JPS6198749A - 耐久撥水加工方法 - Google Patents
耐久撥水加工方法Info
- Publication number
- JPS6198749A JPS6198749A JP22168184A JP22168184A JPS6198749A JP S6198749 A JPS6198749 A JP S6198749A JP 22168184 A JP22168184 A JP 22168184A JP 22168184 A JP22168184 A JP 22168184A JP S6198749 A JPS6198749 A JP S6198749A
- Authority
- JP
- Japan
- Prior art keywords
- gas
- dispersion
- monomer
- sheet material
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Treatments Of Macromolecular Shaped Articles (AREA)
- Graft Or Block Polymers (AREA)
- Chemical Or Physical Treatment Of Fibers (AREA)
- Treatments For Attaching Organic Compounds To Fibrous Goods (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22168184A JPS6198749A (ja) | 1984-10-19 | 1984-10-19 | 耐久撥水加工方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22168184A JPS6198749A (ja) | 1984-10-19 | 1984-10-19 | 耐久撥水加工方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6198749A true JPS6198749A (ja) | 1986-05-17 |
| JPH041776B2 JPH041776B2 (cg-RX-API-DMAC7.html) | 1992-01-14 |
Family
ID=16770606
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP22168184A Granted JPS6198749A (ja) | 1984-10-19 | 1984-10-19 | 耐久撥水加工方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6198749A (cg-RX-API-DMAC7.html) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2015133532A1 (ja) * | 2014-03-04 | 2015-09-11 | ダイキン工業株式会社 | 高分子基材、その用途及びその製造方法 |
-
1984
- 1984-10-19 JP JP22168184A patent/JPS6198749A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2015133532A1 (ja) * | 2014-03-04 | 2015-09-11 | ダイキン工業株式会社 | 高分子基材、その用途及びその製造方法 |
| JP2015180723A (ja) * | 2014-03-04 | 2015-10-15 | ダイキン工業株式会社 | 高分子基材、その用途及びその製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH041776B2 (cg-RX-API-DMAC7.html) | 1992-01-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2990608B2 (ja) | 表面処理方法 | |
| JP7336019B2 (ja) | 撥水ナノ膜及びその製造方法、応用、並びに製品 | |
| JP2010042410A (ja) | 表面コーティング | |
| JP4528634B2 (ja) | 金属膜の形成方法 | |
| JP2002510363A (ja) | 表面コーティング | |
| KR940018419A (ko) | 발수성을 향상시킨 불소 함유 고분자 성형체 및 이로 부터 제조된 세정용 지그 | |
| JP2011501993A (ja) | 新規な方法 | |
| EP2275598B1 (en) | Surface coatings | |
| AU779530B2 (en) | A method of coating the surface of an inorganic substrate with an organic material and the product obtained | |
| JP2009223158A (ja) | 眼用レンズ及び眼用レンズの製造方法 | |
| US5143748A (en) | Timber surface improving treatment process | |
| WO2000020130A1 (en) | Surface coatings | |
| JPS6198749A (ja) | 耐久撥水加工方法 | |
| JP6829857B1 (ja) | コンタクトレンズ消毒用過酸化水素の分解触媒およびその製造方法 | |
| JPS6189236A (ja) | 表面改質法 | |
| JPH05295656A (ja) | コーティング布帛の製造方法 | |
| JPH041775B2 (cg-RX-API-DMAC7.html) | ||
| JPH01154021A (ja) | コンタクトレンズ及びその製造方法 | |
| JPH0413368B2 (cg-RX-API-DMAC7.html) | ||
| JPH02127442A (ja) | フツ化オレフイン重合体成形物の表面処理法 | |
| US4379200A (en) | Novel method of producing ion exchange membrane | |
| JPH0543721A (ja) | フツ素フイルムの表面改質方法 | |
| CN118697945B (zh) | 一种抗菌性cf/peek复合材料及其制备方法和应用 | |
| JPH03217815A (ja) | コンタクトレンズ及びその製造方法 | |
| JPH07279052A (ja) | ポリプロピレン系基材の改質方法 |