JPS603966A - 溶融金属容器内の浮遊スラグの処理法 - Google Patents
溶融金属容器内の浮遊スラグの処理法Info
- Publication number
- JPS603966A JPS603966A JP11025983A JP11025983A JPS603966A JP S603966 A JPS603966 A JP S603966A JP 11025983 A JP11025983 A JP 11025983A JP 11025983 A JP11025983 A JP 11025983A JP S603966 A JPS603966 A JP S603966A
- Authority
- JP
- Japan
- Prior art keywords
- slag
- coolant
- inflow
- molten
- ladle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Casting Support Devices, Ladles, And Melt Control Thereby (AREA)
- Treatment Of Steel In Its Molten State (AREA)
- Furnace Charging Or Discharging (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11025983A JPS603966A (ja) | 1983-06-21 | 1983-06-21 | 溶融金属容器内の浮遊スラグの処理法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11025983A JPS603966A (ja) | 1983-06-21 | 1983-06-21 | 溶融金属容器内の浮遊スラグの処理法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS603966A true JPS603966A (ja) | 1985-01-10 |
JPS6261385B2 JPS6261385B2 (enrdf_load_stackoverflow) | 1987-12-21 |
Family
ID=14531153
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11025983A Granted JPS603966A (ja) | 1983-06-21 | 1983-06-21 | 溶融金属容器内の浮遊スラグの処理法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS603966A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN112760456A (zh) * | 2020-12-22 | 2021-05-07 | 武汉钢铁有限公司 | 一种使铋收得率不低于70%的含铋取向硅钢冶炼方法 |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01171041U (enrdf_load_stackoverflow) * | 1988-05-24 | 1989-12-04 |
-
1983
- 1983-06-21 JP JP11025983A patent/JPS603966A/ja active Granted
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN112760456A (zh) * | 2020-12-22 | 2021-05-07 | 武汉钢铁有限公司 | 一种使铋收得率不低于70%的含铋取向硅钢冶炼方法 |
CN112760456B (zh) * | 2020-12-22 | 2022-03-18 | 武汉钢铁有限公司 | 一种使铋收得率不低于70%的含铋取向硅钢冶炼方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS6261385B2 (enrdf_load_stackoverflow) | 1987-12-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP5772339B2 (ja) | 取鍋内スラグの再利用方法 | |
CN109777918A (zh) | 一种细化高碳铬轴承钢夹杂物颗粒的炉外精炼生产方法 | |
CN103088187B (zh) | 钢的制造方法 | |
CN117089772A (zh) | 一种高质量含硫冷镦钢盘条及其制备方法 | |
JP2011094210A (ja) | シリコクロムの脱炭素方法 | |
EP2692873A1 (en) | Method for manufacturing stainless steel | |
JPS603966A (ja) | 溶融金属容器内の浮遊スラグの処理法 | |
CN117467819A (zh) | 一种用于水雾化生产低氧不锈钢粉的脱氧扒渣方法 | |
JP2008240136A (ja) | 高清浄度鋼の溶製方法 | |
JPH11254109A (ja) | 高Mn丸断面鋳片の連続鋳造用モールドパウダ | |
JPH06218504A (ja) | タンディッシュ精錬法 | |
JP3257263B2 (ja) | 高清浄度溶鋼の製造方法 | |
JP2019000903A (ja) | 鋼の溶製方法及び連続鋳造方法 | |
CN114854939B (zh) | 一种用于铬铁铁水的摇包脱钛渣及铬铁铁水摇包脱钛方法 | |
JPS58154447A (ja) | 浸漬ノズルの閉塞防止方法 | |
JPS6050129A (ja) | テルミット法による金属合金の製造方法 | |
US3063831A (en) | Method of making titaniumcontaining alloys | |
US3024508A (en) | Process for obtaining ingots with a small amount of pipe and of segregation | |
CN107338343A (zh) | 熔剂和使用其的铸造方法 | |
JP6848429B2 (ja) | 製鋼スラグの改質方法 | |
RU2092570C1 (ru) | Способ выплавки стали в кислородном конвертере | |
SU1477761A2 (ru) | Способ производства феррохрома | |
JPH0693324A (ja) | アーク炉精錬における還元性スラグの処理方法 | |
JP3089380B2 (ja) | Ti含有鋼の製造方法 | |
JP2887535B2 (ja) | 鋼中介在物の無害化方法 |