JPS6281273A - ニツケル又はニツケル合金クラツド鋼板の突合せ溶接方法 - Google Patents
ニツケル又はニツケル合金クラツド鋼板の突合せ溶接方法Info
- Publication number
- JPS6281273A JPS6281273A JP22115585A JP22115585A JPS6281273A JP S6281273 A JPS6281273 A JP S6281273A JP 22115585 A JP22115585 A JP 22115585A JP 22115585 A JP22115585 A JP 22115585A JP S6281273 A JPS6281273 A JP S6281273A
- Authority
- JP
- Japan
- Prior art keywords
- welding
- nickel
- groove
- composite material
- clad steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Arc Welding In General (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP22115585A JPS6281273A (ja) | 1985-10-05 | 1985-10-05 | ニツケル又はニツケル合金クラツド鋼板の突合せ溶接方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP22115585A JPS6281273A (ja) | 1985-10-05 | 1985-10-05 | ニツケル又はニツケル合金クラツド鋼板の突合せ溶接方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6281273A true JPS6281273A (ja) | 1987-04-14 |
JPH0465752B2 JPH0465752B2 (cs) | 1992-10-21 |
Family
ID=16762335
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP22115585A Granted JPS6281273A (ja) | 1985-10-05 | 1985-10-05 | ニツケル又はニツケル合金クラツド鋼板の突合せ溶接方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6281273A (cs) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN111390350A (zh) * | 2020-03-26 | 2020-07-10 | 鲁西工业装备有限公司 | 一种c-276复合板埋弧焊接方法 |
-
1985
- 1985-10-05 JP JP22115585A patent/JPS6281273A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN111390350A (zh) * | 2020-03-26 | 2020-07-10 | 鲁西工业装备有限公司 | 一种c-276复合板埋弧焊接方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0465752B2 (cs) | 1992-10-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP2692476B1 (en) | Method for producing laser-welded steel tube | |
WO2022083013A1 (zh) | 一种铝合金薄板大间隙对接的摆动激光填丝焊方法 | |
JPS6332554B2 (cs) | ||
CA1144092A (en) | Thick welded steel pipe of large diameter and production thereof | |
Asai et al. | Application of plasma MIG hybrid welding to dissimilar joints between copper and steel | |
JPH08243754A (ja) | クラッド鋼管の内面溶接方法 | |
KR101008078B1 (ko) | 하이브리드 용접 방법 | |
JP3182672B2 (ja) | クラッド鋼管の内面溶接方法 | |
JPS60221173A (ja) | クラツド管の製造方法 | |
JPS6281273A (ja) | ニツケル又はニツケル合金クラツド鋼板の突合せ溶接方法 | |
JP2563684B2 (ja) | ステンレスクラッド鋼管の溶接方法 | |
JPH07290244A (ja) | クラッド鋼管の溶接方法 | |
JPH08276273A (ja) | クラッド鋼の突合せ溶接方法 | |
KR20240119334A (ko) | 편면 서브머지드 아크 용접 방법 그리고 용접 이음매 및 그 제조 방법 | |
JP2008238265A (ja) | T型継手の貫通溶接方法及びt型継手の貫通溶接構造物 | |
JP7626379B2 (ja) | ハイブリッド溶接方法および溶接継手の製造方法 | |
KR20230121147A (ko) | 레이저 브레이징 접합 방법 | |
JPH08229685A (ja) | クラッド鋼管の溶接方法 | |
JP2833279B2 (ja) | 鋼管の溶接方法 | |
JP2002336982A (ja) | 薄板構造継手の複合溶接方法 | |
JP7560002B1 (ja) | 狭開先ガスシールドアーク溶接方法 | |
JP7571920B1 (ja) | 狭開先ガスシールドアーク溶接方法 | |
US20060027549A1 (en) | Buried arc welding of integrally backed square butt joints | |
JPH06285639A (ja) | クラッド鋼管の内面シーム溶接方法 | |
JPS6030585A (ja) | ステンレスクラツド鋼管の製造方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EXPY | Cancellation because of completion of term |