticity alloy and process for preparation thereof | |
| JPS5942741B2 (ja) | 半硬質磁石合金およびその製造方法 | |
| JP2004124156A (ja) | 生体用超弾性TiNbSn合金の製造方法 | |
| JP3933623B2 (ja) | 生体用超弾性チタン合金の製造方法および超弾性用チタン合金 | |
| JP4554250B2 (ja) | Ti基合金形状記憶素子 | |
| JPS62250136A (ja) | Cu合金製端子 | |
| JP2691567B2 (ja) | 超弾性素子 | |
| JP2603463B2 (ja) | 低温可逆形状記憶合金 | |
| JP3141328B2 (ja) | 超弾性バネ合金の製造方法 | |
| JP2005105388A6 (ja) | 生体用超弾性チタン合金の製造方法および超弾性用チタン合金 | |
| JP2005105388A (ja) | 生体用超弾性チタン合金の製造方法および超弾性用チタン合金 | |
| JP2784613B2 (ja) | 低熱膨張材料の製造方法 | |
| JPH048495B2 (cs) |