JPS61276958A - ほうろう用冷延鋼板およびその製造方法 - Google Patents
ほうろう用冷延鋼板およびその製造方法Info
- Publication number
- JPS61276958A JPS61276958A JP60117294A JP11729485A JPS61276958A JP S61276958 A JPS61276958 A JP S61276958A JP 60117294 A JP60117294 A JP 60117294A JP 11729485 A JP11729485 A JP 11729485A JP S61276958 A JPS61276958 A JP S61276958A
- Authority
- JP
- Japan
- Prior art keywords
- less
- enameling
- cold
- rolled steel
- rolled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Sheet Steel (AREA)
- Electroplating Methods And Accessories (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (11)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60117294A JPS61276958A (ja) | 1985-05-30 | 1985-05-30 | ほうろう用冷延鋼板およびその製造方法 |
| US06/792,697 US4670065A (en) | 1984-10-24 | 1985-10-15 | Cold rolled steel suitable for enamel coating and method for making |
| CA000492962A CA1257789A (en) | 1984-10-24 | 1985-10-15 | Cold rolled steel suitable for enamel coating and method for making |
| ES548025A ES8900172A1 (es) | 1984-10-24 | 1985-10-18 | Procedimiento para la fabricacion de chapas de acero laminadas en frio adecuadas para revestimiento con esmalte |
| EP85113348A EP0179432B1 (en) | 1984-10-24 | 1985-10-21 | Cold rolled steel suitable for enamel coating and method for making |
| DE8585113348T DE3563223D1 (en) | 1984-10-24 | 1985-10-21 | Cold rolled steel suitable for enamel coating and method for making |
| ZA858071A ZA858071B (en) | 1984-10-24 | 1985-10-21 | Cold rolled steel suitable for enamel coating and method for making |
| AU48959/85A AU556276B2 (en) | 1984-10-24 | 1985-10-23 | Cold rolled steel suitable for enamel coating |
| NO854237A NO165408C (no) | 1984-10-24 | 1985-10-23 | Kaldvalset staalplate og fremgangsmaate for fremstilling avdenne. |
| KR1019850007885A KR890003664B1 (ko) | 1984-10-24 | 1985-10-23 | 에나멜 코우팅용 냉연강판과 그 제조방법 |
| CN85108620A CN1003179B (zh) | 1984-10-24 | 1985-10-24 | 适于搪瓷涂层的冷轧钢板及制造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60117294A JPS61276958A (ja) | 1985-05-30 | 1985-05-30 | ほうろう用冷延鋼板およびその製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61276958A true JPS61276958A (ja) | 1986-12-06 |
| JPH0416539B2 JPH0416539B2 (enExample) | 1992-03-24 |
Family
ID=14708191
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60117294A Granted JPS61276958A (ja) | 1984-10-24 | 1985-05-30 | ほうろう用冷延鋼板およびその製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61276958A (enExample) |
Cited By (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0230738A (ja) * | 1988-07-20 | 1990-02-01 | Kawasaki Steel Corp | 耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
| JPH0293046A (ja) * | 1988-09-29 | 1990-04-03 | Kawasaki Steel Corp | 直接一回掛けほうろう用鋼板 |
| JPH0293047A (ja) * | 1988-09-28 | 1990-04-03 | Sumitomo Metal Ind Ltd | ほうろう用鋼板およびその製造方法 |
| JPH02104640A (ja) * | 1988-10-12 | 1990-04-17 | Kawasaki Steel Corp | プレス成形性と耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
| JPH0310048A (ja) * | 1989-03-10 | 1991-01-17 | Kawasaki Steel Corp | 耐つまとび性、耐泡・黒点欠陥性及びプレス成形性に優れたほうろう用鋼板並びにその製造方法 |
| US5152846A (en) * | 1989-07-19 | 1992-10-06 | Kawasaki Steel Corporation | Method of producing steel sheets for porcelain enameling having improved enamel adhesion property |
| US6361624B1 (en) | 2000-09-11 | 2002-03-26 | Usx Corporation | Fully-stabilized steel for porcelain enameling |
| CN103911490A (zh) * | 2014-04-04 | 2014-07-09 | 首钢总公司 | 超低碳搪瓷钢钢水增氮的方法 |
-
1985
- 1985-05-30 JP JP60117294A patent/JPS61276958A/ja active Granted
Cited By (11)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0230738A (ja) * | 1988-07-20 | 1990-02-01 | Kawasaki Steel Corp | 耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
| JPH0293047A (ja) * | 1988-09-28 | 1990-04-03 | Sumitomo Metal Ind Ltd | ほうろう用鋼板およびその製造方法 |
| JPH0293046A (ja) * | 1988-09-29 | 1990-04-03 | Kawasaki Steel Corp | 直接一回掛けほうろう用鋼板 |
| JPH02104640A (ja) * | 1988-10-12 | 1990-04-17 | Kawasaki Steel Corp | プレス成形性と耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
| JPH0310048A (ja) * | 1989-03-10 | 1991-01-17 | Kawasaki Steel Corp | 耐つまとび性、耐泡・黒点欠陥性及びプレス成形性に優れたほうろう用鋼板並びにその製造方法 |
| US5098491A (en) * | 1989-03-10 | 1992-03-24 | Kawasaki Steel Corporation | Method of producing steel sheets for porcelain enameling and the same |
| US5292383A (en) * | 1989-03-10 | 1994-03-08 | Kawasaki Steel Corporation | Steel sheets for procelain enameling and method of producing the same |
| US5152846A (en) * | 1989-07-19 | 1992-10-06 | Kawasaki Steel Corporation | Method of producing steel sheets for porcelain enameling having improved enamel adhesion property |
| US6361624B1 (en) | 2000-09-11 | 2002-03-26 | Usx Corporation | Fully-stabilized steel for porcelain enameling |
| CN103911490A (zh) * | 2014-04-04 | 2014-07-09 | 首钢总公司 | 超低碳搪瓷钢钢水增氮的方法 |
| CN103911490B (zh) * | 2014-04-04 | 2015-08-26 | 首钢总公司 | 超低碳搪瓷钢钢水增氮的方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0416539B2 (enExample) | 1992-03-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR970008164B1 (ko) | 법랑피복용 강판 및 그 제조방법 | |
| US20040244885A1 (en) | Steel sheet for vitreous enameling and method for producing the same | |
| KR20090089791A (ko) | 우수한 연성을 갖는 고강도 강판 및 그 제조 방법 | |
| JP2023515558A (ja) | グラスライニング用鋼及びその製造方法 | |
| US6217675B1 (en) | Cold rolled steel sheet having improved bake hardenability | |
| KR890003664B1 (ko) | 에나멜 코우팅용 냉연강판과 그 제조방법 | |
| KR100264258B1 (ko) | 건축 재료로서 사용하기 위한 냉간압연 강대 및 용융 도금된 냉간압연 강대 및 그 제조방법 | |
| JPH0416539B2 (enExample) | ||
| US5156690A (en) | Building low yield ratio hot-dip galvanized cold rolled steel sheet having improved refractory property | |
| JP3309732B2 (ja) | 深絞り性の優れた直接1回掛けほうろう用冷延鋼板およびその製造方法 | |
| JPS5871360A (ja) | 耐食性ならびに加工性のすぐれたオ−ステナイト系ステンレス鋼とその鋼板の製造方法 | |
| JPS63500B2 (enExample) | ||
| US2006304A (en) | Alloy steel | |
| KR19990053146A (ko) | 박슬래브 직접압연법에 의한 고연성형 강관용 열연강판의 제조방법 | |
| JPS60116746A (ja) | 溶融亜鉛メツキ釜用鋼材 | |
| JPH08120406A (ja) | 溶接性に優れたほうろう用鋼板およびその製造方法 | |
| JPH05320823A (ja) | ほうろう用冷延鋼板およびその製造方法 | |
| JPS63109110A (ja) | 耐加熱黒変性に優れた溶融Alめっき鋼板用鋳片の製造方法 | |
| KR102031458B1 (ko) | 내식성과 균열전파 저항성이 우수한 열간 프레스 성형 부재 및 제조방법 | |
| JP2002241888A (ja) | 高温強度が高く且つ溶損が少ない溶融亜鉛釜用鋼 | |
| JP4312276B2 (ja) | 表面性状およびほうろう性に優れたほうろう用高酸素鋼板およびその製造方法 | |
| JPS581170B2 (ja) | ほうろう性の優れた熱延鋼板の製造法 | |
| RU2002851C1 (ru) | Низколегированна сталь | |
| JPH0653914B2 (ja) | ほうろう用鋼板及びその製造方法 | |
| JPS58217659A (ja) | 耳発生の小さい製缶用鋼板 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |