JPS5933613Y2 - 熱収較性チユ−ブ - Google Patents
熱収較性チユ−ブInfo
- Publication number
- JPS5933613Y2 JPS5933613Y2 JP1977084670U JP8467077U JPS5933613Y2 JP S5933613 Y2 JPS5933613 Y2 JP S5933613Y2 JP 1977084670 U JP1977084670 U JP 1977084670U JP 8467077 U JP8467077 U JP 8467077U JP S5933613 Y2 JPS5933613 Y2 JP S5933613Y2
- Authority
- JP
- Japan
- Prior art keywords
- heat
- tube
- film
- shrinkable
- polyethylene film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Rigid Pipes And Flexible Pipes (AREA)
- Lining Or Joining Of Plastics Or The Like (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1977084670U JPS5933613Y2 (ja) | 1977-06-29 | 1977-06-29 | 熱収較性チユ−ブ |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1977084670U JPS5933613Y2 (ja) | 1977-06-29 | 1977-06-29 | 熱収較性チユ−ブ |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5412119U JPS5412119U (en:Method) | 1979-01-26 |
| JPS5933613Y2 true JPS5933613Y2 (ja) | 1984-09-19 |
Family
ID=29007574
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1977084670U Expired JPS5933613Y2 (ja) | 1977-06-29 | 1977-06-29 | 熱収較性チユ−ブ |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5933613Y2 (en:Method) |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS497943U (en:Method) * | 1972-04-22 | 1974-01-23 |
-
1977
- 1977-06-29 JP JP1977084670U patent/JPS5933613Y2/ja not_active Expired
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5412119U (en:Method) | 1979-01-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA2209518A1 (en) | Heat shrinkable member and method of forming the same | |
| US2964065A (en) | Polytetrafluoroethylene tubing and method of making the same | |
| JPS5933613Y2 (ja) | 熱収較性チユ−ブ | |
| US4032380A (en) | Method of joining of insulated high-voltage cables | |
| JP2619348B2 (ja) | 熱収縮チューブの製造方法 | |
| JPS5854009B2 (ja) | 段階的に収縮する樹脂管の製造方法 | |
| JP3065711B2 (ja) | 熱収縮性物品、その製造法および複合シート | |
| JPS6146302B2 (en:Method) | ||
| JPS609899B2 (ja) | 熱収縮性プラスチツクチユ−ブ | |
| KR19980073852A (ko) | 열수축성 엠보싱 튜브의 제조방법 | |
| SU1767276A1 (ru) | Способ ремонта трубопровода | |
| JP3123578B2 (ja) | 電解コンデンサの製造方法およびその製造装置 | |
| JPS5849382B2 (ja) | チュ−ブの製造法 | |
| JPH0613581Y2 (ja) | シリコ−ンゴム複合熱収縮性チユ−ブ | |
| JPS61242823A (ja) | ポリエスチレンパイプの成形法 | |
| JPS608040A (ja) | 熱収縮チユ−ブ作製方法 | |
| JPS5914341B2 (ja) | 熱回復性合成樹脂成形体 | |
| JPH0259322A (ja) | ヒートパイプ式加熱用マンドレルおよびそのマンドレルを用いた熱収縮チューブの製造方法 | |
| JPS5854647B2 (ja) | 熱収縮性を有するチュ−ブの製造方法 | |
| JPS5918201B2 (ja) | 熱収縮性チユ−ブ | |
| JPS5847830B2 (ja) | ケ−ブル絶縁接続用収縮チユ−ブ | |
| JPS6130897B2 (en:Method) | ||
| JPS5935331B2 (ja) | 膜厚を数分割する未接着部を有する熱収縮性ポリオレフインシ−トの製造方法 | |
| JPS5962142A (ja) | 熱収縮性チユ−ブおよびその製造法 | |
| JPH10146890A (ja) | 熱収縮チューブの製造方法 |