JPS61262590A - 粉状鉱石の流動層還元方法 - Google Patents
粉状鉱石の流動層還元方法Info
- Publication number
- JPS61262590A JPS61262590A JP10272285A JP10272285A JPS61262590A JP S61262590 A JPS61262590 A JP S61262590A JP 10272285 A JP10272285 A JP 10272285A JP 10272285 A JP10272285 A JP 10272285A JP S61262590 A JPS61262590 A JP S61262590A
- Authority
- JP
- Japan
- Prior art keywords
- ore
- fluidized bed
- temperature
- gas
- reduction
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture And Refinement Of Metals (AREA)
- Manufacture Of Iron (AREA)
- Crucibles And Fluidized-Bed Furnaces (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10272285A JPS61262590A (ja) | 1985-05-16 | 1985-05-16 | 粉状鉱石の流動層還元方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10272285A JPS61262590A (ja) | 1985-05-16 | 1985-05-16 | 粉状鉱石の流動層還元方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61262590A true JPS61262590A (ja) | 1986-11-20 |
| JPH0213015B2 JPH0213015B2 (enExample) | 1990-04-03 |
Family
ID=14335157
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP10272285A Granted JPS61262590A (ja) | 1985-05-16 | 1985-05-16 | 粉状鉱石の流動層還元方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61262590A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP7712597B1 (ja) * | 2024-02-05 | 2025-07-24 | 日本製鉄株式会社 | シャフト炉を用いた還元鉄の製造方法 |
| WO2026009488A1 (ja) * | 2024-07-04 | 2026-01-08 | 日本製鉄株式会社 | 水素還元システム及び還元鉄の製造方法 |
-
1985
- 1985-05-16 JP JP10272285A patent/JPS61262590A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP7712597B1 (ja) * | 2024-02-05 | 2025-07-24 | 日本製鉄株式会社 | シャフト炉を用いた還元鉄の製造方法 |
| WO2025169851A1 (ja) * | 2024-02-05 | 2025-08-14 | 日本製鉄株式会社 | シャフト炉を用いた還元鉄の製造方法 |
| WO2026009488A1 (ja) * | 2024-07-04 | 2026-01-08 | 日本製鉄株式会社 | 水素還元システム及び還元鉄の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0213015B2 (enExample) | 1990-04-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US5118479A (en) | Process for using fluidized bed reactor | |
| CA2387690A1 (en) | Method for gasifying organic materials and mixtures of materials | |
| US4265670A (en) | Method and apparatus for the thermal treatment of fine-grained material with hot gases | |
| US3873331A (en) | Process for fluid calcining cement raw meal | |
| JPH03243709A (ja) | 金属酸化物の直接還元方法及び装置 | |
| JP2732522B2 (ja) | 自溶性又は非自溶性で、自己還元性の鉱塊又は鉱石から鉄又は非鉄金属を製造する装置 | |
| JP3057576B2 (ja) | 粒子状材料の加熱処理方法及びその装置 | |
| US20120328507A1 (en) | Reduced moisture chemical reactions | |
| US1742750A (en) | Production and utilization of carbon monoxide | |
| JPH0213015B2 (enExample) | ||
| KR20000030020A (ko) | 유동입자층내의반응수행장치및방법 | |
| JPH02197530A (ja) | 鉄鉱石ペレットプロセスの燃焼方法 | |
| CN212375300U (zh) | 一种双炉型粉矿飞行熔融还原炼钢窑 | |
| JPS6360133A (ja) | 噴流層による造粒方法 | |
| JPS62225887A (ja) | 粉状鉱石の流動層還元方法 | |
| JPS62227020A (ja) | 溶融還元炉で発生した還元ガスの改質・加熱方法 | |
| JPH0152445B2 (enExample) | ||
| JPS58199809A (ja) | リアクタ−製鉄のための装置 | |
| JPS63235436A (ja) | クロム還元ペレツトの製造方法 | |
| JPS59104411A (ja) | 流動層予備還元炉による原料の予備還元方法および流動層予備還元炉 | |
| JPH02282416A (ja) | 流動層加熱方法及び加熱炉 | |
| JP2025527058A (ja) | 金属酸化物材料を製造するための方法及び装置 | |
| JPS6136573B2 (enExample) | ||
| JPS62228872A (ja) | 鉄鉱石予備還元装置 | |
| JPH092850A (ja) | セメントクリンカの製造方法 |