JPS6123624B2 - - Google Patents
Info
- Publication number
- JPS6123624B2 JPS6123624B2 JP10303079A JP10303079A JPS6123624B2 JP S6123624 B2 JPS6123624 B2 JP S6123624B2 JP 10303079 A JP10303079 A JP 10303079A JP 10303079 A JP10303079 A JP 10303079A JP S6123624 B2 JPS6123624 B2 JP S6123624B2
- Authority
- JP
- Japan
- Prior art keywords
- generating material
- particle size
- heat
- heat generating
- average particle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M6/00—Primary cells; Manufacture thereof
- H01M6/30—Deferred-action cells
- H01M6/36—Deferred-action cells containing electrolyte and made operational by physical means, e.g. thermal cells
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Primary Cells (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10303079A JPS5628473A (en) | 1979-08-13 | 1979-08-13 | Thermogenic material for thermoelectric battery |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10303079A JPS5628473A (en) | 1979-08-13 | 1979-08-13 | Thermogenic material for thermoelectric battery |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5628473A JPS5628473A (en) | 1981-03-20 |
| JPS6123624B2 true JPS6123624B2 (enExample) | 1986-06-06 |
Family
ID=14343245
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP10303079A Granted JPS5628473A (en) | 1979-08-13 | 1979-08-13 | Thermogenic material for thermoelectric battery |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5628473A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6077362A (ja) * | 1983-10-04 | 1985-05-01 | Nippon Kayaku Co Ltd | 溶融塩電池用発熱体及びその製造法 |
-
1979
- 1979-08-13 JP JP10303079A patent/JPS5628473A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5628473A (en) | 1981-03-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS6160539B2 (enExample) | ||
| US3536537A (en) | Method of making electrode having improved gas-recombination properties | |
| US4041217A (en) | Thermal battery with metal-metal oxide heating composition | |
| JPS5914260A (ja) | 液状正極電池用グラスフアイバセパレ−タ | |
| CA2098687A1 (en) | Lead-acid battery electrode and method of manufacture | |
| JPH08504052A (ja) | 電気化学的アルカリ金属電池およびその製造方法 | |
| US4053337A (en) | Heating composition | |
| US3471330A (en) | Battery with an electrolyte of solid alkali particles | |
| JPS6123624B2 (enExample) | ||
| CN115621479A (zh) | 一种热电池中间层及其制备方法 | |
| JPS6231789B2 (enExample) | ||
| DE2137737C1 (de) | Thermalbatterie | |
| JPH0261095B2 (enExample) | ||
| JPH05101831A (ja) | 熱電池 | |
| CN120600797B (zh) | 低界面阻抗的磷酸铁锂正极材料及其制备方法、锂电池 | |
| JPH0365624B2 (enExample) | ||
| JPH0234760Y2 (enExample) | ||
| JP3354247B2 (ja) | 正極活物質層の形成方法及び二次電池用正極板 | |
| JPH0234762Y2 (enExample) | ||
| JPH01122562A (ja) | 熱電池用負極の製造法 | |
| JP2600752B2 (ja) | 熱電池 | |
| JPH0234763Y2 (enExample) | ||
| JPS6240822B2 (enExample) | ||
| JP4666959B2 (ja) | 熱電池 | |
| JPH0256857A (ja) | アルカリマンガン電池 |