JPS6219275B2 - - Google Patents
Info
- Publication number
- JPS6219275B2 JPS6219275B2 JP6637082A JP6637082A JPS6219275B2 JP S6219275 B2 JPS6219275 B2 JP S6219275B2 JP 6637082 A JP6637082 A JP 6637082A JP 6637082 A JP6637082 A JP 6637082A JP S6219275 B2 JPS6219275 B2 JP S6219275B2
- Authority
- JP
- Japan
- Prior art keywords
- welding
- segregation
- cracking
- hydrogen
- heating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/235—Preliminary treatment
Landscapes
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Mechanical Engineering (AREA)
- Arc Welding In General (AREA)
- Butt Welding And Welding Of Specific Article (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6637082A JPS58184089A (ja) | 1982-04-22 | 1982-04-22 | ラインパイプの現地溶接における偏析割れ防止法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6637082A JPS58184089A (ja) | 1982-04-22 | 1982-04-22 | ラインパイプの現地溶接における偏析割れ防止法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58184089A JPS58184089A (ja) | 1983-10-27 |
JPS6219275B2 true JPS6219275B2 (enrdf_load_stackoverflow) | 1987-04-27 |
Family
ID=13313876
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6637082A Granted JPS58184089A (ja) | 1982-04-22 | 1982-04-22 | ラインパイプの現地溶接における偏析割れ防止法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS58184089A (enrdf_load_stackoverflow) |
-
1982
- 1982-04-22 JP JP6637082A patent/JPS58184089A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS58184089A (ja) | 1983-10-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN101622365B (zh) | 使用焊后热处理改善缝焊接头性能的方法 | |
CN105665898B (zh) | 一种珠光体耐热钢复合板埋弧自动焊焊接方法 | |
CN109266971B (zh) | 一种抗再热裂纹的含w高强度低合金耐热钢 | |
CN109865955B (zh) | G115大口径管手工钨极氩弧焊和焊条电弧焊结合的焊接方法 | |
US20150202710A1 (en) | Method of welding structural steel and welded steel structure | |
CN111451615A (zh) | 一种异种钢的焊接工艺方法 | |
CN106312268A (zh) | 一种低活化马氏体钢和316l不锈钢异种钢接头的焊接工艺 | |
CN117600655A (zh) | 一种铝硅镀层热成形钢用焊丝及焊接方法 | |
CN114406512B (zh) | 一种用于异种合金的焊接及电脉冲热处理工艺 | |
CN109530849B (zh) | 一种酸性环境碳钢管道焊接施工方法 | |
Maruyama | Arc welding technology for dissimilar joints | |
JPS6219275B2 (enrdf_load_stackoverflow) | ||
US6307178B1 (en) | Method for welding shaped bodies made of carburized heat-resistant steel | |
CN101805822A (zh) | 15CrMoG钢环形焊缝热处理方法 | |
CN112388195A (zh) | 一种中碳调质铸钢的焊接方法 | |
Kumar et al. | Effect of post weld heat treatment on impact toughness of SA 516 GR. 70 Low Carbon Steel Welded by Saw Process | |
JPS58153731A (ja) | 溶接残留応力の低減方法 | |
CN103658923A (zh) | 异种钢的焊接方法 | |
JP3674085B2 (ja) | 原子炉圧力容器ノズルの熱処理方法 | |
CN102941399A (zh) | 珠光体耐热钢结构件气保护焊接方法 | |
JPS63176434A (ja) | 溶接部の熱処理方法 | |
JPS59163094A (ja) | 耐熱耐食合金鋼溶接割れ防止法 | |
JPS5832594A (ja) | 溶接方法 | |
Liu et al. | Welding defects of SUPER304H steel and their countermeasures | |
US2146315A (en) | Method of making welded ferrous metal articles |