JPS61157699A - 電気めつき用ニツケル陽極材 - Google Patents
電気めつき用ニツケル陽極材Info
- Publication number
- JPS61157699A JPS61157699A JP27660484A JP27660484A JPS61157699A JP S61157699 A JPS61157699 A JP S61157699A JP 27660484 A JP27660484 A JP 27660484A JP 27660484 A JP27660484 A JP 27660484A JP S61157699 A JPS61157699 A JP S61157699A
- Authority
- JP
- Japan
- Prior art keywords
- nickel
- anode
- anode material
- electroplating
- plating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Electroplating And Plating Baths Therefor (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP27660484A JPS61157699A (ja) | 1984-12-29 | 1984-12-29 | 電気めつき用ニツケル陽極材 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP27660484A JPS61157699A (ja) | 1984-12-29 | 1984-12-29 | 電気めつき用ニツケル陽極材 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61157699A true JPS61157699A (ja) | 1986-07-17 |
JPH0357200B2 JPH0357200B2 (enrdf_load_stackoverflow) | 1991-08-30 |
Family
ID=17571754
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP27660484A Granted JPS61157699A (ja) | 1984-12-29 | 1984-12-29 | 電気めつき用ニツケル陽極材 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61157699A (enrdf_load_stackoverflow) |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63149970U (enrdf_load_stackoverflow) * | 1987-03-20 | 1988-10-03 | ||
WO2010064642A1 (ja) * | 2008-12-02 | 2010-06-10 | 住友金属工業株式会社 | ニッケル材及びニッケル材の製造方法 |
JP2010132934A (ja) * | 2008-12-02 | 2010-06-17 | Sumitomo Metal Ind Ltd | ニッケル冷間圧延コイル、及びニッケル冷間圧延コイルの製造方法 |
JP2010132933A (ja) * | 2008-12-02 | 2010-06-17 | Sumitomo Metal Ind Ltd | ニッケル材及びニッケル材の製造方法 |
JP2010261097A (ja) * | 2009-04-07 | 2010-11-18 | Sumitomo Metal Ind Ltd | ニッケル材料及びその製造方法 |
KR101311558B1 (ko) * | 2008-12-02 | 2013-09-26 | 신닛테츠스미킨 카부시키카이샤 | 니켈재 및 니켈재의 제조 방법 |
CN108456807A (zh) * | 2017-12-19 | 2018-08-28 | 重庆材料研究院有限公司 | 一种耐高温熔融烧碱腐蚀的镍材 |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5983796A (ja) * | 1982-11-01 | 1984-05-15 | Takeo Meguro | 鍍金用電解ニツケル・アノ−ド及びその製造方法 |
-
1984
- 1984-12-29 JP JP27660484A patent/JPS61157699A/ja active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5983796A (ja) * | 1982-11-01 | 1984-05-15 | Takeo Meguro | 鍍金用電解ニツケル・アノ−ド及びその製造方法 |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63149970U (enrdf_load_stackoverflow) * | 1987-03-20 | 1988-10-03 | ||
WO2010064642A1 (ja) * | 2008-12-02 | 2010-06-10 | 住友金属工業株式会社 | ニッケル材及びニッケル材の製造方法 |
JP2010132934A (ja) * | 2008-12-02 | 2010-06-17 | Sumitomo Metal Ind Ltd | ニッケル冷間圧延コイル、及びニッケル冷間圧延コイルの製造方法 |
JP2010132933A (ja) * | 2008-12-02 | 2010-06-17 | Sumitomo Metal Ind Ltd | ニッケル材及びニッケル材の製造方法 |
KR101311558B1 (ko) * | 2008-12-02 | 2013-09-26 | 신닛테츠스미킨 카부시키카이샤 | 니켈재 및 니켈재의 제조 방법 |
JP2010261097A (ja) * | 2009-04-07 | 2010-11-18 | Sumitomo Metal Ind Ltd | ニッケル材料及びその製造方法 |
CN108456807A (zh) * | 2017-12-19 | 2018-08-28 | 重庆材料研究院有限公司 | 一种耐高温熔融烧碱腐蚀的镍材 |
Also Published As
Publication number | Publication date |
---|---|
JPH0357200B2 (enrdf_load_stackoverflow) | 1991-08-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR890002621B1 (ko) | 복합합금의 제조방법 | |
CN100460544C (zh) | 一种变形铝-锰系合金及其制备方法 | |
CN111471905B (zh) | 一种用于3D打印的Al-Zn-Mg-Sc系铝合金丝材及其制备方法 | |
JP2007308766A (ja) | アルミニウム合金厚板の製造方法およびアルミニウム合金厚板 | |
JPS61157699A (ja) | 電気めつき用ニツケル陽極材 | |
CN119243001B (zh) | 一种多元微合金化高强耐蚀镁合金棒材及其制备方法 | |
JPH01168837A (ja) | 高モリブデンニッケル基合金 | |
JP2007308768A (ja) | アルミニウム合金厚板の製造方法およびアルミニウム合金厚板 | |
US3649487A (en) | Process for the recovery from secondary material of such metals as nickel cobalt iron and copper said secondary material comprising in addition one or more metals having a high melting point | |
JPH0748658A (ja) | 耐食性に優れた防食用犠牲電極用材料 | |
CN102418009B (zh) | 一种可消解高硬度化合物的铝合金及其熔炼方法 | |
US2923671A (en) | Copper electrodeposition process and anode for use in same | |
US3403997A (en) | Treatment of age-hardenable coppernickel-zinc alloys and product resulting therefrom | |
US2964399A (en) | Tantalum-titanium corrosion resistant alloy | |
NO792551L (no) | Fremgangsmaate ved galvanisering av jern-nikkel legeringer | |
US6309529B1 (en) | Method for producing sputtering target material | |
US3269825A (en) | Method of producing homogeneous alloys containing refractory metals | |
JPH03177594A (ja) | 高純度チタンの製造方法及び装置 | |
US2909473A (en) | Process for producing titanium group metals | |
CN109055842A (zh) | 一种Ti-Nb中间合金及其制备方法和应用 | |
RU2418084C2 (ru) | Способ получения алюминиевых сплавов для прокатки фольги | |
KR102044983B1 (ko) | 고내식 마그네슘 합금 및 그 제조방법 | |
CN112695234A (zh) | 一种耐蚀铝合金及其制备方法 | |
US2801917A (en) | Recovery plates and method of making same | |
CN110205528A (zh) | 一种高耐晶间腐蚀的Al-Mg合金及其制备方法 |