JPS62161992A - 無機多孔質体の表面強化法 - Google Patents
無機多孔質体の表面強化法Info
- Publication number
- JPS62161992A JPS62161992A JP393686A JP393686A JPS62161992A JP S62161992 A JPS62161992 A JP S62161992A JP 393686 A JP393686 A JP 393686A JP 393686 A JP393686 A JP 393686A JP S62161992 A JPS62161992 A JP S62161992A
- Authority
- JP
- Japan
- Prior art keywords
- porous body
- inorg
- inorganic porous
- impregnated
- org
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Powder Metallurgy (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP393686A JPS62161992A (ja) | 1986-01-11 | 1986-01-11 | 無機多孔質体の表面強化法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP393686A JPS62161992A (ja) | 1986-01-11 | 1986-01-11 | 無機多孔質体の表面強化法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62161992A true JPS62161992A (ja) | 1987-07-17 |
| JPH0244914B2 JPH0244914B2 (enExample) | 1990-10-05 |
Family
ID=11571020
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP393686A Granted JPS62161992A (ja) | 1986-01-11 | 1986-01-11 | 無機多孔質体の表面強化法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62161992A (enExample) |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0428898A (ja) * | 1990-05-25 | 1992-01-31 | Yokoyama Hyomen Kogyo Kk | 陽極酸化皮膜を有する物品及びその製造方法 |
| WO2008092947A1 (en) * | 2007-02-01 | 2008-08-07 | Shell Internationale Research Maatschappij B.V. | Organic molybdenum compounds and lubricating compositions which contain said compounds |
| JP2010001507A (ja) * | 2008-06-18 | 2010-01-07 | Minoru Mitani | アルミニウム又はアルミニウム合金の表面処理方法及びその表面処理方法により処理されたアルミニウム又はその合金製品 |
| US8158565B2 (en) | 2007-02-01 | 2012-04-17 | Shell Oil Company | Molybdenum alkylxanthates and lubricating compositions |
| US8188017B2 (en) | 2007-02-01 | 2012-05-29 | Shell Oil Company | Organic molybdenum compounds and oil compositions containing the same |
| US8329624B2 (en) | 2007-02-01 | 2012-12-11 | Shell Oil Company | Organic molybdenum compounds and lubricating compositions which contain said compounds |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS58217699A (ja) * | 1982-06-11 | 1983-12-17 | Pilot Precision Co Ltd | 潤滑性を有するa1のアノ−ド皮膜 |
-
1986
- 1986-01-11 JP JP393686A patent/JPS62161992A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS58217699A (ja) * | 1982-06-11 | 1983-12-17 | Pilot Precision Co Ltd | 潤滑性を有するa1のアノ−ド皮膜 |
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0428898A (ja) * | 1990-05-25 | 1992-01-31 | Yokoyama Hyomen Kogyo Kk | 陽極酸化皮膜を有する物品及びその製造方法 |
| WO2008092947A1 (en) * | 2007-02-01 | 2008-08-07 | Shell Internationale Research Maatschappij B.V. | Organic molybdenum compounds and lubricating compositions which contain said compounds |
| US8158565B2 (en) | 2007-02-01 | 2012-04-17 | Shell Oil Company | Molybdenum alkylxanthates and lubricating compositions |
| US8188017B2 (en) | 2007-02-01 | 2012-05-29 | Shell Oil Company | Organic molybdenum compounds and oil compositions containing the same |
| US8329624B2 (en) | 2007-02-01 | 2012-12-11 | Shell Oil Company | Organic molybdenum compounds and lubricating compositions which contain said compounds |
| US8530686B2 (en) | 2007-02-01 | 2013-09-10 | Shell Oil Company | Organic molybdenum compounds and lubricating compositions which contain said compounds |
| JP2010001507A (ja) * | 2008-06-18 | 2010-01-07 | Minoru Mitani | アルミニウム又はアルミニウム合金の表面処理方法及びその表面処理方法により処理されたアルミニウム又はその合金製品 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0244914B2 (enExample) | 1990-10-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US5534308A (en) | Ceramic, Heat insulation layer on metal structural part and process for its manufacture | |
| KR950001221B1 (ko) | 알루미늄 복합품의 제조방법 | |
| US6379523B1 (en) | Method of treating surface of aluminum blank | |
| JPS62161992A (ja) | 無機多孔質体の表面強化法 | |
| US4895625A (en) | Method for producing a galvanically deposited protection layer against hot gas corrosion | |
| US4439287A (en) | Method for anodizing aluminum materials and aluminized parts | |
| US4455201A (en) | Bath and method for anodizing aluminized parts | |
| US3438789A (en) | Lubricant coating for friction surfaces and process for producing same | |
| US3676308A (en) | Electrolytic codeposition of polyvinylidene and copolymer particles with copper | |
| Benea | Electrodeposition of zirconia particles in a copper matrix | |
| RU2169800C1 (ru) | Способ получения оксидного композиционного покрытия на алюминии и его сплавах | |
| US3506555A (en) | Electrodeposition of polytetrafluoroethylene on metals | |
| JPH07268687A (ja) | アルミニウム又はその合金及びその表面処理法 | |
| US3840442A (en) | Titanium or titanium alloys having an anodized surface layer and method of forming | |
| JPH0368778A (ja) | 摺動部材 | |
| CN119553332B (zh) | 一种铝合金微弧氧化镀液及其制备方法和应用 | |
| KR100360536B1 (ko) | 경질 크롬 도금과 그 제조방법 | |
| JPH0428898A (ja) | 陽極酸化皮膜を有する物品及びその製造方法 | |
| JPS5812358B2 (ja) | アルミニウム合金の表面処理方法 | |
| JP2944799B2 (ja) | アルミニウムまたはアルミニウム合金の表面処理方法 | |
| JPH09228092A (ja) | 耐腐食性鉄メッキ膜およびメッキ方法 | |
| US3342708A (en) | Process for lubricating a bearing surface | |
| JP2005060720A (ja) | アルミニウム系部材とその製造方法およびアルミニウム系部材の表面処理方法 | |
| JP2014084481A (ja) | 潤滑性着色アルマイト皮膜とその生産方法 | |
| Váradi et al. | Simultaneous cataphoretic and electrolytic deposition of nickel for cathode bases of reliable electron tubes |