JPS6071554A - Manufacture of pair glass - Google Patents

Manufacture of pair glass

Info

Publication number
JPS6071554A
JPS6071554A JP58177428A JP17742883A JPS6071554A JP S6071554 A JPS6071554 A JP S6071554A JP 58177428 A JP58177428 A JP 58177428A JP 17742883 A JP17742883 A JP 17742883A JP S6071554 A JPS6071554 A JP S6071554A
Authority
JP
Japan
Prior art keywords
sealing material
glass
pair
leading end
filling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP58177428A
Other languages
Japanese (ja)
Inventor
Satoshi Kitagawa
聡 北川
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
National House Industrial Co Ltd
Original Assignee
National House Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by National House Industrial Co Ltd filed Critical National House Industrial Co Ltd
Priority to JP58177428A priority Critical patent/JPS6071554A/en
Publication of JPS6071554A publication Critical patent/JPS6071554A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To simplify the sealing by heating the leading end of a hot melt sealing material, coating and filling the four circumferential sides of a pair glass with the sealing material which keeping an uncured state, and jointing smoothly the terminal end with the leading end. CONSTITUTION:A pair glass 2 is formed by opposing a pair of glass plates 1 to each other through a spacer 4 made of Al, etc., and a recessed groove 5 to be filled with a hot melt sealing material 3 is provided to the cirvumference between the glass plates 1. The leading end 3a of the sealing material 3 to start the filling is pintched from the upper part of the glass plates 1 with a clip 6 furnished with a heater, and the sealing material 3 is successively filled into the four circumferential sides of the pair glass 2 while heating the leading end 3a and keeping the sealing material 3 in an uncured state. When the four sides are completely filled, the terminal end 3b is bonded to the uncured leading end 3a. The leading end 3a is satisfactorily bonded and combined to the terminal end 3b in this way, and the completely sealed pair glass can be obtained.

Description

【発明の詳細な説明】 〔技術分野〕 本発明は家屋の窓等に用いられるペアガラスの製造方法
に関する。
DETAILED DESCRIPTION OF THE INVENTION [Technical Field] The present invention relates to a method for manufacturing double glass used for windows of houses and the like.

〔背景技術〕[Background technology]

従来は、ペアカラス(2)の周縁にホット)ルトシール
材(3)を充填する場合、始端部(8a)から始めてペ
アガラス(2)周縁にホットメルトシール材(3)を連
続的に充填し、塗布を一周して始めに戻り、終端部(8
b)を始端部(8a)に接着させて打ち継ぐとき、始端
部(8a)は既に温度が低下して硬化が進行しており、
始端部(8a)と終端部(8b)の良好な接着が得られ
々かった。その為、四周にホットメルトシール材(3)
を塗布した後、始端部(8a)を再び加熱して再軟化さ
せて打ち継ぎ部を打ち直していた。
Conventionally, when filling the periphery of the pair glass (2) with the hot melt sealant (3), the hot melt sealant (3) is continuously filled around the periphery of the pair glass (2) starting from the starting end (8a), Go around the application, return to the beginning, and apply at the end (8
When bonding b) to the starting end (8a) and splicing, the temperature of the starting end (8a) has already decreased and hardening has progressed,
Good adhesion between the starting end (8a) and the ending end (8b) could not be obtained. Therefore, hot melt sealing material (3) is used around the four circumferences.
After coating, the starting end (8a) was heated again to soften it again, and the spliced part was recast.

〔発明の目的〕[Purpose of the invention]

本発明は収車の従来例の欠点に鑑みてなされたものであ
り、その目的とするところはホットメルトシール材の始
端部を加熱して未硬化状態を維持しながら四周への塗布
を行なうことによりスムーズに終端部を始端部に接着し
て打ち継ぐことができ、シール作業を簡単にすることに
ある。
The present invention was made in view of the shortcomings of conventional vehicle collection systems, and its purpose is to heat the starting end of the hot melt sealant and apply it to all four circumferences while maintaining an uncured state. This allows the terminal end to be bonded to the start end smoothly and jointed, thereby simplifying the sealing work.

〔発明の開示」 本発明ペアガラスの製造方法は、一対のガラス板(1)
を対向させたペアガラス(2)の四周にホットメルトシ
ール材(3)を連続的に充填するに際し、充填始めのホ
ットメルトシール材(3)の始端部(8a)を加熱して
未硬化状態を維持−しながらペアガラス(2)の周縁に
ホットメルトシール材(3)を連続的に充填し、充填線
りの終端部(8b)を上記始端部(8a)に接着して始
端部(8a)と終端部(8b)とを連続させることを特
徴とするものであって、これによって上記目的を達成し
たものである。
[Disclosure of the Invention] The method for manufacturing double glass of the present invention comprises a pair of glass plates (1).
When continuously filling the four circumferences of the pair of glass glasses (2) with the hot melt sealant (3), the starting end (8a) of the hot melt sealant (3) at the beginning of filling is heated to bring it into an uncured state. The hot melt sealant (3) is continuously filled around the periphery of the double glass (2) while maintaining the temperature, and the terminal end (8b) of the filling wire is adhered to the starting end (8a) to form the starting end ( 8a) and the terminal end (8b) are continuous, thereby achieving the above object.

以下、本発明を添付図により詳述する。(2)はアルミ
ニウム製のスペーサー(4)を介して1対のガラス板(
1)を対向させたペアカラスであり、ガラス板(1)間
の周囲にはホットメルトシール材(3)を充填するため
の凹溝(5)が設けられている。まず、ペアカラス(2
)の適所にホットメルト系づチルゴム等のホットメルト
シール材(3)を充填開始し、この始端部(8a)をカ
ラス板(1)の上から第8図に示すような電気し−9内
蔵のし一夕付クリップ(6)で挾み、し−タ付クリップ
(6)で始端部(3a)を加熱して未硬化状態を維持さ
せたまま、ペアカラス(2)の四周に連続的にホットメ
ルトシール材(3)を充填し、−周したところで終端部
(8b)を未硬化状態の始端部(8a)に接着させる。
Hereinafter, the present invention will be explained in detail with reference to the accompanying drawings. (2) is a pair of glass plates (
This is a pair of glasses with glass plates (1) facing each other, and a groove (5) for filling a hot-melt sealant (3) is provided around the space between the glass plates (1). First, a pair of crows (2
), start filling the hot-melt sealing material (3) such as hot-melt butyl rubber, and insert the starting end (8a) from above the glass plate (1) into the electric seal-9 built-in as shown in Figure 8. Hold it in place with the clips (6) and heat the starting end (3a) with the clip (6) with the insulator, keeping it in an uncured state, continuously around the four circumferences of the pair of crows (2). The hot-melt sealing material (3) is filled, and after one round, the terminal end (8b) is adhered to the uncured starting end (8a).

これによって始端部(8a)と終端部(3b)とが良好
′に接着されて一抹となり、簡単にシール作業できると
共にシールを完全に行なえるのである。
As a result, the starting end (8a) and the ending end (3b) are well bonded and form a single line, making it possible to perform the sealing operation easily and to perform the sealing completely.

〔発明の効果〕〔Effect of the invention〕

本発明は叙述の如く樋底されているから、ホットメルト
シール材をペアカラスの周囲に充填した後、始端部を再
加熱したりすることなくそのままで終端部を始端部に良
好に接着させることができ、シール作業を簡単に行なえ
ると共に確実にガラス板間の間隙部をシールできるとい
う利点がある
Since the present invention uses a gutter bottom as described above, after the hot melt sealant is filled around the pair of crows, the terminal end can be well bonded to the starting end without reheating the starting end. This has the advantage of making sealing work easier and reliably sealing the gaps between glass plates.

【図面の簡単な説明】[Brief explanation of drawings]

第1図は従来例の説明図、第2図は本□発明の一実施例
を示す説明図、第8図は同上の始端部の断面図である。 +1)・・・カラス板、+21 ・・・ペアカラス、(
3)・・・ホットメルトシール材、(8a)・・・始端
部、(8b)・・・終端部。 代理人 弁理士 石 1)長 七
FIG. 1 is an explanatory diagram of a conventional example, FIG. 2 is an explanatory diagram showing an embodiment of the present invention, and FIG. 8 is a sectional view of the starting end portion of the same. +1)...Crow board, +21...Pair crow, (
3) Hot melt sealing material, (8a) Starting end, (8b) Ending end. Agent Patent Attorney Ishi 1) Choshichi

Claims (1)

【特許請求の範囲】[Claims] (1)一対のカラス板を対向させたペアカラスの四周に
ホットメルトシール材を連続的に充填するに際し、充填
始めのホットメルトシール材の始端部を加熱して未硬化
状態を維持しながらペアガラスの周縁にホットメルトシ
ール材を連続的に充填し、充填路りの終端部を上記始端
部に接着して始端部と終端部とを連続させることを特徴
とするペアガラスの製造方法。
(1) When continuously filling the four circumferences of the paired crow with a pair of glass plates facing each other with hot melt sealant, the starting end of the hot melt sealing material at the beginning of filling is heated to maintain an uncured state while the glass is heated. 1. A method for manufacturing double glass, comprising: continuously filling the periphery of the glass with a hot-melt sealing material; and bonding the terminal end of the filling path to the starting end, thereby making the starting end and the terminal end continuous.
JP58177428A 1983-09-26 1983-09-26 Manufacture of pair glass Pending JPS6071554A (en)