JPS62174209A - 膨潤性物質の製造方法 - Google Patents
膨潤性物質の製造方法Info
- Publication number
- JPS62174209A JPS62174209A JP28330986A JP28330986A JPS62174209A JP S62174209 A JPS62174209 A JP S62174209A JP 28330986 A JP28330986 A JP 28330986A JP 28330986 A JP28330986 A JP 28330986A JP S62174209 A JPS62174209 A JP S62174209A
- Authority
- JP
- Japan
- Prior art keywords
- polymerization
- water
- ammonium
- acrylic acid
- solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Polymerisation Methods In General (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28330986A JPS62174209A (ja) | 1986-11-29 | 1986-11-29 | 膨潤性物質の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28330986A JPS62174209A (ja) | 1986-11-29 | 1986-11-29 | 膨潤性物質の製造方法 |
Related Parent Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13090278A Division JPS5558208A (en) | 1978-10-24 | 1978-10-24 | Production of swelling substance |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62174209A true JPS62174209A (ja) | 1987-07-31 |
| JPH0260681B2 JPH0260681B2 (enExample) | 1990-12-18 |
Family
ID=17663787
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP28330986A Granted JPS62174209A (ja) | 1986-11-29 | 1986-11-29 | 膨潤性物質の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62174209A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2004503762A (ja) * | 2000-06-15 | 2004-02-05 | スカンラブ アーゲー | スキャンニング装置用の位置検出器 |
-
1986
- 1986-11-29 JP JP28330986A patent/JPS62174209A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2004503762A (ja) * | 2000-06-15 | 2004-02-05 | スカンラブ アーゲー | スキャンニング装置用の位置検出器 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0260681B2 (enExample) | 1990-12-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0922717B1 (en) | Production process of water-absorbent resin | |
| US5567478A (en) | Process for producing a water-absorbing sheet material and the use thereof | |
| EP0398653B1 (en) | Process for producing highly water-absorptive polymers | |
| EP0238050B1 (de) | Verfahren zur diskontinuierlichen Herstellung von vernetzten, feinteiligen Polymerisaten | |
| EP0289338B2 (en) | Hydrophilic polymer and method for production | |
| US5210298A (en) | Method for production of acrylate and acrylate-containing polymer | |
| US5124416A (en) | Method for production of absorbent polymer | |
| US5185413A (en) | Process for producing highly water-absortive polymers | |
| US3405106A (en) | Polymerization of water soluble vinyl monomers in presence of metal salts | |
| EP2641920A1 (en) | Method for producing water-absorbent resin | |
| JPH0114242B2 (enExample) | ||
| JPH11228604A (ja) | 吸水性樹脂の製造方法 | |
| JP2954360B2 (ja) | 吸水性複合体の製造法 | |
| JP3603970B2 (ja) | 粉末の吸水性樹脂組成物の製造方法 | |
| EP0206808A2 (en) | Continuous method for preparing polyacrylate resins | |
| JPS62174209A (ja) | 膨潤性物質の製造方法 | |
| JPS6228801B2 (enExample) | ||
| US4820742A (en) | Method for continuous manufacture of solid water absorbing resin | |
| JPH0214925B2 (enExample) | ||
| JPH0364301A (ja) | 吸水性ポリマーの製造方法 | |
| JP2745703B2 (ja) | 吸水性ポリマーの製造方法 | |
| JPH0678390B2 (ja) | 吸水性ポリマーの製造方法 | |
| JPH02242809A (ja) | 耐塩性吸水性樹脂の製造法 | |
| JPH0321562B2 (enExample) | ||
| JPH02129207A (ja) | 吸水性ポリマーの製造方法 |